Present Status of the W Consumption and Prediction of W Demand AITranslate

Changsha Nonferrous Metallurgical Design Research Institute;Changsha Nonferrous Metallurgical Design Research Institute
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The paper describes and analyzes the W Consumption and demand in recent years both at home and abroad.Preliminary prediction is made of W consumption trend and market demand.

KeyWords AITranslate

W consumption consumption trend demand prediction

1王明明,王琨琳.加强钨业管理 应对入世挑战[J].中国钨业,2002,17(1):6-10. 被引量:1

2Micheal Maby.国际钨协第14届年会市场报告[J].中国钨业,2001,16(5):129-134. 被引量:1

3郭声琨.浅谈我国钨业经济增长方式的转变[J].中国钨业,1996,0(6):1-2. 被引量:1

1文博杰,陈毓川,王高尚,代涛.2035年中国能源与矿产资源需求展望[J].中国工程科学,2019,21(1):68-73. 被引量:26

1任晓娟,范凤岩,柳群义,樊礼军.中国铝土矿的供应安全评价[J].中国矿业,2019,28(7):52-59. 被引量:12

2周艳晶,梁海峰,李建武,王高尚.钴资源供需格局及全球布局研究[J].中国矿业,2019,28(7):65-69. 被引量:13

3万倩,肖浩南,钱京,何正斌,伊松林.泡沫铁对石蜡相变储热过程的影响[J].储能科学与技术,2020,9(1):44-50. 被引量:11

4李敬,张寿庭,商朋强,赵玉.萤石资源现状及战略性价值分析[J].矿产保护与利用,2019,39(6):62-68. 被引量:37

5田金梁.萤石在某化工公司的使用研究[J].当代化工研究,2020(15):58-59.

6高印,杜婷婷.铝电解过剩电解质产生原因及利用方法探讨[J].世界有色金属,2020(16):10-11.

7麻衡,徐凯,孙乾.我国煤机液压支架用高强钢的生产现状与发展趋势[J].轧钢,2020,37(6):71-76. 被引量:7

8杨建锋,余韵,马腾,张翠光,王泉.工业革命驱动下能源与金属资源需求演变特征与前景分析[J].中国人口·资源与环境,2020,30(12):45-54. 被引量:7

9李晓峰,朱艺婷,徐净.关键矿产资源铟研究进展[J].科学通报,2020,65(33):3678-3687. 被引量:13

10王琨,陈其慎,张艳飞,王芳,邢佳韵,郑国栋,龙涛,张涛,崔博京.海外铜矿投资项目的一种综合评价方法探讨——以非洲为例[J].地球学报,2021,42(2):229-235. 被引量:2

1张帆.中国的粮食消费与需求[J].管理世界,1998(4):186-196. 被引量:9

2于晓霞.拉动农村经济发展促进农村居民消费与需求[J].南北桥,2009(1).

3魏晓露,么伟伟,邸丽霞.河北省旅游服务业人才现状及需求预测[J].中国外资,2010(20):228-228.

4周福根.国内外环氧树脂现状及需求预测[J].中国涂料,2000,15(2):44-48. 被引量:9

5陈永军.辽宁港口集装箱运输发展现状及需求预测[J].中国港口,2006(10):28-30. 被引量:1

6尹强.服务业发展水平影响因素分析[J].消费导刊,2013(2):20-20.

7广东省城乡贫困家庭青少年现状及需求调查问卷2[J].黄金时代:下半月,2016,0(10):80-80.

8杜延杰,雷志敏.中国铁矿石进口现状及需求形式浅析[J].商场现代化,2009(19):11-13. 被引量:1

9罗正霞.青海省旅游商品需求特征分析与开发策略[J].青海科技,2008,15(1):8-10. 被引量:1

10王鑫,王爱华.我国燃料油现货市场的状况[J].价值工程,2007,26(3):126-128. 被引量:1

Basic Information:

DOI:

Chinese Library Classification Number:F764.2[经济管理—产业经济]

Citation Information:

The paper describes and analyzes the W Consumption and demand in recent years both at home and abroad.Preliminary prediction is made of W consumption trend and market demand.

quote

GB/T 7714-2015 [1] YI Xiao-jian, LIU Meng-qi. Present Status of the W Consumption and Prediction of W Demand[J]. Rare Metals and Cemented Carbides, 2002(4): 51-53.
MLA [1] YI Xiao-jian, and LIU Meng-qi. "Present Status of the W Consumption and Prediction of W Demand." Rare Metals and Cemented Carbides, no. 4, 2002, pp. 51-53.
APA [1] YI Xiao-jian, & LIU Meng-qi. (2002). Present Status of the W Consumption and Prediction of W Demand. Rare Metals and Cemented Carbides(4), 51-53.
IEEE [1] YI Xiao-jian and LIU Meng-qi, "Present Status of the W Consumption and Prediction of W Demand," Rare Metals and Cemented Carbides, no. 4, pp. 51-53, 2002. keywords: {W consumption;consumption trend;demand prediction}