Preparation of Nanometer Titanium Dioxide Powder AITranslate
Abstract AITranslate
The nanometer anatase TiO2 powder was prepared by hydrolysis and homogeneous precipitation.The most favorable operating conditions were also studied.The morphology,size,crystal shape and specific surface area of nanometer TiO2 powder waere characterized by TEM,XRM,BET and DTA-TG methods.The results show that the TiO2 particle appears spherical shape,the average particle diameter is 20nm,and the specific surface area is 90m2/g.The new technology is simple to operate with low cost and is easy to be industrialized.The obtained nanometer titanium dioxide powder can meet the needs of markets.
KeyWords AITranslate
1袁荞龙,罗宁.国内钛白粉生产、研究及应用进展[J].化工进展,1997,16(5):5-7. 被引量:30
2解宪英.纳米级二氧化钛的制备及其应用进展(下)[J].上海化工,2001,26(5):16-18. 被引量:18
3Haro-poinatowski E,et al.Crystallization of nanosized titania particles prepared by ths sol-gel process[J].J Mater Res,1994,9(8):2 102.
4武瑞涛,魏雨.沸腾回流强迫水解法制备纳米TiO_2微粒[J].无机材料学报,1999,14(3):461-464. 被引量:46
5李晓娥,陈秀娟,张淼,祖庸.醇盐水解制备纳米级二氧化钛[J].稀有金属材料与工程,1995,24(5):65-70. 被引量:19
6徐华蕊,李凤生,陈舒林,宋洪昌.沉淀法制备纳米级粒子的研究——化学原理及影响因素[J].化工进展,1996,15(5):29-31. 被引量:71
7Nakagawa Y,et al.Synthesis of TiO2 and TiN nanosized powders by intense light ion-beam evaporation[J].J Mater Sci,1998,33(1):529.
8赵旭,王子忱,赵敬哲,赵纯,刘艳华,杨少凤,赵慕愚.球形二氧化钛的制备[J].功能材料,2000,31(3):303-305. 被引量:35
1孙家跃,肖昂,杜海燕.均相沉淀-发泡法制备纳米氧化钛的应用研究[J].国外建材科技,2004,25(4):57-59. 被引量:7
2郑典模,陈早明,陈喜蓉.硫酸氧钛液相法制备纳米二氧化钛[J].无机盐工业,2005,37(3):17-19. 被引量:5
3范荣玉.纳米二氧化钛粉体的制备及其在环境保护中的应用[J].南平师专学报,2004,23(2):64-69. 被引量:2
4沈毅,张智丹,沈上越,李珍.二氧化钛微米球形颗粒的制备与研究[J].硅酸盐通报,2005,24(3):96-98. 被引量:10
5孙家跃,肖昂,夏志国,杜海燕.均相沉淀-发泡法制备纳米氧化钛及其表征分析[J].化学世界,2005,46(8):449-452. 被引量:2
6殷立雄,王芬,冯海涛.均匀沉淀法制备纳米粉体的研究的综述[J].陕西科技大学学报:自然科学版,2005,23(6):135-137. 被引量:8
7于延芬,柴立元,彭兵,韦顺文,苏维丰,苑春.用工业钛液制备纳米偏钛酸的影响因素[J].中南大学学报:自然科学版,2006,37(1):52-57. 被引量:6
8郑典模,黄飞来,陈喜蓉,郑建辉.硫酸亚铁液相法制纳米氧化铁的研究[J].化学研究与应用,2006,18(7):840-843. 被引量:6
9王瑞侠,许根水.纳米TiO_2的制备研究[J].池州师专学报,2006,20(5):61-64. 被引量:2
10张凌云,黎汉生,张东翔.用反萃界面沉淀法制备二氧化钛超细粉体[J].材料研究学报,2007,21(2):199-204. 被引量:3
1闫淑梅,傅水香,王鑫,廖涛.纳米二氧化钛的制备及其光催化性能研究[J].环境科学与技术,2007(z1):190-192.
