Use of Adsorption Column for Separation of Molybdenum from Sodium Tungstate Solution
Rare Metals and Cemented Carbides | Vol., Issue 1, 1994 |
pp. 1-4
Experiments and study on the separation of molybdenum from sodium tungstate solution have been carried out.It has been shown that the use of granular active carbon adsorption column for separating molybdenum (preyiously converted into sulphomolybdate in solution) can obtained satisfactory result with less of tungsten.
DOI: Cited: 0 Download: 0