daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

In and Ge Integrate Recovery during Zn Metallurgy AITranslate

Changsha Nonferrous Metallurgical Design Research Institute;Changsha Nonferrous Metallurgical Design Research Institute
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The article discusses the distribution, enrichment and integrate recovery of In and Ge in Zn metallurgy with I. S. P or hot-acid-leaching process. It is pointed out that the use of pressure leaching of Zn concentrate can directly enrich sornemetal values such as Zn, In and Ge, during Zn extraction with large leaching rate and recovery.

KeyWords AITranslate

zinc metallurgy indium germanium pressure leaching integrate recovery

1吴成春.提锗工艺的技术改造[J].有色金属:冶炼部分,2005(3):36-39. 被引量:6

2王吉坤,何蔼平.现代锗冶金[M].北京:冶金工业出版社,2006.

3北京有色冶金设计研究总院.重有色金属冶炼设计手册(铅锌铋卷)[M].北京:冶金工业出版社,1996.

1俞小花,谢刚,李永刚,刘春侠,刘康.含铟硫酸浸出液中铟的富集[J].中国有色金属学报,2008,18(E01):121-125. 被引量:7

2袁铁锤,宁顺明,陈志飞,周科朝.从高铟锌精矿中综合回收锌和铟[J].湖南有色金属,2008,24(1):27-28. 被引量:5

3许冬,阮胜寿,贾荣,朱军.锌冶炼废渣中铟回收技术综述[J].材料研究与应用,2009,3(4):231-233. 被引量:18

4刘厚凡,史爱芹,周新木,潘庆辉,王素敏.硫酸体系中P507对铟锌锰的萃取分离研究[J].无机盐工业,2010,42(3):20-22. 被引量:7

5代淑娟,孟宇群,胡志刚,白丽梅.某窑渣中炭的浮选回收试验研究[J].矿业研究与开发,2010,30(4):30-32.

6高远,赖复兴,吴斌秀,吴成春,王坚,王继民,陈少纯.盐酸体系N503萃取分离回收铟[J].有色金属:冶炼部分,2012(1):35-38. 被引量:6

7何静,王小能,鲁君乐,罗超,王涛.含铟低酸浸出液中富集铟的研究[J].矿冶工程,2012,32(1):77-80. 被引量:9

8沈丽娟,吴克明,袁芳沁,高耀文.锌冶炼过程中铟的富集与回收技术研究进展[J].矿产综合利用,2012(4):3-6. 被引量:17

9蒋文龙,杨斌,戴永年.从火法炼锌炉底积铁中回收银和铟的研究[J].昆明理工大学学报:自然科学版,2014,39(3):1-4. 被引量:4

10杨永强,王成彦,杨玮娇,袁文辉,邢鹏.锌烟灰焙砂浸出铟、锗、锌的研究[J].有色金属:冶炼部分,2014(7):11-13. 被引量:7

1何纯田,罗昆旭,吕留彦.贵州省威宁县哲觉镇典型土法炼锌堆渣场环境污染评价[J].冶金管理,2021(15):176-177.

2杨大锦.2008年云南冶金年评[J].云南冶金,2009,38(2):36-53.

3周存,何静,唐谟堂,吴胜男.锌焙砂还原浸出液中和沉铟及净化工艺研究[J].化学工程与装备,2010(2):5-8. 被引量:3

4黎红兵,周志辉,陈志飞,宁顺民,袁铁锤.黄钾铁矾法炼锌的沉矾过程研究[J].湖南有色金属,2010,26(4):27-29. 被引量:10

5代淑娟,孟宇群,胡志刚,白丽梅.某窑渣中炭的浮选回收试验研究[J].矿业研究与开发,2010,30(4):30-32.

6孙进贺,贾永忠,景燕,王小华,孟宪党,徐跃伟.P204-Cyanex 923磺化煤油用于铟的萃取和反萃研究[J].有色金属:冶炼部分,2011(1):26-28. 被引量:10

7姚芝茂,赵丽娜,徐成.锌冶炼工业有价金属回收潜力与现状分析[J].中国有色冶金,2011,40(1):49-54. 被引量:13

8周升福.铜厂采区黄牛前临近固定边坡爆破实践[J].铜业工程,2011(1):20-22. 被引量:1

9伍赠玲.铟的资源、应用与分离回收技术研究进展[J].铜业工程,2011(1):25-30. 被引量:24

10班双,王林生,李敏.锂云母浸出母液的萃取除杂试验研究[J].世界有色金属,2011(12):44-46.

1邓孟俐,谢冰.锌冶炼工艺过程中铟、锗的综合回收[J].工程设计与研究(长沙),2007(2):1-3.

2陈阜东.硫化锌精矿加压氧浸回收有价金属的工艺[J].铜业工程,2015(4):71-74. 被引量:4

3曹耀华,高照国,刘红召,王威.从某低品位金钼粗精矿中浸出金、钼试验研究[J].湿法冶金,2014,33(5):339-342. 被引量:2

4王令明.硫化锌精矿加压氧浸的矿浆降温降压冷却方法[J].铜业工程,2016(1):68-70.

5仝一喆,陈龙义.硫化锌精矿加压氧浸工艺的酸平衡分析[J].湖南有色金属,2012,28(2):38-39. 被引量:2

6李东波,蒋继穆.国内外锌冶炼技术现状和发展趋势[J].中国金属通报,2015,0(6):44-46. 被引量:10

7曹康学,李少龙,邓涛,洪钰,张诗光,郑继祖.艾妙电解技术在高镍锍加压氧浸液中脱铜的试验研究[J].中国有色冶金,2011,40(4):63-65. 被引量:2

8李允斌.一种硫化锌精矿加压氧浸的蒸汽加热方法[J].铜业工程,2015(6):26-27.

9谢冰.湿法炼锌工艺过程除铁技术的发展[J].矿冶工程,2012,32(2):100-102. 被引量:16

10王令明.一种用于湿法锌冶炼清洁生产的高效除铁方法[J].铜业工程,2014(6):19-21. 被引量:3

Basic Information:

DOI:

Chinese Library Classification Number:TF843[冶金工程—有色金属冶金]

Citation Information:

The article discusses the distribution, enrichment and integrate recovery of In and Ge in Zn metallurgy with I. S. P or hot-acid-leaching process. It is pointed out that the use of pressure leaching of Zn concentrate can directly enrich sornemetal values such as Zn, In and Ge, during Zn extraction with large leaching rate and recovery.

quote

GB/T 7714-2015 [1] DENG Meng-li, XIE Bing. In and Ge Integrate Recovery during Zn Metallurgy[J]. Rare Metals and Cemented Carbides, 2007(2): 21-24.
MLA [1] DENG Meng-li, and XIE Bing. "In and Ge Integrate Recovery during Zn Metallurgy." Rare Metals and Cemented Carbides, no. 2, 2007, pp. 21-24.
APA [1] DENG Meng-li, & XIE Bing. (2007). In and Ge Integrate Recovery during Zn Metallurgy. Rare Metals and Cemented Carbides(2), 21-24.
IEEE [1] DENG Meng-li and XIE Bing, "In and Ge Integrate Recovery during Zn Metallurgy," Rare Metals and Cemented Carbides, no. 2, pp. 21-24, 2007. keywords: {zinc metallurgy;indium;germanium;pressure leaching;integrate recovery}