2杜文乐,田鹏,鲁捷,孙露,秦天灵,于超洋.二氧化钛催化超声降解玫瑰红[J].沈阳工程学院学报:自然科学版,2012,8(4):369-371. 被引量:1
3马军委,张海波,董振波,吴雪文,韩团辉.纳米二氧化钛制备方法的研究进展[J].无机盐工业,2006,38(10):5-7. 被引量:28
4王瑞侠,许根水.纳米TiO_2的制备研究[J].池州师专学报,2006,20(5):61-64. 被引量:2
5杨志平,刘玉峰,王利伟,余泉茂,熊志军,徐小岭.用于白光LED的单一基质白光荧光粉Ca_2SiO_3Cl_2:Eu^(2+),Mn^(2+)的发光性质[J].物理学报,2007,56(1):546-550. 被引量:53
6郝晶玉,刘宗怀.纳米二氧化钛光催化剂的研究进展[J].钛工业进展,2007,24(1):36-41. 被引量:13
7唐电,叶城池,邵艳群,王欣.腐蚀液回收制取纳米二氧化钛转变过程[J].材料热处理学报,2007,28(B08):319-322. 被引量:1
8毛爱丽,彭兵,柴立元,王佳,刘立强,游芳,高慧妹.载银纳米TiO_2抗菌竹炭制备工艺研究[J].材料导报,2007,21(F11):229-231. 被引量:4
9杨志平,杨广伟,王少丽,田晶,李盼来,李旭.Sr_5SiO_4Cl_6∶Eu^(2+)蓝白色荧光粉的发光特性研究[J].中国稀土学报,2007,25(6):668-671. 被引量:4
10徐航,张东翔,徐文国.用反萃界面沉淀法制备氧化锌超细粉体[J].功能材料,2008,39(4):673-676. 被引量:1
1汪多仁.纳米二氧化钛粉末的开发与应用进展[J].无机盐技术,2007(3):6-13.
2袁军文,段学臣.纳米二氧化钛粉末的制备[J].硬质合金,2002,19(4):218-220. 被引量:3
3丁延伟,范崇政.纳米二氧化钛表面包覆的研究[J].现代化工,2001,21(7):18-22. 被引量:49
4方世杰,徐明霞,黄卫友,张玉珍.纳米TiO_2光催化降解甲基橙[J].硅酸盐学报,2001,29(5):439-442. 被引量:90
5许海娟.试剂配比对纳米二氧化钛晶型转变温度的影响[J].韶关学院学报,2008,29(3):55-58. 被引量:1
6史晓亮.Photocatalytic Degradation of Rhodamine B Dye with High Purity Anatase Nano-TiO_2 Synthesized by a Hydrothermal Method[J].武汉理工大学学报:材料科学英文版,2011,26(4):600-605. 被引量:2
7蒋玉龙,王智宇,唐培松,钱国栋,樊先平.量子尺寸纳米TiO_2的水热制备及光催化性能[J].浙江大学学报:工学版,2005,39(3):440-444. 被引量:19
8严安,刘泽华,苗冉冉.不同粒径的二氧化钛对甲基红的光催化降解[J].杭州化工,2009,39(4):16-19. 被引量:4
9刘朝晖,杨怀霞,沈新元,董会超,温丽.纳米TiO_2的制备研究进展[J].河南化工,2002,21(8):3-5. 被引量:9
10孙悦,任铁强,乔庆东.溶胶凝胶水热法制备Fe^(3+)掺杂纳米TiO_2的应用研究[J].化学与粘合,2014,36(1):46-49. 被引量:1
Basic Information:
DOI:
Chinese Library Classification Number:TQ134.11[化学工程—无机化工];TF1[冶金工程—冶金物理化学]
Citation Information:
The nanometer anatase TiO2 powder was prepared by hydrolysis and homogeneous precipitation.The most favorable operating conditions were also studied.The morphology,size,crystal shape and specific surface area of nanometer TiO2 powder waere characterized by TEM,XRM,BET and DTA-TG methods.The results show that the TiO2 particle appears spherical shape,the average particle diameter is 20nm,and the specific surface area is 90m2/g.The new technology is simple to operate with low cost and is easy to be industrialized.The obtained nanometer titanium dioxide powder can meet the needs of markets.
quote
| GB/T 7714-2015 | [1] DUAN Xue-chen, GAO Gui-lan, WU Xiang-wei, et al. Preparation of Nanometer Titanium Dioxide Powder[J]. Rare Metals and Cemented Carbides, 2002(4): 17-30. |
| MLA | [1] DUAN Xue-chen, et al., "Preparation of Nanometer Titanium Dioxide Powder." Rare Metals and Cemented Carbides, no. 4, 2002, pp. 17-30. |
| APA | [1] DUAN Xue-chen, GAO Gui-lan, WU Xiang-wei, & YANG Xiang-ping. (2002). Preparation of Nanometer Titanium Dioxide Powder. Rare Metals and Cemented Carbides(4), 17-30. |
| IEEE | [1] DUAN Xue-chen, GAO Gui-lan, WU Xiang-wei, and YANG Xiang-ping, "Preparation of Nanometer Titanium Dioxide Powder," Rare Metals and Cemented Carbides, no. 4, pp. 17-30, 2002. keywords: {nanometer titanium dioxide;hydrolysis;homogeneous precipitation} |