daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone qikanliebiao
Article List
Browse all articles published in this journal

The Production of Circular Saw Diamond Tool Tips for Stone Cutting by Hot Pressing

Rare Metals and Cemented Carbides | Vol., Issue 3, 1994 | pp. 62-68
Choice of raw materials for the production of circular saw diamond tool tips by hot pressing, preparation of blend. structure and materials of dies and hot pressing process have beed described. The causes of product defects have been analyzed. It has been shown that at present hot pressing is the most widely used for it and the fastest developed method.
DOI: Cited: 0 Download: 0

Mixed Praseodymium and Neodymium Oxides As Catalyst For Synthesizing DOP, DOM and DOA

Rare Metals and Cemented Carbides | Vol., Issue 2, 1994 | pp. 1-4
The cheap raw material, mixed praseodymium and neodymiumoxides, can be used as catalyst for synthesizing plasticizer, such asDOP, DOM and DOA, with significant catalytic effect. The productscan be purified through simple processes. The catalysts can be recovered and regenerated with the same catalytic ability.
DOI: Cited: 0 Download: 0

Milling Behaviours of Various Ni Powders and Their Effects on the Structure and Properties of WC-9%Ni Cemented Carbide

Rare Metals and Cemented Carbides | Vol., Issue 2, 1994 | pp. 5-10
In this paper, the milling behaviours of carbonyl. electrolyticand reduced Ni powders and' reduced Co powder and their effects on thestructure and properties of WC-- 9 qoNi cemented' carbide are investigatedrespectiyely. The results show that Ni powder is much more aggregatedduring milling than Co powder. Of all Ni powders, carbonyl Ni powderhas the best technological performance. A new type of cemented carbide,equiyalent to WC--CO alloy, can be obtained from the carbonyl Nipowder and by process improvements.
DOI: Cited: 0 Download: 0

Change of Micrographs during Co Powder Production and Its Influence on Characters of WC--Co Mixture

Rare Metals and Cemented Carbides | Vol., Issue 2, 1994 | pp. 10-16
A SEM study is made on Co oxalate, Co oxide and Co metalpowders obtained from above sources. Detailed micros tructure comparison shows the change of their micrographs. Technological propertiesof WC--Co mixtures made from both powders are not the same. Presentpaper giyes a description of their influence.
DOI: Cited: 0 Download: 0

Study of Hot Pressed Micro--crystalline Boron Carbide

Rare Metals and Cemented Carbides | Vol., Issue 2, 1994 | pp. 16-20
Study is made of hot pressing of micro--crys talline boron carbide from ultra--fine boron carbide. The grain size, porosity, transverse s trength, fracture morphology and I notion factor of the ma tenalis also investigated. The relationship between transverse strength andgrain size is expressed' as follows: a ̄387. 6+ 182. 3 1The friction factor of boron carbide is determined as: K ̄0. 093.
DOI: Cited: 0 Download: 0

Application of Aqueous Caustic Ball Milling To Wolframate Production

Rare Metals and Cemented Carbides | Vol., Issue 2, 1994 | pp. 20-22
Practice shows, that the use of aqueous caustic ball milling ofwolframite concentrates instead' of traditional water ball milling notonly can reduce the mill liner wear and ball consumption, but also increase the decomposition rate during thermic caustic decomposition, a ndlower the consumption of flake caustic and operation cost. Thisprocess is practical and+' efficient.
DOI: Cited: 0 Download: 0

Development and Application of The New Synthetic Diamond Tip

Rare Metals and Cemented Carbides | Vol., Issue 2, 1994 | pp. 23-25
The test and application of a new efficient and durable synthetic diamond tip on disc saw are described. The diamonffeimpregnatedtip features good' performance, long life and high efficiency. Its cuttingefficiency and tool life are increased by 25qO and' 48. sqO respectivelyas compared to other diamond tips when it is used for cutting 7--scalehard rock.
DOI: Cited: 0 Download: 0

浸出过程的理论基础及实践

Rare Metals and Cemented Carbides | Vol., Issue 2, 1994 | pp. 28-32
浸出过程的理论基础及实践李洪桂(中南工业大学长沙410083)第六讲浸出过程在有色冶金中的应用1碱性浸出1.1俄没法在有色冶金申应用简况碱浸出主要指用NaOH或Na。COs浸出,在某些情况下的氨浸过程亦属于碱浸。碱浸出为有色冶金中应用较广的浸出方法之...
DOI: Cited: 0 Download: 0

难熔金属与硬质材料进展──从第十三届国际普兰西会议看发展动向(Ⅱ)

Rare Metals and Cemented Carbides | Vol., Issue 2, 1994 | pp. 33-38
难熔金属与硬质材料进展──从第十三届国际普兰西会议看发展动向(Ⅱ)邹志强(中南工业大学粉末冶金研究所长沙410083)3.3新材料进展经过数十年反复探索和研究,仅在最近几年才分别在法国和德国研制成功铁基粘结剂的第一代韧化TiB2金属陶瓷,并获得美国法...
DOI: Cited: 0 Download: 0

稀散金属近况(Ⅱ)

Rare Metals and Cemented Carbides | Vol., Issue 2, 1994 | pp. 39-45
稀散金属近况(Ⅱ)周令治,邹家炎(广州有色金属研究院广州510651)2SM的重要用途2.1近年国外SM的应用结构多年来美与日是世界耗SM的大户,两匡应用SM的情况具有代表性。今将1985~199:年间国外SM的应用结构列入表8~14。表8美与日的镓...