daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Development of Precipitation Phase Research of High-density Tungsten Alloys AITranslate

School of Materials Science and Engineering, Beijing University of Science and Technology;School of Materials Science and Engineering, Beijing University of Science and Technology;School of Materials Science and Engineering, Beijing University of Science and Technology
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

In this paper,the rescent research trend on precipitation phase in tungsten heavy alloys was revieved.At the same time,methods of precipitation strengthening and achievements obtained were also described.In the end some advice on the development of precipitation phase strengthening was proposed.

KeyWords AITranslate

high-density tungsten alloys precipitation strengthening brittleness

1赵幕岳 王伏生 梁容海.高比重合金在国防工业和民用工业中的应用.粉末冶金技术,1983,1(6):20-23.

2范爱国.Ni-Mn体粘结相的烧结W合金.兵器材料科学与工程,1999,5:25-28.

3黄继华,周国安,赖和怡,张滨茹.近十年高比重钨合金强韧化研究动态[J].兵器材料科学与工程,1991(10):38-44. 被引量:9

4曲选辉,毛金英,李志林,李益民,邱光汉.MIM工艺对W-Ni-Fe高密度合金力学性能的影响[J].稀有金属材料与工程,1999,28(3):166-170. 被引量:5

5Williams D J,et al.Production of tungsten-iron-nickel alloys by mechanical alloying technique[J].Powder Metallurgy,1980,(2):92.

6贾成厂,刘小扬,解子章,赵军.用机械活化粉末制备钨合金[J].清华大学学报:自然科学版,1999,39(6):35-38. 被引量:16

7黄继华,张立春,桂晓峰.高Ni/Fe比W-Ni-Fe系重合金烧结行为[J].北京科技大学学报,2000,22(2):149-152. 被引量:5

8Crowson A,et al.Development of fine-grained ductile tungslen alloys for armor/anti-armor applications[P].US Pat AD-A231857.

9Posthill J B,et al.Precipitation at tungsten/tungsten interfaces in tungsten-nickel-iron heavy alloys[J].Powder Metallurgy,1986,29(1):45.

10Edmonds D V,et al.Interfacial Embrittlement in liquid-phase sintered tungsten heavy alloys[J].Metallurgical Transactions A,1979,10A(3):289.

1蔡立辉,刘桂荣,曹靖.高能球磨对WNiFe合金力学性能影响的初步探讨[J].粉末冶金工业,2005,15(3):15-18. 被引量:6

1晏建武,刘莹,彭阿芳,卢全国.Fabrication of nano-crystalline W-Ni-Fe pre-alloyed powders by mechanical alloying technique[J].中国有色金属学会会刊:英文版,2009,0(S3):711-717.

2王季林.钨粉粒度和烧结工艺对高比重钨合金组织结构和力学性能的影响[J].粉末冶金工业,2009,19(2):16-21. 被引量:12

3周伟,高翔,周永贵,罗丰华.95W-5(Ni/Fe)合金的延、脆性断裂行为及热处理影响[J].粉末冶金材料科学与工程,2010,15(2):141-144. 被引量:3

4罗来马,卢泽龙,李浩,罗广南,昝祥,吴玉程.稀土改性钨合金的研究现状与发展趋势[J].稀有金属,2013,37(6):993-1003. 被引量:17

5张陈增,张雪辉,周亮亮,王成,章标,李晓闲,陈颢.稀土CeO_2对W-Ni-Fe高比重合金摩擦磨损性能的影响[J].中国钨业,2016,31(6):18-24.

6张雪辉,周亮亮,李晓闲,张陈增,王成,章标,陈颢,梁彤祥.Y_2O_3对W-4.9Ni-2.1Fe合金摩擦磨损行为的影响[J].材料工程,2017,45(11):115-121. 被引量:4

1张瑞华,胡荣华,聂大.新型萃取剂Cyanex 272在溶剂萃取稀土中的应用[J].稀有金属与硬质合金,1995,23(1):19-24. 被引量:1

2曹妙康.直流电弧炉底电极及其相关技术的发展[J].上海金属,1995,17(2):13-20.

3朱立光,金山同.连铸保护渣研究动态述评[J].连铸,1997,0(5):38-42.

4张晨,刘世洲.去除废钢中的有色金属[J].钢铁研究,1998(3):60-63.

5王应群.金属萃取/湿法冶金的研究动向[J].世界有色金属,1992(4):9-13.

6高建祥,曲选辉,赵赛.金属粉末注射成形技术的最新研究动态与发展趋势[J].硬质合金,2003,20(1):56-60. 被引量:14

7蔡方寒,唐霞辉,秦应雄,李立波,朱国富.金刚石工具用预合金粉末的研究动态[J].金刚石与磨料磨具工程,2004,24(5):77-80. 被引量:25

8张廷安,赫冀成.自蔓延高温合成研究动态[J].中国有色金属学报,1998,8(S2):272-276. 被引量:2

9杜懋华.国外钢锭塑性加工研究动态[J].锡钢科技,1996(17):64-69.

10张晨,刘世洲.脱除废钢中有色金属的研究动态[J].辽宁冶金,1997(4):29-34.

Basic Information:

DOI:

Chinese Library Classification Number:TF125.241[冶金工程—粉末冶金]

Citation Information:

In this paper,the rescent research trend on precipitation phase in tungsten heavy alloys was revieved.At the same time,methods of precipitation strengthening and achievements obtained were also described.In the end some advice on the development of precipitation phase strengthening was proposed.

quote

GB/T 7714-2015 [1] WANG Fu-zhong, LI Rong-hua, FEI Ying. Development of Precipitation Phase Research of High-density Tungsten Alloys[J]. Rare Metals and Cemented Carbides, 2002(4): 39-41.
MLA [1] WANG Fu-zhong, et al., "Development of Precipitation Phase Research of High-density Tungsten Alloys." Rare Metals and Cemented Carbides, no. 4, 2002, pp. 39-41.
APA [1] WANG Fu-zhong, LI Rong-hua, & FEI Ying. (2002). Development of Precipitation Phase Research of High-density Tungsten Alloys. Rare Metals and Cemented Carbides(4), 39-41.
IEEE [1] WANG Fu-zhong, LI Rong-hua, and FEI Ying, "Development of Precipitation Phase Research of High-density Tungsten Alloys," Rare Metals and Cemented Carbides, no. 4, pp. 39-41, 2002. keywords: {high-density tungsten alloys;precipitation strengthening;brittleness}