Research on the Relationship between the Coercive Force and Maximum Sintering Temperature of WC-Co Cemented Carbides
Rare Metals and Cemented Carbides | Vol., Issue 2, 2007 |
pp. 18-20
The factors that affect the coercive force of cemented carbides are analyzed theoretically. Under high-temperate operation mode and actual operation mode,the coercive force is mainly relatedto the maximal sintering temperature. Research is carried out on the high temperature field of PVA sintering furnace. Data processing and analysis is done to obtain the quantitative relationship between coercive force and maximal sintering temperature.
DOI: Cited: 0 Download: 0