Modern Developments in RM & HM─Taken out from 13th Plansee Seminar(Ⅰ) AITranslate

Powder Metallurgical Research Institute of Zhongnan University of Technology
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Basing on the publications and the information from 13th Plansee Seminar, a survey on global modern R and D in refractory metals (RM) and hard materials(HM) was presented. The general introduction in bilef of the Seminar was submitted at first. and then, the recent developments in RM.HM and coating techniques were reviewed. Some problems were discussed.

KeyWords AITranslate

Plansee Seminar refractoy metals bard materials development tendency.

1杨敏陔,李舜兰.钼科技进步发展研究[J].中国钼业,1996,20(6):3-7. 被引量:11

2李风光.化学液相共沉淀制备超细氧化物粉末[J].稀有金属与硬质合金,1998,26(3):42-43. 被引量:5

3杨敏陔.展望21世纪硬质合金工业[J].中国钨业,1995,0(7):12-17.

1黄艳华,贺跃辉,谢志刚,向波.金刚石工具用Ni-Co合金粉末的制备及表征[J].超硬材料工程,2006,18(5):1-5. 被引量:9

2林小芹,贺跃辉,王政伟,熊继.钼粉的制备技术及其发展[J].粉末冶金材料科学与工程,2003,8(2):128-133. 被引量:12

3郑少华,王平,王介强,姜奉华.超声波-共沉淀法制备ZrO_2-MgO超细粉[J].中国粉体技术,2004,10(3):17-20. 被引量:9

4陈玉平,郑少华.超声波——共沉淀法制备ZrO2—MgO超细粉[J].江西建材,2004(4):3-4. 被引量:2

5杨永顺,刘祎冉,陈国清,宋志真,王建甫,杨正海.ZrO_2(3Y)-CaO-SiO_2-TiO_2多元纳米复合粉体的制备及表征[J].稀有金属材料与工程,2007,36(A01):184-187.

6吴贤,张健,康新婷,荆鹏.钼粉的制备技术及研发现状[J].稀有金属材料与工程,2007,36(A03):562-566. 被引量:24

7杨敏陔.调整我国钼产业结构问题的探讨[J].中国钼业,1997,21(5):3-6. 被引量:3

8张文禄.我国钼业出口商品结构调整和优化问题[J].中国钼业,1998,22(4):73-74.

9黄蓉,陈仕奇.草酸盐共沉淀法制备Cu-Sn预合金粉末[J].粉末冶金材料科学与工程,2010,15(5):525-529. 被引量:9

10傅小明.纳米钼粉的制备技术及研发现状[J].中国钼业,2010,34(6):37-39. 被引量:7

1第16届国际普兰西会议[J].稀有金属材料与工程,2004,33(5):477-477.

2杨宁,杨帆.激光熔覆工艺及熔覆材料进展[J].铜业工程,2010(3):56-58. 被引量:10

3郑延庆,危森,刘允环.当代切削工具与机床结构的材料进展[J].机械工程师,1995(2):51-53.

4李政.普兰西金属加工厂难熔金属生产简介[J].世界有色金属,1990(4):23-24. 被引量:1

5钟培全.奥地利正筹备’97年国际普兰西会议[J].中国钨业,1996,0(8):30-31.

6常用涂层材料进展及超硬涂层技术[J].超硬材料工程,2014,26(5):4-4. 被引量:2

7宋琳.普兰西工厂难熔金属进展[J].上海钢研,1993(3):49-51.

8殷为宏,张德尧,谢惠久,沈玉蓉,石明柱.难熔金属、耐磨材料和涂层技术的新进展——第十三届国际普兰西学术会议总结[J].稀有金属材料与工程,1993,22(4):77-81. 被引量:2

9杨全民.贮氢合金电极材料进展[J].金属热处理学报,2000,21(2):46-49. 被引量:4

10田震,李晋平,杜志刚,李少华,穆江华.机械合金法制备贮氢材料进展[J].材料导报,1997,11(6):24-27. 被引量:2

Basic Information:

DOI:

Chinese Library Classification Number:TG146.41[金属学及工艺—金属材料]

Citation Information:

Basing on the publications and the information from 13th Plansee Seminar, a survey on global modern R and D in refractory metals (RM) and hard materials(HM) was presented. The general introduction in bilef of the Seminar was submitted at first. and then, the recent developments in RM.HM and coating techniques were reviewed. Some problems were discussed.

quote

GB/T 7714-2015 [1] ZOU Zhi-qiang. Modern Developments in RM & HM─Taken out from 13th Plansee Seminar(Ⅰ)[J]. Rare Metals and Cemented Carbides, 1994(1): 28-35.
MLA [1] ZOU Zhi-qiang. "Modern Developments in RM & HM─Taken out from 13th Plansee Seminar(Ⅰ)." Rare Metals and Cemented Carbides, no. 1, 1994, pp. 28-35.
APA [1] ZOU Zhi-qiang. (1994). Modern Developments in RM & HM─Taken out from 13th Plansee Seminar(Ⅰ). Rare Metals and Cemented Carbides(1), 28-35.
IEEE [1] ZOU Zhi-qiang, "Modern Developments in RM & HM─Taken out from 13th Plansee Seminar(Ⅰ)," Rare Metals and Cemented Carbides, no. 1, pp. 28-35, 1994. keywords: {Plansee Seminar;refractoy metals;bard materials;development tendency.}