Research and Application of External Magnetic Field in the Directional Solidification AITranslate
Abstract AITranslate
In view of the influence of magnetic field on the solidified structure, the paper reviews the latest application and development of alternating and steady magnetic fields during directional solidification, and summarized the microstructure action mechanism of the external magnetic field indirectional solidification. The future development directionis also prospected.
KeyWords AITranslate
1王晖,任忠鸣,蒋国昌.均恒强磁场在材料科学中的应用[J].材料科学与工程,2001,19(2):119-123. 被引量:30
2王强,王恩刚,赫冀成.静磁场在材料生产过程中的应用研究评述[J].材料科学与工程学报,2003,21(4):590-595. 被引量:26
3李双明,郝启堂,李金山,寇宏超,傅恒志,贾均,郭景杰.交变电磁场下金属熔体的电磁约束连续成形与凝固[J].材料导报,2001,15(3):10-12. 被引量:7
4苏彦庆,郭景哲,刘畅,郭景杰,贾均,傅恒志.定向凝固技术与理论研究的进展[J].特种铸造及有色合金,2006,26(1):25-30. 被引量:39
5沈军.电磁约束成形过程研究[D].西安:西北工业大学,1997.
6李新涛,李丘林,李廷举,宋艳琴,张金利,金俊泽.电磁场对水平连铸紫铜管表面质量及组织性能的影响[J].中国有色金属学报,2004,14(12):2060-2065. 被引量:21
7王建元,陈长乐,孟小华.旋转磁场作用下Pb-Sn合金的凝固行为[J].材料导报,2006,20(3):152-154. 被引量:6
8Nikrityuk P A, Eckert K, Grundmann R. A numerical study of directional solidification of binary metal alloy under influence of a rotatingmagnetic field[J]. Heat and Mass transfer,2006,49:1 501-1 511.
9Willers B, Eckert S, Michel U,et al. The columnar-to-equiaxed transition in Pb-Sn alloys affected by electromagnetically driven convection[J]. Materials Science and Engineering, 2005,402A : 55-65.
10Steinbach S, Ratke L. The effect of rotating magnetic fields on the microstructure of directionally solidified Al-Si-Mg alloys[J]. Materials Science and Engineering, 2005,413A : 200-204.
1翟富刚,张庆,付宇明,李娟.交变磁处理对金刚石锯片切割性能的影响[J].金刚石与磨料磨具工程,2008,28(6):31-36. 被引量:1
1杨晓军,唐营,杨乐乐,王前进.金刚石锯片锋利性试验分析[J].科技创新与应用,2015,5(15):50-50. 被引量:2
1龚锋,沈军,刘林,傅恒志.定向凝固过程流动、传热、传质的耦合数值模拟-Ⅰ数学模型[J].自然科学进展,2006,16(8):1038-1041. 被引量:2
2李梅娥,杨根仓,周尧和.二元合金高速定向凝固过程的相场法数值模拟[J].物理学报,2005,54(1):454-459. 被引量:26
3牛晓武,赵志龙,刘林.Al-Cu合金定向凝固脉冲磁场分布数值模拟[J].机械设计与制造,2006(6):75-77.
4郭春文,李俊杰,马渊,王锦程.定向凝固过程中枝晶侧向分枝生长行为与强制调控规律[J].物理学报,2015,64(14):329-336. 被引量:6
5刘晓华,郭喜平,介万奇,周尧和.定向凝固过程中的溶质径向分凝[J].材料研究学报,1998,12(2):123-127. 被引量:4
6王志军,王锦程,杨根仓.各向异性作用下合金定向凝固界面稳定性的渐近分析[J].物理学报,2008,57(2):1246-1253. 被引量:11
7朱鸣芳,陈晋,孙国雄,洪俊杓.枝晶生长的数值模拟[J].金属学报,2005,41(6):583-587. 被引量:19
8吴伟,孙东科,戴挺,朱鸣芳.枝晶生长和气泡形成的数值模拟[J].物理学报,2012,61(15):39-47. 被引量:9
9刘俊成.ACRT强迫对流对定向凝固过程传热传质的影响[J].自然科学进展,2003,13(12):1293-1300. 被引量:6
10曹海涛,胡锐,寇宏超,马丽,马晓勇,高恩志,周廉.限制定向凝固法制备YBCO超导体单畴生长的分析[J].稀有金属材料与工程,2007,36(1):166-169.
Basic Information:
DOI:
Chinese Library Classification Number:O482.5[理学—固体物理];TG249.9[金属学及工艺—铸造]
Citation Information:
In view of the influence of magnetic field on the solidified structure, the paper reviews the latest application and development of alternating and steady magnetic fields during directional solidification, and summarized the microstructure action mechanism of the external magnetic field indirectional solidification. The future development directionis also prospected.
quote
| GB/T 7714-2015 | [1] LI Qing-lin, WU Chun-yan. Research and Application of External Magnetic Field in the Directional Solidification[J]. Rare Metals and Cemented Carbides, 2007(2): 44-47. |
| MLA | [1] LI Qing-lin, and WU Chun-yan. "Research and Application of External Magnetic Field in the Directional Solidification." Rare Metals and Cemented Carbides, no. 2, 2007, pp. 44-47. |
| APA | [1] LI Qing-lin, & WU Chun-yan. (2007). Research and Application of External Magnetic Field in the Directional Solidification. Rare Metals and Cemented Carbides(2), 44-47. |
| IEEE | [1] LI Qing-lin and WU Chun-yan, "Research and Application of External Magnetic Field in the Directional Solidification," Rare Metals and Cemented Carbides, no. 2, pp. 44-47, 2007. keywords: {external magnetic field;directional solidification;application and research;microstructure;action mechanism} |