Microyield Strength of Beryllium Materials Used in Inertial Guidance Instrument AITranslate

Northwest Rare Metal Materials Research Institute;Northwest Rare Metal Materials Research Institute;Northwest Rare Metal Materials Research Institute;Northwest Rare Metal Materials Research Institute;Northwest Rare Metal Materials Research Institute
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Survey is made of study and testing methods of microyield strength(MYS) of beryllium materials used in inertial guidance instrument. The influence of grain size, impurity (BeO), heat treatment and microalloying on MYS of beryllium is discussed. The conclusion is that impact attritioned powder with finer grain size and lower oxide content and its isostatic press ing consolidation are an important way to obtain high MYS beryllium materials.

KeyWords AITranslate

beryllium microyield strength inertial guidance instrument

1康慧灵,何力军,许德美,钟景明,王战宏,孙本双,刘霄霞.粉末冶金多晶态铍室温断裂行为的研究进展[J].材料导报,2013,27(15):94-97. 被引量:1

2钟景明,李志年,王战宏,王东新,李峰,李军义,张健康.惯性器件用铍材研究及其应用进展[J].粉末冶金工业,2018,28(1):1-6. 被引量:6

1刘军,孙洪涛,李晖,王志萍,陈红,李娜.电感耦合等离子体原子发射光谱法测定铍中氧化铍的含量[J].理化检验:化学分册,2019,55(12):1452-1454. 被引量:3

2陈晓磊,王锐,邱增帅,严小军,刘建梅.铍材薄壁回转零件加工刀具磨损研究[J].工具技术,2020,54(7):20-23. 被引量:2

3于万洋,朱亮.电爆法制备钽微米粉[J].金属功能材料,2020,27(5):1-5.

4郑莉芳,王晓刚,岳丽娜,黄俊忠,钟景明.稀有轻金属铍及其合金的应用进展[J].稀有金属,2021,45(4):475-483. 被引量:7

5赵世丰,何力军,李美岁,宋明泽,张健康,李志年.室温金属铍拉伸形变的构成及其对本构行为的决定[J].宁夏大学学报:自然科学版,2022,43(2):152-156.

6黄旭刚,李志年,刘兆刚.机械加工对粉末冶金铍材表面残余应力的影响[J].粉末冶金工业,2023,33(1):73-77.

7高亢亢,马靖,韦娉婷,洪涛.超级金属铍:未来路在何方[J].矿物岩石地球化学通报,2023,42(1):248-252. 被引量:1

1付晓旭,钟景明,王东新,王学泽,王零森.氧化铍对铍材微屈服强度的影响[J].宇航材料工艺,2002,32(3):50-53. 被引量:4

2孙本双.惯性器件用高性能铍材及其尺寸稳定性[J].宇航材料工艺,1996,26(6):26-30. 被引量:1

3孙本双.惯性导航用铍材研制技术与进展[J].材料科学与工程,1990,8(3):40-44.

4徐翠平.铍与铍材惯性器件及其标准化[J].航天标准化,2010(3):5-7. 被引量:1

5叶世雄.几种航空航天用铍材的性能及其生产工艺[J].宇航材料工艺,1989(6):34-37.

6王晓东,宋雪杰,章培成,常江.铍材在高精度石英挠性加速度计上的应用[J].导弹与航天运载技术,2015(1):96-99. 被引量:4

7李志林,刘伟,姚忠凯.SiCw/Al复合材料的尺寸稳定性[J].宇航学报,1996,17(1):62-65. 被引量:6

8张鸿金.加强铍材研究贡献航天事业[J].有色金属工业,2003(12):30-31. 被引量:7

9胡卫平,王兆元,等.关于铍加工的综述[J].惯导与仪表,2001(2):46-48. 被引量:2

10陈明和,傅桂龙,张中元,徐洁,葛国华,张中光.SiC陶瓷在航天器高温结构件研制中的应用[J].南京航空航天大学学报,2000,32(2):132-136. 被引量:18

Basic Information:

DOI:

Chinese Library Classification Number:TJ765.22[兵器科学与技术—武器系统与运用工程];V252.2[一般工业技术—材料科学与工程]

Citation Information:

Survey is made of study and testing methods of microyield strength(MYS) of beryllium materials used in inertial guidance instrument. The influence of grain size, impurity (BeO), heat treatment and microalloying on MYS of beryllium is discussed. The conclusion is that impact attritioned powder with finer grain size and lower oxide content and its isostatic press ing consolidation are an important way to obtain high MYS beryllium materials.

quote

GB/T 7714-2015 [1] ZHONG Jing-ming, NIE Da-jun, FU Xiao-xu, et al. Microyield Strength of Beryllium Materials Used in Inertial Guidance Instrument[J]. Rare Metals and Cemented Carbides, 1999(1): 43-47.
MLA [1] ZHONG Jing-ming, et al., "Microyield Strength of Beryllium Materials Used in Inertial Guidance Instrument." Rare Metals and Cemented Carbides, no. 1, 1999, pp. 43-47.
APA [1] ZHONG Jing-ming, NIE Da-jun, FU Xiao-xu, WANG Xue-ze, & WANG Ling-sen. (1999). Microyield Strength of Beryllium Materials Used in Inertial Guidance Instrument. Rare Metals and Cemented Carbides(1), 43-47.
IEEE [1] ZHONG Jing-ming, NIE Da-jun, FU Xiao-xu, WANG Xue-ze, and WANG Ling-sen, "Microyield Strength of Beryllium Materials Used in Inertial Guidance Instrument," Rare Metals and Cemented Carbides, no. 1, pp. 43-47, 1999. keywords: {beryllium, microyield strength, inertial guidance instrument}