Development and Application of The New Synthetic Diamond Tip AITranslate

Zhongnan University of Technology;Zhongnan University of Technology;Zhongnan University of Technology
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The test and application of a new efficient and durable synthetic diamond tip on disc saw are described. The diamonffeimpregnatedtip features good' performance, long life and high efficiency. Its cuttingefficiency and tool life are increased by 25qO and' 48. sqO respectivelyas compared to other diamond tips when it is used for cutting 7--scalehard rock.

KeyWords AITranslate

synthetic diamond disc sawing tip powder metallurgy

1唐存印.影响人造金刚石刀头焊接质量的几个问题[J].石材,1999(8):4-7. 被引量:1

Basic Information:

DOI:

Chinese Library Classification Number:TG711.06[金属学及工艺—刀具与模具]

Citation Information:

The test and application of a new efficient and durable synthetic diamond tip on disc saw are described. The diamonffeimpregnatedtip features good' performance, long life and high efficiency. Its cuttingefficiency and tool life are increased by 25qO and' 48. sqO respectivelyas compared to other diamond tips when it is used for cutting 7--scalehard rock.

quote

GB/T 7714-2015 [1] LUO Xin-geng, WANG Xing-hua, LIU San-sheng. Development and Application of The New Synthetic Diamond Tip[J]. Rare Metals and Cemented Carbides, 1994(2): 23-25.
MLA [1] LUO Xin-geng, et al., "Development and Application of The New Synthetic Diamond Tip." Rare Metals and Cemented Carbides, no. 2, 1994, pp. 23-25.
APA [1] LUO Xin-geng, WANG Xing-hua, & LIU San-sheng. (1994). Development and Application of The New Synthetic Diamond Tip. Rare Metals and Cemented Carbides(2), 23-25.
IEEE [1] LUO Xin-geng, WANG Xing-hua, and LIU San-sheng, "Development and Application of The New Synthetic Diamond Tip," Rare Metals and Cemented Carbides, no. 2, pp. 23-25, 1994. keywords: {synthetic diamond, disc sawing tip, powder metallurgy}