Preparation of Nanometer Titanium Dioxide Powder
Rare Metals and Cemented Carbides | Vol., Issue 4, 2002 |
pp. 17-30
The nanometer anatase TiO2 powder was prepared by hydrolysis and homogeneous precipitation.The most favorable operating conditions were also studied.The morphology,size,crystal shape and specific surface area of nanometer TiO2 powder waere characterized by TEM,XRM,BET and DTA-TG methods.The results show that the TiO2 particle appears spherical shape,the average particle diameter is 20nm,and the specific surface area is 90m2/g.The new technology is simple to operate with low cost and is easy to be industrialized.The obtained nanometer titanium dioxide powder can meet the needs of markets.