Abstract AITranslate

In this article,review is made of the present status of application of cast Ti and Ti alloy in dentistry.

KeyWords AITranslate

titanium titanium alloy casting dentistry

1Lautenschlager E P,et al.Titanium and titanium alloys as dental materials[J].International Dental Journal.1993,43:245.

2Okabe T,et al.The use of titanium in dentastrg[J].Cells and Materials,1995,5:211.

3Nakajima H,et al.Titanium in dentistry:Development and research in the USA[J].Dental Materials Journal,1996,15:77.

4Takada Y,et al.Evaluation of binarg metastable β titanium alloys for dental application[J].J of Dental Research,1997,76:402.

5Watanabe I,et al.Castability of titanium and dental alloys[J].J Dental Research,1997,76:402.

6Okabe J,et al.Dental Castiging of Titanium Alloys,Non-Aerospace Applications of Titanium[M].War rendale,Pennsylrania:TMS,1998.207.

7黄虹.钛及其合金的非航空航天用途[J].稀有金属与硬质合金,2001,29(3):46-49. 被引量:8

1蔡建宾,吴宇建,张冬冬,戴品强.Al_(0.5)CoCrFeNiB_x多主元高熵合金的组织结构和力学性能[J].稀有金属与硬质合金,2011,39(4):37-40. 被引量:11

2费阳,汪涛,缪润杰,王倩,袁揭.微量氧含量对Ti-3Zr合金微观组织与力学性能的影响[J].稀有金属与硬质合金,2019,47(6):52-58.

3原晨岩,潘一帆,崔红力,史文祥.常见铸造钛合金性能及在阀门行业的应用[J].科技创新与应用,2022,12(31):162-164.

1彭存远,马明星,叶晓阳,吴绮雯,张伟明,刘文今.添加Mn对激光制备Al_(1.3)FeCoNiCuCr涂层组织和性能的影响[J].应用激光,2014,34(3):175-180. 被引量:8

2安旭龙,刘其斌,郑波.碳化钨对激光熔覆高熵合金的影响[J].强激光与粒子束,2014,26(12):249-254. 被引量:15

3李栋梁,周芳,余师豪.激光熔覆FeCrNiMnMo_xB_(0.5)高熵合金涂层组织与耐蚀性能[J].强激光与粒子束,2016,28(2):190-195. 被引量:18

4饶湖常,戴品强,陈鼎宁,王乾廷.碳含量对FeCoCrNiMnC_x高熵合金显微组织与性能的影响[J].机械工程材料,2016,40(8):76-80. 被引量:10

5李涵,马玲玲,位超群,孙琳,张维平.钛合金表面激光熔覆AlB_xCoCrNiTi高熵合金涂层的组织与性能[J].表面技术,2017,46(6):226-231. 被引量:28

6黄纯可,李伟,刘平,张柯,马凤仓,刘新宽,陈小红,何代华.磁控溅射法制备Al_xCoCrFeNi高熵合金薄膜的微观组织和力学性能研究[J].功能材料,2017,48(6):6144-6148. 被引量:17

7李安敏,史君佐,谢明款.高熵合金力学性能的研究进展[J].材料导报,2018,32(3):461-466. 被引量:13

8谢亚茜,陈业新,马星星.硼含量对FeCoNiCrAl_(0.1)B_(x)高熵合金组织和力学性能的作用[J].上海大学学报:自然科学版,2021,27(2):280-288. 被引量:1

9李荣斌,邹传乐,张志玺,张如林,彭望君.硼对铸态Al_(0.3)CoCrFeNi高熵合金组织及性能的影响[J].稀有金属材料与工程,2023,52(2):667-674.

10赵森林,陈希章.Al_(1.2)Co_(x)CrFeNi高熵合金的相形成规律及其力学性能[J].材料工程,2023,51(5):104-111.

1阎蕴琪.硼对齿科用铸造Ti合金的组织与力学性能的影响[J].稀有金属快报,2003(11):26-28. 被引量:2

2吴全兴.牙科用贵金属合金的现状和未来[J].稀有金属快报,2003(9):1-1.

3张新平,于思荣,何镇明,韩秋华.新型Ti-Fe-Mo-Mn-Nb-Zr系钛合金的力学性能[J].中国有色金属学报,2002,12(z1):78-82. 被引量:14

421世纪的牙科医疗发展方向[J].吉林医学情报,1992(2).

5张新平,于思荣,夏连杰,何镇明.钛及钛合金在牙科领域中的研究现状[J].稀有金属材料与工程,2002,31(4):246-251. 被引量:29

6赵西成,兰新哲,尚再燕.两种牙科贵金属铸造合金的组织结构研究[J].贵金属,2001,22(4):13-16. 被引量:2

7吴全兴.日本钢铁协会第145次大会报告[J].稀有金属快报,2003(12):26-27.

8开头记忆合金在人体上的应用[J].稀有金属快报,2000(6):1-2.

9孙序,何勇健.新型Ti-Ni牙齿矫形丝的相变[J].稀有金属,1996,20(5):386-388.

10余彤,李颖超,刘洪臣,宫琦玮.老年人牙根纵裂病因探讨[J].军医进修学院学报,2002,23(2):156-157. 被引量:1

Basic Information:

DOI:

Chinese Library Classification Number:R783.1[医药卫生—口腔医学];TG146[金属学及工艺—金属材料]

Citation Information:

In this article,review is made of the present status of application of cast Ti and Ti alloy in dentistry.

quote

GB/T 7714-2015 [1] QIN Chuan. Application of Cast Titanium and Ti Alloys in Dentistry[J]. Rare Metals and Cemented Carbides, 2002(4): 54-56.
MLA [1] QIN Chuan. "Application of Cast Titanium and Ti Alloys in Dentistry." Rare Metals and Cemented Carbides, no. 4, 2002, pp. 54-56.
APA [1] QIN Chuan. (2002). Application of Cast Titanium and Ti Alloys in Dentistry. Rare Metals and Cemented Carbides(4), 54-56.
IEEE [1] QIN Chuan, "Application of Cast Titanium and Ti Alloys in Dentistry," Rare Metals and Cemented Carbides, no. 4, pp. 54-56, 2002. keywords: {titanium;titanium alloy;casting;dentistry}