The latest Development of Sm_2Fe17N_x Rare-earth Permanent Magnetic Material AITranslate

School of Metallurgical Science and Engineering, Central South University;School of Metallurgical Science and Engineering, Central South University
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

In this paper, the crystal structure, the intrinsic magnetism, and the relationship between magnetic properties and the number of N atoms of rare-earth permanent magnetic material are briefly analyzed. Meanwhile,the methods and existing problems of preparing Sm2 Fe17Nx permanent magnetic material are especially described. Finally,the latest development and future development trend of the said material are pointed out.

KeyWords AITranslate

Sm2 Fe17 Nx rare-earth permanent magnetic material preparation process latest development

1Coey J M D, Hong Sun. Improved magnetic properties by treatment of iron-based rare earth intermetallic compounds in ammonia [J]. Magnetism and Magnetic Materials, 1990,87(3) :251-254.

2席生歧,周敬恩,王笑天.Sm_2Fe_(17)N_x永磁材料研制进展[J].稀有金属材料与工程,1994,23(5):14-18. 被引量:11

3Hong Sun,Coey J M D,Dtani Y,et al. Magnetic properties of a new Series of rare earth iron nitrides:R2 Felt Ny (y-2.6)[J].J Phys:Condens Matters,1992,2:6 465.

4Iriyama T, Kobayashi K, Imaoka N, et al. Effect of nitrogen content on magnetic properties of Sin2Fe17Nx(0< 6)[J]. IEEE Trans Magn,1992,28(5):2 326-2 331.

5Wei Y N,Sun K,Fen Y B. Structural and intrinsic magnetic properties of Sm2 Fe17Ny (y = 2-8) [J]. Alloys and Compounds, 1993,194(1) :9-12.

6居毅,李宗权.机械合金化的原理及在磁性材料研究中的应用[J].功能材料,2002,33(1):12-14. 被引量:21

7Kuhrt C, Schnitzke K, Wecker J, et al. Ti-substituted hard magnetic mechanically alloyed Sm2Fe17Nx[J]. IEEE Trans Magn,1993,29(6):2 818-2 820.

8周寿增 董清飞.稀土永磁材料及其应用[M].北京:冶金工业出版社,1995.77-78.

9Katter M, Wecker J, chultz S L. Structural and hard magnetic properties of rapidly solidified Sm-Fe-N [J]. Appl Phys, 1991,70(7) :3 188-3 193.

10Zhou Shouzeng, Yan Jun, Zhang Maocao, et al. The Preparation and Magnetic Properties of Sm2 (Fe1-xMx)17Nx Powder with High Performance[R]. Canberra:Proc 12^t/h Int Workshop on Rare Earth Manets and Their Applicattion, 1992.44.

1邓庚凤,何桂荣,邓华军,黄崛起.还原扩散法制备钐铁氮磁性材料的组织结构与性能研究[J].中国稀土学报,2010,28(6):676-679. 被引量:5

2李大勇,段焕强.钐铁氮稀土永磁材料产业化进展[J].中国新技术新产品,2012(20):146-148. 被引量:17

3王书桓,张凯璇,赵定国,宋春燕,柳昆.高压环境雾化钐铁液滴冷却过程的研究[J].铸造技术,2017,38(3):617-621. 被引量:1

4王书桓,袁亮亮,赵定国,高爱民,宋春燕,李彬.Sm_2Fe_(17)型合金氮化工艺的研究进展[J].中国稀土学报,2017,35(3):315-321. 被引量:9

5宋春燕,程世伟,王书桓,赵定国,胡利光.铜模喷铸对钐铁合金组织形貌及物相组成的影响[J].稀有金属与硬质合金,2019,47(5):37-42.

6宋春燕,程世伟,王书桓,赵定国,胡利光.Sm2Fe17N3晶体的价电子结构分析和结合能、最强键能计算[J].中国稀土学报,2020,38(1):46-52.

7柳昆,王书桓,张一昆,李博海.钐铁合金感应熔炼实验参数的探究[J].稀有金属与硬质合金,2020,48(2):35-40.

8宋春燕,胡利光,王书桓,赵定国.Sm2Fe17的价电子结构及性能研究[J].稀有金属,2019,0(5):551-555. 被引量:3

1袁亮亮,高爱民,马海涛,王书桓,赵定国.钐铁熔体底吹氮气工艺中气泡的形成机理[J].稀土,2018,39(6):28-33. 被引量:1

2潘贤斌,邓庚凤,姬传红,吴继平,邓亮亮.超声波辅助共沉淀法制备钐铁复合氧化物粉体[J].有色金属科学与工程,2016,7(5):7-12. 被引量:3

3周林,李宗安,陈德宏,王志强,庞思明,赵斌.LiF-CaF_2-SmF_3体系熔盐电解制备SmFe合金的电化学机制研究[J].稀有金属,2017,41(2):190-195. 被引量:4

4王书桓,张凯璇,赵定国,宋春燕,柳昆.高压环境雾化钐铁液滴冷却过程的研究[J].铸造技术,2017,38(3):617-621. 被引量:1

5王书桓,张凯璇,方云楚,宋春燕,赵定国.钐铁熔体高压雾化氮淬过程的数值模拟[J].中国粉体技术,2017,23(4):17-21.

