Investigation on Uncoventional Coarsening of W Powder by Alkali Metal Elements during WO_3 Reduction AITranslate

Powder Metallurgical Factory of Zhongnan University of Technology;Powder Metallurgical Factory of Zhongnan University of Technology;Powder Metallurgical Factory of Zhongnan University of Technology
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The characters and differences of unconventional coarsening of W powder caused by Li, Na, K are studied in the paper. It reveals that Li is the optimum element for coarsening of W Powder. Very coarse crystal W powder with an average particle size of 100μm is obtained when doping amount of Li is not less than 400ppm and reduction temperature is not lower than 1000℃.

KeyWords AITranslate

alkali metal WO3 W grain coarsening hydrogen reduction

1傅练英.蓝钨中钠含量对钨粉、碳化钨粉粒度影响的研究[J].硬质合金,1995,12(4):216-222. 被引量:3

2莫玉琛,罗振中.结晶钨粉的研制[J].稀有金属与硬质合金,1994,22(4):1-3. 被引量:2

1德志强.高质量结晶钨粉制取的工艺研究[J].硬质合金,2014,31(3):166-172. 被引量:1

2谭征,刘咏,贡太敏.Na元素掺杂方式对超粗晶碳化钨及其合金性能的影响[J].中国锰业,2017,35(2):108-112. 被引量:4

3全温灿,钟奕晖,严润,史冠勇,豆志河.稀释剂种类对自蔓延高温合成钨粉的影响[J].稀有金属与硬质合金,2022,50(2):26-30.

4张太全,龙本夫,林高安.合金元素对氧化钨氢还原过程和钨相关材料的组织与性能影响研究综述[J].中国材料进展,2022,41(6):466-476. 被引量:1

1谢俊杰,张龙辉,常卿卿,黄一春.掺杂与湿氢工艺制备超粗钨粉及其对合金性能的影响[J].硬质合金,2018,35(1):37-43. 被引量:3

2蔡海燕.超粗晶硬质合金的研究现状与发展趋势[J].硬质合金,2018,35(4):297-303. 被引量:10

3邹爱忠,黄星,王永生,郭圣达.基于截齿用途的粗晶钨合金材料的再利用技术研究[J].中国钨业,2020,35(1):56-61.

4李哲雨,李尚杰,李必红,王峰,同剑,苏红辈.钨粉颗粒形貌对钨铜合金药型罩破甲性能的影响[J].工程爆破,2021,27(4):94-99. 被引量:1

5郭景锋,王亦东,陈正领.钨粉还原炉Cr30Ni20合金高温炉管焊缝失效研究[J].材料导报,2022,36(S02):394-397.

6张文科,顾金宝,时凯华,董定乾,向新,熊萧,贺逢源,廖军,张立.超粗晶WC-Co硬质合金制备技术及发展趋势[J].稀有金属与硬质合金,2023,51(1):97-101.

1吴迪.碱金属对高炉生产的影响[J].北方钒钛,2014,0(Z1):7-8. 被引量:3

2莫玉琛,罗振中.结晶钨粉的研制[J].稀有金属与硬质合金,1994,22(4):1-3. 被引量:2

3莫玉琛,罗振中.结晶钨粉的研制[J].四川有色金属,1994(4):5-7. 被引量:2

4伍世辉,刘三林,李鲜明.韶钢6号高炉碱金属的危害及其控制[J].南方金属,2009(1):38-40. 被引量:6

5孙宝琦,陈一鸣.锂活化钨氧化物氢还原制取粗结晶钨粉过程的初步探讨[J].稀有金属与硬质合金,1999(1):1-6. 被引量:3

6伍世辉,刘三林,李鲜明.韶钢6号高炉碱金属危害的控制[J].炼铁,2009,28(1):39-41. 被引量:9

7王涛.养生不是追求长寿[J].健身科学,2015(7):1-1.

8德志强.高质量结晶钨粉制取的工艺研究[J].硬质合金,2014,31(3):166-172. 被引量:1

9冯以啸.2009年3月中国很可能成为钢材净进口国[J].锻造与冲压,2009(5):14-14.

10明宪权,吴晓丹,黄冠汉.高铁高磷难选锰矿高炉生产富锰渣的影响因素[J].中国锰业,2016,34(3):131-133. 被引量:3

Basic Information:

DOI:

Chinese Library Classification Number:TF123.24[冶金工程—粉末冶金]

Citation Information:

The characters and differences of unconventional coarsening of W powder caused by Li, Na, K are studied in the paper. It reveals that Li is the optimum element for coarsening of W Powder. Very coarse crystal W powder with an average particle size of 100μm is obtained when doping amount of Li is not less than 400ppm and reduction temperature is not lower than 1000℃.

quote

GB/T 7714-2015 [1] SUN Bao-qi, WU Guo-long, CHEN Yi-ming. Investigation on Uncoventional Coarsening of W Powder by Alkali Metal Elements during WO_3 Reduction[J]. Rare Metals and Cemented Carbides, 1998(4): 1-6.
MLA [1] SUN Bao-qi, et al., "Investigation on Uncoventional Coarsening of W Powder by Alkali Metal Elements during WO_3 Reduction." Rare Metals and Cemented Carbides, no. 4, 1998, pp. 1-6.
APA [1] SUN Bao-qi, WU Guo-long, & CHEN Yi-ming. (1998). Investigation on Uncoventional Coarsening of W Powder by Alkali Metal Elements during WO_3 Reduction. Rare Metals and Cemented Carbides(4), 1-6.
IEEE [1] SUN Bao-qi, WU Guo-long, and CHEN Yi-ming, "Investigation on Uncoventional Coarsening of W Powder by Alkali Metal Elements during WO_3 Reduction," Rare Metals and Cemented Carbides, no. 4, pp. 1-6, 1998. keywords: {alkali metal, WO3, W grain coarsening, hydrogen reduction}