Production and Market of MoS 2 AITranslate

Beijing Nonferrous Metallurgical Design Research Institute
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The raw material for MoS 2 production, the process and main equipment, the product quality and properties, its application and market as well as its development strategy and future prospect are presented.

KeyWords AITranslate

MoS 2 production market prospect

1产品调查编委会.中国有色金属产品调查与研究[M].北京:科学出版社,1995.320.

2张文征.-[J].中国钼业,1997,(2):130-130.

1李大成,周新文,唐丽霞.二硫化钼生产制备技术及应用分析[J].中国钼业,2008,32(3):8-11. 被引量:16

2单继宏,宁桂玲,林源.MoS_2的润滑应用及新的合成技术[J].化工科技,2002,10(3):42-45. 被引量:4

1陈玮,张晔.MoS_2基复合润滑薄膜的制备及其摩擦性能[J].机械工程材料,2008,32(8):47-49. 被引量:8

2葛新建,孙建林,范慧莉.粘结固体润滑膜的摩擦学特性研究[J].润滑与密封,2006,31(10):134-136. 被引量:8

3张文轩,钟宏,符剑刚,闻振乾.常用钼化学品的生产应用现状[J].稀有金属与硬质合金,2009,37(1):61-64.

4徐志昌,张萍.MoS_2纳米材料化学合成工艺流程的研究[J].中国钼业,2009,33(6):11-25. 被引量:2

5郭军刚,崔玉青,卜春阳.氮气高温预处理对二硫化钼中碳含量影响研究[J].中国钼业,2011,35(1):32-34. 被引量:2

6周军,兰新哲,张秋利,宋永辉,邢相栋.微乳液法制备纳米二硫化钼酸沉过程研究[J].有色金属:冶炼部分,2011(8):47-51. 被引量:7

7陈寅,肖清贵,徐红彬,郭奋,张懿.单分散球形MoS_2超细粉体材料的制备[J].材料科学与工艺,2011,19(6):117-122. 被引量:1

8唐扬,刘利国,王泽宇,周洪梅,刘小华,丁诗泳.45#钢在含有微米级二硫化钼的18#齿轮油中的摩擦磨损性能[J].江南大学学报:自然科学版,2014,13(1):76-79. 被引量:4

9惠三顺,解小锋,胡耕科,李航宇.硝酸钠替代部分硝酸在二硫化钼生产中的应用研究[J].中国钼业,2014,38(3):37-39. 被引量:2

10缑卫军.纳米二硫化钼应用进展与我国钼资源展望[J].中国钼业,2015,39(2):4-6.

1汪一佛.磨机采用二硫化钼润滑[J].云南建材,1995(3):9-9.

2王铭洛.论我国水泥工业湿法回转窑的发展对策[J].广西建材,1994(3):1-6.

3何祚云.间二甲苯和间苯二甲酸生产工艺技术[J].合成纤维工业,2000,23(2):41-45. 被引量:5

4赵洪义,石效吉,李跃宏,郑德田.机立窑水泥发展对策[J].四川水泥,2002(3):5-10.

5秦勇,李宗全.MoS_2中的位错[J].金属学报,1993,29(8).

6邹济林.二硫化钼在设备润滑和机械加工中的应用[J].材料保护,1998,31(2):38-38.

7潘叶金.CaO存在时,MoS_2还原-碳化直接合成Mo_2C[J].中国钼业,2003,27(3):51-51.

8江显异,赵英,陈雄飞,陈增森.陶瓷釉面砖生产工艺技术的探讨[J].陶瓷,1996(3):31-34. 被引量:1

9专利名称:一种基于氯化钠模板的二硫化钼纳米片制备方法[J].中国钼业,2017,41(1):41-41.

10Mary.首个基于二硫化钼二维材料的微处理器芯片诞生[J].今日电子,2017,0(5):23-23.

Basic Information:

DOI:

Chinese Library Classification Number:TQ136.12[化学工程—无机化工]

Citation Information:

The raw material for MoS 2 production, the process and main equipment, the product quality and properties, its application and market as well as its development strategy and future prospect are presented.

quote

GB/T 7714-2015 [1] LIN He-cheng. Production and Market of MoS 2[J]. Rare Metals and Cemented Carbides, 1999(1): 48-53.
MLA [1] LIN He-cheng. "Production and Market of MoS 2." Rare Metals and Cemented Carbides, no. 1, 1999, pp. 48-53.
APA [1] LIN He-cheng. (1999). Production and Market of MoS 2. Rare Metals and Cemented Carbides(1), 48-53.
IEEE [1] LIN He-cheng, "Production and Market of MoS 2," Rare Metals and Cemented Carbides, no. 1, pp. 48-53, 1999. keywords: {MoS 2, production, market,prospect}