Review on oxidizing Roasters with NaCl for Vanadium containing Carbon Shales AITranslate

Changsha Nonferrous Metallurgical Design Research Institute
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Oxidizing roasting with NaCl is a key step for V 2O 5 extraction from vanadium containing carbon shales. Analysis is made of the design and operation of different roasters and processes for this application, particularly of the 50t V 2O 5/year 5.5m 2 fluidized bed furnace at Danjiangkou Vanadium Plant.

KeyWords AITranslate

V bearing carbon shale roasting fluidized bed furnace V 2O 5 conversion rate

1周宛谕,施正伦,王勤辉,徐耀斌.循环流化床中含钒石煤料球的焙烧特性试验研究[J].动力工程,2009,29(10):904-908. 被引量:3

2蔡晋强.石煤提钒工艺及设备进展[J].稀有金属与硬质合金,2010,38(2):67-71. 被引量:10

3兰涛,张晓瑜.石煤提钒工艺及焙烧设备的清洁性评价[J].安全与环境工程,2011,18(3):46-50. 被引量:5

4邢学永,宁顺明.石煤发热值与提钒工艺选择[J].中国有色冶金,2013,42(6):28-31. 被引量:3

1胡凯龙,刘旭恒.含钒石煤焙烧工艺综述[J].稀有金属与硬质合金,2015,43(1):1-6. 被引量:12

2王辉,兰新哲,马红周,宋永辉.微波焙烧对石煤钒矿浸出的影响[J].湿法冶金,2011,30(4):290-292. 被引量:3

3董辉,冯军胜,李鹏,蔡九菊,张井凡,陈广平.一种新型钒氧化钠化焙烧竖炉的研究[J].工业炉,2012,34(6):5-8. 被引量:4

4兰涛,张晓瑜,武征,孙愿.陕西省石煤提钒行业存在的问题及对策研究[J].环境科学与管理,2013,38(5):83-87. 被引量:4

5蔡晋强,龚加齐,郑越,姚玉梅.硫酸铵焙烧法从石煤钒矿中提取钒和铝的试验研究[J].稀有金属与硬质合金,2013,41(4):1-4. 被引量:6

6张焕侠.陕西小型石煤钒矿综合利用前景分析[J].陕西地质,2013,31(1):62-68. 被引量:3

7冯军胜,董辉,李朋,王爱华,张井凡,胡嘉.石煤提钒焙烧竖炉研究[J].钢铁钒钛,2013,34(6):12-16. 被引量:1

8邢学永,宁顺明.石煤发热值与提钒工艺选择[J].中国有色冶金,2013,42(6):28-31. 被引量:3

9田水承,杜娇,田志辉.基于HAZOP法的太阳能电池厂危险有害因素辨识与分析[J].安全与环境工程,2014,21(2):135-138.

10邱伟佳,魏昶,邓志敢,李旻廷,李兴彬,张帆.石煤发电飞灰碱浸提钒工艺[J].过程工程学报,2014,14(3):421-426. 被引量:2

1孙金阶.丹江口弘源公司10000KVA碳化硅电阻炉投产[J].磨料磨具通讯,2005(9):14-14.

2任丹洪.PLC在电石生产中的应用[J].湖北水力发电,2008(5):94-96. 被引量:1

3铬盐文摘[J].无机盐技术,2011(1):37-37.

4红矾钠技术改造示范工程[J].无机盐工业,2010(3):39-39.

5彭声谦,许国镇.石煤提钒中钠盐的作用[J].西南工学院学报,1998,13(1):9-12. 被引量:17

6丹江口弘源氮化硅一碳化硅制品工程项目荣获2010年度中国机械工业科学技术奖二等奖[J].磨料磨具通讯,2011(1):45-45.

7赵杰三,潘三红.带盖环式焙烧炉与敞开环式焙烧炉应用之比较[J].炭素技术,2010,29(6):47-49. 被引量:2

8胡杨甲,张一敏,刘涛,黄晶,陆岷,李建华.复合添加剂对石煤提钒焙烧过程影响的研究[J].金属矿山,2009(1):166-168. 被引量:10

9高峰,石美莲,周再兴,华骏,颜文斌.湘西含钒石煤提钒工艺研究[J].矿冶工程,2011,31(3):93-96. 被引量:10

10郑志远.辊道窑烧成带各段燃料消耗量计算及应用[J].福建轻纺,2002(7):7-9. 被引量:1

Basic Information:

DOI:

Chinese Library Classification Number:TQ135.11[化学工程—无机化工]

Citation Information:

Oxidizing roasting with NaCl is a key step for V 2O 5 extraction from vanadium containing carbon shales. Analysis is made of the design and operation of different roasters and processes for this application, particularly of the 50t V 2O 5/year 5.5m 2 fluidized bed furnace at Danjiangkou Vanadium Plant.

quote

GB/T 7714-2015 [1] ZHANG Xiao-hui. Review on oxidizing Roasters with NaCl for Vanadium containing Carbon Shales[J]. Rare Metals and Cemented Carbides, 1999(1): 53-57.
MLA [1] ZHANG Xiao-hui. "Review on oxidizing Roasters with NaCl for Vanadium containing Carbon Shales." Rare Metals and Cemented Carbides, no. 1, 1999, pp. 53-57.
APA [1] ZHANG Xiao-hui. (1999). Review on oxidizing Roasters with NaCl for Vanadium containing Carbon Shales. Rare Metals and Cemented Carbides(1), 53-57.
IEEE [1] ZHANG Xiao-hui, "Review on oxidizing Roasters with NaCl for Vanadium containing Carbon Shales," Rare Metals and Cemented Carbides, no. 1, pp. 53-57, 1999. keywords: {V bearing carbon shale, roasting, fluidized bed furnace,V 2O 5, conversion rate}