daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

The Application of Solvent Impregnated Resin into Scandium Hydrometallurgy AITranslate

Department of Materials Science and Engineering, Central South University;Department of Materials Science and Engineering, Central South University
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The paper lntroduced research and application of solvent impregnated resin in extraction of scandiumAs a new kind of extractant,solvent impregnated resins can notably improve the capacity and the efficiency of scandium extraction,and is suitable in the ore pulp extraction that the general liquid extraction is hard to apply,indicating its unique good application prospect.

KeyWords AITranslate

solvent impregnated resins scandium hydrometallurgy application

1КоровинВЮ,идр.ЭкстракцияскандияизсернокислыхрастворовТБФиТВЭКС-ТБФподаннымЯМР 31 P и 45 Sc[J].Жнеоргхимии,1990,35(9):2 404.

2КоровинВЮ,идр.Экстракцияскандиятвёрдымэкстрагентом(ТВЭКС-ТБФ)изотходовтитаномагниевогопроизводства[J].Жприклхимии,1992,66(8):1 744.

3КоровинВЮ.Механизмызкстракциискандия(Ⅲ)Д2ЭГФКиТВЭКС-Д2ЭГФКподаннымспектроскопииЯМР 31p,45Sc[J].Координационнаяхимия,1991,17(4):561.

4Korovin V Yu,et al.31 P and 45Sc NMR studies on the extraction of scandium from hydrochloric acid solutions with liquid tributyl phosphate and tributyl phosphate in solid polymeric matrix of extractants[J].Russ J Coord Chem,1996,22(8):597.

5Korovin V Yu,et al.Processing of wates of titanium-magnesium production with scandium extraction by a solid extractant(TVEX-TBP)[J].Экотехнол.ресурсосбережение,1994,(3):25.

6КудрявскийЮΠ,идр.Концентрированиескандияизотходовтитановогопроизводства[J].Цвметаллы,1999,(1):60.

7КудрявскийЮΠ.Сорбционноеконцентрированиескандия(Ⅲ) измногокомпонентныхрастворов[J].Жприклхимии,1994,67(11):1 780.

8周春山,徐卫红,熊兴安,潘炳贤.CL-P_(350)萃淋树脂的合成及性能测定[J].中南工业大学学报,1997,28(3):294-297. 被引量:3

9尤曙彤,张平伟,张力,蒋蕴华,侯嵩寿.CL-TBP萃取色层法制备高纯氧化钪[J].稀有金属,1991,15(5):330-332. 被引量:12

10张平伟,蒋蕴华,张力,侯嵩寿.Cl-P_(350)萃淋树脂及其对钪的萃取[J].稀土,1990,11(2):12-16. 被引量:11

1李小康,许秀莲.溶剂萃取法提钪研究进展[J].南方冶金学院学报,2005,26(3):8-12. 被引量:4

2王碧,张凤金,覃松,廖学品.胶原纤维固化黑荆树单宁对钪吸附的研究[J].林产化学与工业,2008,28(1):33-38. 被引量:5

3孔晓朵,孙怡.钪萃取分离的研究进展[J].安徽大学学报:自然科学版,2009,33(2):89-94. 被引量:3

4罗文静,谢家理,田芳,吴剑平.P_(204)-TBP浸渍树脂对硫酸介质中Sc^(3+)的吸附行为研究及其应用[J].离子交换与吸附,2003,19(6):547-553. 被引量:6

5刘军深,蔡伟民.萃淋树脂技术分离稀散金属的研究现状及展望[J].稀有金属与硬质合金,2003,31(4):36-39. 被引量:25

1陈松,王培,张力,罗岁斌,郎书玲.萃取色层法净化钴溶液制备高纯钴的研究[J].稀有金属,2010,34(4):595-600. 被引量:3

2刘爽,黄益平,邹鑫,夏伟,刘毅,徐景富.“蓝皮”胶原吸附剂对于Cr(Ⅵ)的吸附特征研究[J].化工新型材料,2011,39(S2):100-102.