6胡国辉,朱代漫,高俊彦,张威峰,熊君,贾立颖,王倩,孙威,刘荣明,李炳山.高性能Sm_2Fe_(17)N_3永磁粉末的还原扩散工艺研究[J].金属功能材料,2017,24(5):17-21. 被引量:1

7张世勇,刘竞艳,李望,任永军,温和瑞.铬酸根作为抗衡离子的钕18-冠-6配合物的合成与晶体结构[J].中国稀土学报,2018,36(1):86-92. 被引量:1

8王书桓,崔少璞,孙鑫,赵定国,方云楚,宋春燕.钐铁熔体雾化过程中雾化角度的数值模拟[J].钢铁钒钛,2018,39(1):155-159.

9高爱民,袁亮亮,马海涛,王书桓,赵定国.钐铁合金熔体渗氮中主要影响因素的研究[J].中国稀土学报,2018,36(3):308-313. 被引量:3

10袁亮亮,高爱民,马海涛,王书桓.钐铁合金熔体渗氮实验研究[J].稀有金属与硬质合金,2018,46(3):29-34. 被引量:1

1李杰民,崔春翔,韩瑞平.Sm_2Fe_(17)N_x永磁体的商品化现状和发展趋势[J].金属功能材料,2002,9(4):11-14. 被引量:12

2郑青.稀土永磁体Sm_2Fe_(17)N_x的制备方法研究进展[J].科技视界,2013(29):121-121. 被引量:1

3廖恒成,孙国雄.永磁材料的进展[J].机械工程材料,1999,23(1):1-5. 被引量:5

4邓庚凤,孙光飞,陈菊芳,胡国辉,方克明.Sm_2Fe_(17)N_x永磁材料的研究进展[J].材料导报,2004,18(12):37-40. 被引量:2

5林国标,王显荣,于一公,尹有祥,于申军,周寿增.低温氢处理对制取Sm_2Fe_(17)N_x的作用[J].有色金属:冶炼部分,1996(1):48-48. 被引量:4

6林才顺,王新东,王淑燕,马立军.微型直接甲醇燃料电池的研究现状及进展[J].湿法冶金,2007,26(1):22-24.

7张然,刘颖,李芳,高升吉,涂铭旌.Sm_2Fe_(17)合金的氮化处理及其相关影响[J].磁性材料及器件,2004,35(2):39-41. 被引量:4

8王小红,刘颖,叶金文,涂铭旌.合金元素对Sm_2Fe_(17)N_x微观结构和性能的影响[J].材料导报,2007,21(F05):304-306. 被引量:2

9席生歧,周敬恩,王笑天.Sm_2Fe_(17)N_x永磁材料研制进展[J].稀有金属材料与工程,1994,23(5):14-18. 被引量:11

10张东涛,岳明,姬永成,张久兴.高性能Sm_2Fe_(17)N_x磁粉制备关键技术研究[J].功能材料与器件学报,2004,10(4):446-450. 被引量:7

Basic Information:

DOI:

Chinese Library Classification Number:TM273[一般工业技术—材料科学与工程]

Citation Information:

In this paper, the crystal structure, the intrinsic magnetism, and the relationship between magnetic properties and the number of N atoms of rare-earth permanent magnetic material are briefly analyzed. Meanwhile,the methods and existing problems of preparing Sm2 Fe17Nx permanent magnetic material are especially described. Finally,the latest development and future development trend of the said material are pointed out.

quote

GB/T 7714-2015 [1] XUE Ping, GUO Xue-yi. The latest Development of Sm_2Fe17N_x Rare-earth Permanent Magnetic Material[J]. Rare Metals and Cemented Carbides, 2007(2): 53-57.
MLA [1] XUE Ping, and GUO Xue-yi. "The latest Development of Sm_2Fe17N_x Rare-earth Permanent Magnetic Material." Rare Metals and Cemented Carbides, no. 2, 2007, pp. 53-57.
APA [1] XUE Ping, & GUO Xue-yi. (2007). The latest Development of Sm_2Fe17N_x Rare-earth Permanent Magnetic Material. Rare Metals and Cemented Carbides(2), 53-57.
IEEE [1] XUE Ping and GUO Xue-yi, "The latest Development of Sm_2Fe17N_x Rare-earth Permanent Magnetic Material," Rare Metals and Cemented Carbides, no. 2, pp. 53-57, 2007. keywords: {Sm2 Fe17 Nx;rare-earth permanent magnetic material;preparation process;latest development}