Milling Behaviours of Various Ni Powders and Their Effects on the Structure and Properties of WC-9%Ni Cemented Carbide AITranslate
Abstract AITranslate
In this paper, the milling behaviours of carbonyl. electrolyticand reduced Ni powders and' reduced Co powder and their effects on thestructure and properties of WC-- 9 qoNi cemented' carbide are investigatedrespectiyely. The results show that Ni powder is much more aggregatedduring milling than Co powder. Of all Ni powders, carbonyl Ni powderhas the best technological performance. A new type of cemented carbide,equiyalent to WC--CO alloy, can be obtained from the carbonyl Nipowder and by process improvements.
KeyWords AITranslate
1杨碧华,周建华,李晋尧.镍代钴WC-9(Ni-Co)硬质合金的研究[J].稀有金属材料与工程,1996,25(6):36-39. 被引量:1
2李启厚,张程,王红军,刘志宏,刘智勇.超细镍粉的制备、应用现状及发展趋势[J].湿法冶金,2009,28(4):193-197. 被引量:4
3肖冬明,罗世铭,陈旭军,江林,陈正乾,毛海娜,张媛庆.羰基镍粉的制备及其在硬质合金行业的应用[J].硬质合金,2020,37(6):466-471.
4周建华,陈一鸣,孙宝琦.共沉淀法掺杂Al对Ni-Co硬质合金性能的影响[J].凿岩机械气动工具,2002,28(3):36-40. 被引量:2
1黄艳华,贺跃辉,谢志刚,向波.金刚石工具用Ni-Co合金粉末的制备及表征[J].超硬材料工程,2006,18(5):1-5. 被引量:9
2黄蓉,陈仕奇.草酸盐共沉淀法制备Cu-Sn预合金粉末[J].粉末冶金材料科学与工程,2010,15(5):525-529. 被引量:9
3张军,王修才,李莉莉,李承轩,李晶晶.单分散超细球状镍的制备及其磁性分析[J].河南科技大学学报:自然科学版,2013,34(4):98-100. 被引量:1
4孙磊,李军义,郭顺,罗文,杨国启.超细镍粉工艺现状与发展趋势[J].湖南有色金属,2014,30(5):57-60. 被引量:3
5余勇,曾归余,肖明清,乐晨,欧建雄.不同工艺对真空气雾化Ni粉粒度的影响研究[J].粉末冶金工业,2015,25(1):38-41. 被引量:13
6罗学全,于涛,温光华,朱光柱.球磨时间对WC-7%Co-3%Ni硬质合金组织和性能的影响[J].硬质合金,2020,37(3):240-247. 被引量:2
7刘龙辉,沈少波,赵天骄,成瑶,陈小雨.不同形貌纳米镍粉的制备[J].材料科学,2014,4(5):218-224.
1周建华,孙宝琦,吴国龙.不同粒度镍粉对WC-9%Ni硬质合金性能和组织的影响[J].稀有金属与硬质合金,1994,22(3):21-25. 被引量:4
2何会琴.ACC-9系列连铸保护渣的使用效果[J].四川冶金,1989,11(4):31--35.
3唐绍基.钨的不同形态对离子交换树脂的选择性[J].湖南冶金,1990(3):22-24. 被引量:4
4陈军,姚萍屏,盛洪超,徐国富.碳对铜基粉末冶金摩擦材料性能的影响[J].热加工工艺,2006,35(14):13-16. 被引量:23
5董凯林,曹万里,时凯华,江庆,高建.碳含量对WC-9Ni-1Cr细晶硬质合金组织结构及性能的影响[J].粉末冶金材料科学与工程,2015,20(3):449-455. 被引量:3
6辛海艳,史顺亮,吴翔,肖科.WC总碳含量对WC-9%Co硬质合金收缩系数影响的研究[J].稀有金属与硬质合金,2015,43(6):69-72. 被引量:2
7蔡康健,裴广林.PC-9机轮刹车盘的工艺及模具设计[J].航空精密制造技术,2004,40(2):42-43.
8郭文明,张延玲,刘洋,贾昕磊.不同形态Fe对Cr_2O_3还原的影响[J].工程科学学报,2015,37(10):1296-1304.
9戴湘平,易军,付胜,杨志礼.不同形态炭黑对粗颗粒钨粉配碳的影响[J].中国钨业,2013,28(4):40-43. 被引量:1
10范必威,王秀英,张华兵.不同形态钙对活性炭活性的影响及其消除方法的研究[J].黄金,2002,23(7):25-27. 被引量:2
Basic Information:
DOI:
Chinese Library Classification Number:TF125.3[冶金工程—粉末冶金]
Citation Information:
In this paper, the milling behaviours of carbonyl. electrolyticand reduced Ni powders and' reduced Co powder and their effects on thestructure and properties of WC-- 9 qoNi cemented' carbide are investigatedrespectiyely. The results show that Ni powder is much more aggregatedduring milling than Co powder. Of all Ni powders, carbonyl Ni powderhas the best technological performance. A new type of cemented carbide,equiyalent to WC--CO alloy, can be obtained from the carbonyl Nipowder and by process improvements.
quote
| GB/T 7714-2015 | [1] ZHOU Jian-hua, SUN Bao-qi, WU Guo-long. Milling Behaviours of Various Ni Powders and Their Effects on the Structure and Properties of WC-9%Ni Cemented Carbide[J]. Rare Metals and Cemented Carbides, 1994(2): 5-10. |
| MLA | [1] ZHOU Jian-hua, et al., "Milling Behaviours of Various Ni Powders and Their Effects on the Structure and Properties of WC-9%Ni Cemented Carbide." Rare Metals and Cemented Carbides, no. 2, 1994, pp. 5-10. |
| APA | [1] ZHOU Jian-hua, SUN Bao-qi, & WU Guo-long. (1994). Milling Behaviours of Various Ni Powders and Their Effects on the Structure and Properties of WC-9%Ni Cemented Carbide. Rare Metals and Cemented Carbides(2), 5-10. |
| IEEE | [1] ZHOU Jian-hua, SUN Bao-qi, and WU Guo-long, "Milling Behaviours of Various Ni Powders and Their Effects on the Structure and Properties of WC-9%Ni Cemented Carbide," Rare Metals and Cemented Carbides, no. 2, pp. 5-10, 1994. keywords: {Ni powder. milling. cemented carbide} |