The Production of Circular Saw Diamond Tool Tips for Stone Cutting by Hot Pressing AITranslate

Powder Metallurgical Factory of Zhongnan University of Technology
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Choice of raw materials for the production of circular saw diamond tool tips by hot pressing, preparation of blend. structure and materials of dies and hot pressing process have beed described. The causes of product defects have been analyzed. It has been shown that at present hot pressing is the most widely used for it and the fastest developed method.

KeyWords AITranslate

circular saw diamond tool tip hot pressing process

1吴睿.基于SPWM控制的恒温装置的设计研究[J].计算机光盘软件与应用,2012,15(22):232-233.

1黄德明.硬质合金圆锯的特点[J].刃具研究,1997(2):15-22.

2姜树权.G607圆锯床的改造[J].机械制造,1991,29(1):16-16.

3潘雅琴,杨昭苏.TC4钛合金热压变形行为的研究[J].稀有金属材料与工程,1993,22(5):45-51. 被引量:6

4潘雅琴,杨昭苏.TC11钛合金热压变形行为[J].稀有金属材料与工程,1992,21(3):18-26. 被引量:3

5杨志达.俄罗斯石材加工用金刚石工具[J].超硬材料与工程,1994(4):28-29.

6吕应曾.圆锯与带锯的比较[J].有色金属加工,1994(2):41-44.

7邵平,孙成文.氧化铝与金属的热压封接[J].上海硅酸盐,1992(2):104-108.

8赵永生,曾庆良,陈玉良.陶瓷刀具在干切削加工中的应用[J].组合机床与自动化加工技术,2004(8):19-20. 被引量:1

9李豫府.铝锭锯切工艺与设备综述[J].有色金属加工,1999(4):30-30.

10王琴,王长兰,张慧,王孝琪.石材加工用金刚石工具技术的进展[J].磨料磨具与磨削,1994(1):31-35. 被引量:4

Basic Information:

DOI:

Chinese Library Classification Number:TG717[金属学及工艺—刀具与模具]

Citation Information:

Choice of raw materials for the production of circular saw diamond tool tips by hot pressing, preparation of blend. structure and materials of dies and hot pressing process have beed described. The causes of product defects have been analyzed. It has been shown that at present hot pressing is the most widely used for it and the fastest developed method.

quote

GB/T 7714-2015 [1] HU Shun-sui. The Production of Circular Saw Diamond Tool Tips for Stone Cutting by Hot Pressing[J]. Rare Metals and Cemented Carbides, 1994(3): 62-68.
MLA [1] HU Shun-sui. "The Production of Circular Saw Diamond Tool Tips for Stone Cutting by Hot Pressing." Rare Metals and Cemented Carbides, no. 3, 1994, pp. 62-68.
APA [1] HU Shun-sui. (1994). The Production of Circular Saw Diamond Tool Tips for Stone Cutting by Hot Pressing. Rare Metals and Cemented Carbides(3), 62-68.
IEEE [1] HU Shun-sui, "The Production of Circular Saw Diamond Tool Tips for Stone Cutting by Hot Pressing," Rare Metals and Cemented Carbides, no. 3, pp. 62-68, 1994. keywords: {circular saw, diamond tool tip, hot pressing process}