daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Research on the Relationship between the Coercive Force and Maximum Sintering Temperature of WC-Co Cemented Carbides AITranslate

School of Energy Science and Engineering, Central South University;School of Energy Science and Engineering, Central South University;School of Energy Science and Engineering, Central South University
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The factors that affect the coercive force of cemented carbides are analyzed theoretically. Under high-temperate operation mode and actual operation mode,the coercive force is mainly relatedto the maximal sintering temperature. Research is carried out on the high temperature field of PVA sintering furnace. Data processing and analysis is done to obtain the quantitative relationship between coercive force and maximal sintering temperature.

KeyWords AITranslate

WC-Co cemented carbides coercive force sintering temperature

1刘永福.硬质合金的烧结气氛及其控制[J].硬质合金,1996,13(3):176-179. 被引量:18

2洪溵程,李学芳.硬质合金氢气烧结的变形机理及其控制[J].硬质合金,2000,17(3):156-160. 被引量:8

3刘寿荣.WC-Co硬质合金的矫顽磁力[J].中国有色金属学报,1995,5(2):132-134. 被引量:22

4王国栋.硬质合金烧结原理[M].北京:冶金工业出版社(第一版),1988.

5刘寿荣,郝建民,褚连青.硬质合金的比矫顽磁力[J].硬质合金,2000,17(1):48-51. 被引量:13

1陈慧,彭玲玲,姜中涛,邓莹,涂铭旌.真空烧结温度对WC-TiC-TaC-Co硬质合金组织和性能的影响[J].粉末冶金工业,2015,25(3):33-36. 被引量:9

2李金普,丁存光,李一,柳学全,李楠,李发长.低压烧结温度对YG15粗晶硬质合金性能的影响[J].硬质合金,2016,33(1):33-37. 被引量:4

3范昆.串级控温在硬质合金低压烧结炉中的应用[J].机械工程师,2017(9):147-149.

4刘先柱,沈志农,龚静,吴炳辉,高明凯,孙文康.烧结工艺对破碎再生料硬质合金性能的影响[J].湖南工业大学学报,2018,32(2):38-42. 被引量:2

5罗学全,于涛,温光华,朱光柱.球磨时间对WC-7%Co-3%Ni硬质合金组织和性能的影响[J].硬质合金,2020,37(3):240-247. 被引量:2

6易长宾,金星,吴翔.添加W粉对YG20C硬质合金组织及性能的影响[J].稀有金属与硬质合金,2019,47(2):68-73. 被引量:2

1范昆.串级控温在硬质合金低压烧结炉中的应用[J].机械工程师,2017(9):147-149.

2庞立娟,邓刚,张雪峰,肖洪.(Ti,M)C复式碳化物制备方法的研究进展[J].粉末冶金工业,2017,27(3):57-62. 被引量:4

3刘强,陈吉,杨明川.真空烧结烧结温度和保温时间对WC-6%Ni细晶硬质合金组织及性能的影响[J].硬质合金,2017,34(6):393-397. 被引量:2

4郑娟,赵志伟,刘晓芳,陈飞晓,杨宝震.纳米复合抑制剂对微波法制备WC-TiC-Co硬质合金组成和微观结构的影响[J].粉末冶金工业,2018,28(4):21-25. 被引量:2

5刘强,陈吉,杨明川.成形工艺对WC-6Ni细晶硬质合金烧结致密度及组织缺陷的影响[J].稀有金属与硬质合金,2018,46(5):79-82.

6施远,金洙吉,姜冠楠,刘作涛,周忠正,王泽北.YG15硬质合金电化学腐蚀机理研究[J].中国腐蚀与防护学报,2019,39(3):253-259. 被引量:2

7隋毅,梁强.组合形活塞销冷镦挤成形工艺[J].锻压技术,2020,45(1):109-113. 被引量:6

8孟湘君,汪巍,周新华,金鹏.烧结温度对WC-15%(Co-Ni)粗晶硬质合金组织及性能的影响[J].硬质合金,2020,37(4):301-307. 被引量:4

9董良.深冷及深冷后回火处理对截齿硬质合金头耐磨性的影响[J].金属热处理,2021,46(2):105-108. 被引量:1

10孔德方,金鹏,管玉明,龙坚战,罗海辉,刘斌,赵玉玲,张卫兵.WC-10%Co细晶硬质合金晶粒夹粗的模拟研究[J].硬质合金,2021,38(2):88-95. 被引量:4

1韩永传.高温耐磨堆焊焊条的研究[J].烟台大学学报:自然科学与工程版,2003,16(2):129-132. 被引量:2

2王江萍,栗卓新,魏琪,马辉.电弧喷涂制备高硬度、耐磨、抗氧化涂层及其性能研究[J].新技术新工艺,2004(6):45-47. 被引量:4

3盛晔,袁世东.高温工况下铬钼钢与不锈钢的焊接[J].机械制造文摘:焊接分册,2012(3):46-48. 被引量:2

4苏铁健,王富耻,李树奎,王鲁.合金钢的热导率计算[J].北京理工大学学报,2005,25(1):91-94. 被引量:11

5张文周.具有高效冷却效果的内齿面竖炉齿辊[J].金属加工:热加工,2015,0(1):86-87.

6祖方遒,吴有进.成分及第二相组织对球墨铸钢热疲劳性能的影响[J].钢铁研究学报,1998,10(1):58-63. 被引量:4

7王宽福.焊接结构的蠕变断裂失效与防治[J].石油工程建设,1999,25(4):1-5. 被引量:1

8史春元,杨锡玉,范英,陈辉,杨德新,陈字刚.焊缝界面区域应力状态对异种钢接头蠕变断裂行为的影响[J].大连铁道学院学报,1997,18(2):69-73. 被引量:2

9一种多元高镍铬合金耐磨铸铁及其制备工艺[J].梅山科技,2009(1):40-40.

10吴建新,江伯鸿,徐祖耀.含硼的Cu-Zn-Al合金中母相晶粒度和有序度对M_s的影响[J].金属学报,1989,25(2). 被引量:11

Basic Information:

DOI:

Chinese Library Classification Number:TG113.225[金属学及工艺—物理冶金]

Citation Information:

The factors that affect the coercive force of cemented carbides are analyzed theoretically. Under high-temperate operation mode and actual operation mode,the coercive force is mainly relatedto the maximal sintering temperature. Research is carried out on the high temperature field of PVA sintering furnace. Data processing and analysis is done to obtain the quantitative relationship between coercive force and maximal sintering temperature.

quote

GB/T 7714-2015 [1] FAN You-ming, SHI Zhang-ming, CHEN Yi. Research on the Relationship between the Coercive Force and Maximum Sintering Temperature of WC-Co Cemented Carbides[J]. Rare Metals and Cemented Carbides, 2007(2): 18-20.
MLA [1] FAN You-ming, et al., "Research on the Relationship between the Coercive Force and Maximum Sintering Temperature of WC-Co Cemented Carbides." Rare Metals and Cemented Carbides, no. 2, 2007, pp. 18-20.
APA [1] FAN You-ming, SHI Zhang-ming, & CHEN Yi. (2007). Research on the Relationship between the Coercive Force and Maximum Sintering Temperature of WC-Co Cemented Carbides. Rare Metals and Cemented Carbides(2), 18-20.
IEEE [1] FAN You-ming, SHI Zhang-ming, and CHEN Yi, "Research on the Relationship between the Coercive Force and Maximum Sintering Temperature of WC-Co Cemented Carbides," Rare Metals and Cemented Carbides, no. 2, pp. 18-20, 2007. keywords: {WC-Co;cemented carbides;coercive force;sintering temperature}