Experimental Study on the Relationship Between the Wear and the Thermoelectric Property of YS25 Cemented Carbide Insert AITranslate
Abstract AITranslate
The relationship between the wear and the thermoelectric poverty of YS25 cemented carbide inserts has been experimentally studied in this paper. Then the corresponding experimental formula is established.
KeyWords AITranslate
1陈舜青,张发英,陈澄洲.YT15硬质合金微观组织对其热电特性的影响研究[J].硬质合金,1995,12(3):134-139. 被引量:4
1孟广耀,陈舜青.YS25硬质合金热电特性的研究[J].机械设计与制造,2002(3):112-113.
2陈舜青,孟广耀.热电势预测硬质合金刀片寿命的研究[J].硬质合金,2011,28(4):251-255.
3陈舜青,陈澄洲,张发英.对YW1硬质合金热电特性诸因素的分析[J].机械工程材料,1997,21(6):26-28. 被引量:2
4孟广耀,陈舜青,王福忠.对影响YS25硬质合金热电特性的诸因素分析[J].内蒙古工业大学学报:自然科学版,1996,15(1):19-27.
5陈舜青.YS25硬质合金热电特性的影响因素研究[J].硬质合金,1997,14(2):69-73. 被引量:3
6陈舜青,张发英,陈澄洲.YT15硬质合金微观组织对其热电特性的影响研究[J].硬质合金,1995,12(3):134-139. 被引量:4
7邓世平,张平,潘雄,郭卫民,唐光明.Ni-12Fe-1Mn-0.3Al和Ni-2.7Mn-1.7Al-1.1Si-0.8Co合金的热电特性[J].功能材料,2004(z1):1749-1751.
8陈舜青,张发英,陈澄洲.YT15硬质合金刀片热电特性与磨损关系的研究[J].华南理工大学学报:自然科学版,1996,24(2):68-72. 被引量:1
9陈舜青,孟广耀.YW2硬质合金刀片的热电性能与其耐磨性的相关性[J].中国机械工程,2010,21(17):2037-2039. 被引量:1
10GAO Jiacheng WANG Qiang WANG Yong LI Wei NIU Wenjuan.Microstructure and kinetics of hot deformation WE43 magnesium alloy[J].稀有金属:英文版,2008,27(4):405-409. 被引量:4
Basic Information:
DOI:
Chinese Library Classification Number:TG711.01[金属学及工艺—刀具与模具]
Citation Information:
The relationship between the wear and the thermoelectric poverty of YS25 cemented carbide inserts has been experimentally studied in this paper. Then the corresponding experimental formula is established.
quote
| GB/T 7714-2015 | [1] CHEN Shun-qing, YUAN Zhen-bo, WANG Gang. Experimental Study on the Relationship Between the Wear and the Thermoelectric Property of YS25 Cemented Carbide Insert[J]. Rare Metals and Cemented Carbides, 1998(4): 25-27. |
| MLA | [1] CHEN Shun-qing, et al., "Experimental Study on the Relationship Between the Wear and the Thermoelectric Property of YS25 Cemented Carbide Insert." Rare Metals and Cemented Carbides, no. 4, 1998, pp. 25-27. |
| APA | [1] CHEN Shun-qing, YUAN Zhen-bo, & WANG Gang. (1998). Experimental Study on the Relationship Between the Wear and the Thermoelectric Property of YS25 Cemented Carbide Insert. Rare Metals and Cemented Carbides(4), 25-27. |
| IEEE | [1] CHEN Shun-qing, YUAN Zhen-bo, and WANG Gang, "Experimental Study on the Relationship Between the Wear and the Thermoelectric Property of YS25 Cemented Carbide Insert," Rare Metals and Cemented Carbides, no. 4, pp. 25-27, 1998. keywords: {YS25 cemented Carbide, wear, thermoelectric potential, relationship} |