3王荣耕,李学平,翟学良.离子交换树脂回收钴镍技术进展[J].无机盐工业,2005,37(11):11-13. 被引量:15

4刘军深,宋文芹,李桂华,刘春萍,陈学颖.分离提取铟的几种新方法[J].广州化工,2005,33(5):17-20. 被引量:4

5刘军深,李桂华.螯合树脂法分离回收镓和铟的研究进展[J].稀有金属与硬质合金,2005,33(4):42-45. 被引量:14

6刘军深,李桂华,宋文芹,刘春萍.螯合树脂法从酸性溶液中分离回收铟和镓[J].有色金属:冶炼部分,2006(3):32-35. 被引量:9

7廖春发,焦芸芬,邱定蕃.膦(磷)类萃取剂浸渍树脂吸附重稀土的性能[J].过程工程学报,2007,7(2):268-272. 被引量:10

8丁健刚,焦利敏,王安,廖学品.磷酸化胶原纤维对Cu^(2+)的吸附特性研究[J].皮革科学与工程,2007,17(5):7-11. 被引量:2

9钱强.溶剂萃取在湿法冶金中的应用进展[J].中国资源综合利用,2007,25(10):14-15. 被引量:6

10王碧,张凤金,覃松,廖学品.胶原纤维固化黑荆树单宁对钪吸附的研究[J].林产化学与工业,2008,28(1):33-38. 被引量:5

1刘建,王秀山,杨子超,陈秋平,于欣,阎居梅.CL—P_(5709)萃淋树脂吸附及分离钨钼性能的研究[J].化工冶金,1990,11(3):222-228. 被引量:2

2游建南.萃淋树脂分离技术的发展及其在湿法冶金分析中的应用[J].湿法冶金,2000,19(1):57-63. 被引量:17

3刘建,胡小玲.磷型萃淋树脂吸附MoO_2^(2+)的扩散动力学研究[J].湿法冶金,1992(4):15-20.

4宋华德.超高功率电炉及相关技术[J].冶金矿山与冶金设备,1996(3):165-171.

5希利琴科,周永益.苏联回收锡的工艺研究和应用[J].金属再生,1989(1):32-33.

6汪学瑶.近代电弧炉的容量和输入功率[J].特殊钢,2000,21(1):19-23. 被引量:1

7田长荫.我国硅铁专用焦的研究和应用[J].铁合金,1989(2):1-9.

8孔宪庭.合理选择铁合金电炉变压器容量的探讨[J].铁合金,1990(4):11-12. 被引量:1

9张盛昌,陈树林,周淑华.提高结晶器寿命的措施[J].河南冶金,2003,11(4):37-38. 被引量:2

10王开力,马廷温,刘建新,宋丽生,王效孔.电炉虹吸出钢法的研究和应用[J].炼钢,1993,9(1):41-45.

Basic Information:

DOI:

Chinese Library Classification Number:TF845.1[冶金工程—有色金属冶金]

Citation Information:

The paper lntroduced research and application of solvent impregnated resin in extraction of scandiumAs a new kind of extractant,solvent impregnated resins can notably improve the capacity and the efficiency of scandium extraction,and is suitable in the ore pulp extraction that the general liquid extraction is hard to apply,indicating its unique good application prospect.

quote

GB/T 7714-2015 [1] JIANG Feng, LI Han-guang. The Application of Solvent Impregnated Resin into Scandium Hydrometallurgy[J]. Rare Metals and Cemented Carbides, 2002(4): 34-38.
MLA [1] JIANG Feng, and LI Han-guang. "The Application of Solvent Impregnated Resin into Scandium Hydrometallurgy." Rare Metals and Cemented Carbides, no. 4, 2002, pp. 34-38.
APA [1] JIANG Feng, & LI Han-guang. (2002). The Application of Solvent Impregnated Resin into Scandium Hydrometallurgy. Rare Metals and Cemented Carbides(4), 34-38.
IEEE [1] JIANG Feng and LI Han-guang, "The Application of Solvent Impregnated Resin into Scandium Hydrometallurgy," Rare Metals and Cemented Carbides, no. 4, pp. 34-38, 2002. keywords: {solvent impregnated resins;scandium;hydrometallurgy;application}