Investigation on Uncoventional Coarsening of W Powder by Alkali Metal Elements during WO_3 Reduction

Rare Metals and Cemented Carbides | Vol., Issue 4, 1998 | pp. 1-6
The characters and differences of unconventional coarsening of W powder caused by Li, Na, K are studied in the paper. It reveals that Li is the optimum element for coarsening of W Powder. Very coarse crystal W powder with an average particle size of 100μm is obtained when doping amount of Li is not less than 400ppm and reduction temperature is not lower than 1000℃.
DOI: Cited: 0 Download: 0

The Effects of Forming Agent on the Forgeability of Steel-bonded Cemented Carbides

Rare Metals and Cemented Carbides | Vol., Issue 4, 1998 | pp. 11-14
The differences of powder fluidity oxidability and compaction pressure between the powders with or without forming have been studied in this paper. The results show that forming agent will eliminate the compact's defects during compaction and sintering and improve the blank. Analysis is made of the effect of porosity of sintering compact on the fracture property of large-size tungsten carbide grain and the plastic fluidity of steel substrate during forging.
DOI: Cited: 0 Download: 0

Study of Non-homogeneous Hard Alloys and Its Application in Hard-rock Drilling Tools

Rare Metals and Cemented Carbides | Vol., Issue 4, 1998 | pp. 15-20
Based on the average WC particle size and distribution in the powder and alloy, according to alloy's WC subcrystalline size, microstrain and Co-phase distribution, study is made of the influence of we particle size compositions and Co phase distribution on the physical mechanical properties of mining cemented carbides. The cemented carbides with a combination of non-homogeneous Co-phase and non-homogeneous hard phase has been satisfactorily used for hard-rock drilling tools.
DOI: Cited: 0 Download: 0

Effect of Ball-milling Conditions on the Properties of Steel-bonded WC Hard Alloy

Rare Metals and Cemented Carbides | Vol., Issue 4, 1998 | pp. 21-24
In this paper the influence of ball-milling conditions of steel-bonded WC hard alloy on the properties has been investigated. By altering ball-milling conditions, uniformity of powder mixture can be improved to obtain steel-bonded WC hard alloy with the uniform microstructure and good performance.
DOI: Cited: 0 Download: 0