daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Mixed Praseodymium and Neodymium Oxides As Catalyst For Synthesizing DOP, DOM and DOA AITranslate

Department of Chemistry, Anhui Normal University;Department of Chemistry, Anhui Normal University;Department of Chemistry, Anhui Normal University;Department of Chemistry, Anhui Normal University
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The cheap raw material, mixed praseodymium and neodymiumoxides, can be used as catalyst for synthesizing plasticizer, such asDOP, DOM and DOA, with significant catalytic effect. The productscan be purified through simple processes. The catalysts can be recovered and regenerated with the same catalytic ability.

KeyWords AITranslate

Praseodymium & neodymium oxide catalyst esterification

1陈其瑞,张凤美,郑爱华,焦肇林.混合氯化稀土催化合成DOP、DOM和DOA[J].稀有金属与硬质合金,1996,24(4):17-21. 被引量:2

2陈其瑞,邵明霞.Ln_2O_3/X-13分子筛作酯化反应催化剂的研究[J].稀有金属与硬质合金,1997,25(4):11-14. 被引量:3

3周开志,马培华.酯化反应中的化学催化方法研究进展[J].兴义民族师范学院学报,2010,0(1X):120-124. 被引量:3

4陈其瑞.Ln_2O_3/Al_2O_3催化合成内增塑剂DOM[J].稀有金属与硬质合金,1999,27(4):24-26. 被引量:1

5李沂濛,史建公,张毅,张敏宏.PVC耐寒增塑剂DOA用催化剂及工艺研究进展[J].合成树脂及塑料,2016,33(3):59-66.

1江琦,李向召,高智勤.稀土在催化中的应用研究进展[J].信阳师范学院学报:自然科学版,2005,18(4):467-470. 被引量:7

2李永梅,徐勇军.稀土分子筛的合成与应用研究进展[J].广东化工,2009,36(3):47-50. 被引量:7

3陈其瑞,邵明霞.Ln_2O_3/ZrO_2催化合成DOP、DOM和DOA[J].稀有金属与硬质合金,2001,29(3):23-26. 被引量:1

4李沂濛,史建公,张毅,张敏宏.PVC耐寒增塑剂DOA用催化剂及工艺研究进展[J].合成树脂及塑料,2016,33(3):59-66.

5师亚宁,赵永红,张广良,董庆斌.十二烷基磷酸单酯的合成工艺研究[J].印染助剂,2017,34(12):13-16.

6赵新,章小林.季鏻盐离子液体催化剂的制备及其催化合成乙酸正丁酯[J].石油化工,2018,47(10):66-72. 被引量:5

7张照明,赵艳丰.多元碳醇酯合成过程催化剂的研究进展[J].化学工程与装备,2019,0(11):204-205.

8陈其瑞.Ln_2O_3/MgO催化合成增塑剂IOP的研究[J].稀有金属与硬质合金,2003,31(4):16-17.

1蒋平平.酯化法合成增塑剂DOTP的研究[J].化学世界,1994,35(8):411-415. 被引量:13

2方海林,袁淑军.用硫酸氢钠作催化剂合成增塑剂DOS的研究[J].山东化工,1998(1):7-8. 被引量:4

3郭锡坤,高文华,张颍.吡啶对相转移催化合成增塑剂BBP产率的影响[J].精细石油化工,1997,14(1):27-29. 被引量:4

4周建伟,张引沁,黄艳芹,刘伟.相转移催化合成增塑剂BBP的反应动力学研究[J].化学世界,1999,40(9):471-473.

5杨钟辉,熊国华.固体酸催化合成增塑剂DEDB的工艺研究[J].金山油化纤,1997,16(1):19-22. 被引量:2

6杨志成,章小芬.大孔树脂催化合成增塑剂DBP的研究[J].华东地质学院学报,1998,21(2):171-177. 被引量:1

7高文华,郭锡坤,余穗军.相转移催化合成邻苯二甲酸丁苄酯的研究[J].汕头大学学报:自然科学版,1998,13(1):13-16. 被引量:1

8张晓娟.非酸性催化直接酯化法合成增塑剂DOTP[J].辽阳石油化专学报,1997,13(1):37-41.

9王晶,严盛槐,谷延松,白格尔,赵淑欣.涤纶废料合成增塑剂DOTP的研究[J].松辽学刊:自然科学版,1996(2):6-9.

10严福君,葛德其,钮庭树.用新型催化剂QS-1合成增塑剂酯的研究[J].精细石油化工,1998,15(4):10-12. 被引量:5

Basic Information:

DOI:

Chinese Library Classification Number:TQ414[化学工程]

Citation Information:

The cheap raw material, mixed praseodymium and neodymiumoxides, can be used as catalyst for synthesizing plasticizer, such asDOP, DOM and DOA, with significant catalytic effect. The productscan be purified through simple processes. The catalysts can be recovered and regenerated with the same catalytic ability.

quote

GB/T 7714-2015 [1] CHEN Qi-rui, ZHANG Feng-mei, LUO Ming-run, et al. Mixed Praseodymium and Neodymium Oxides As Catalyst For Synthesizing DOP, DOM and DOA[J]. Rare Metals and Cemented Carbides, 1994(2): 1-4.
MLA [1] CHEN Qi-rui, et al., "Mixed Praseodymium and Neodymium Oxides As Catalyst For Synthesizing DOP, DOM and DOA." Rare Metals and Cemented Carbides, no. 2, 1994, pp. 1-4.
APA [1] CHEN Qi-rui, ZHANG Feng-mei, LUO Ming-run, & JIAO Zhao-lin. (1994). Mixed Praseodymium and Neodymium Oxides As Catalyst For Synthesizing DOP, DOM and DOA. Rare Metals and Cemented Carbides(2), 1-4.
IEEE [1] CHEN Qi-rui, ZHANG Feng-mei, LUO Ming-run, and JIAO Zhao-lin, "Mixed Praseodymium and Neodymium Oxides As Catalyst For Synthesizing DOP, DOM and DOA," Rare Metals and Cemented Carbides, no. 2, pp. 1-4, 1994. keywords: {Praseodymium &neodymium oxide, catalyst, esterification}