A Review of Scattered Metels(Ⅰ) AITranslate

Guangzhou Nonferrous Metal Research Institute;Guangzhou Nonferrous Metal Research Institute
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

This paper is a review of the scattered metals(such as Ga In.T1.Ge.Se.Te and Re),including their geology. reserch. process technology. uses.market,environment and outlook both at home and abroad in recent years.It indicates that the scattered metals have played an important part in the Gulf War and have a great significance in state security.

KeyWords AITranslate

Scattered metals(Ga In T1 Ge Se Te and Re) review both at home and abroad

1周令治,邹家炎.稀散金属近况(Ⅲ)[J].稀有金属与硬质合金,1994,22(3):58-62.

2汪锦瑞.稀散金属铼的提取及研究进展[J].金川科技,2009(3):58-60.

3光宇.“稀散金属”四兄弟[J].金属世界,2000(5):14-14.

4周令治,邹家炎.稀散金属近况(Ⅱ)[J].稀有金属与硬质合金,1994,22(2):39-45. 被引量:2

5黄作仁,李若彬.稀散金属应用及市场预测[J].株冶科技,1989,17(3):48-56.

6陈守东,陈敬超,吕连灏.稀散金属在半导体中的应用及研究进展[J].稀有金属材料与工程,2012,41(S2):214-217. 被引量:1

7刘世友.漫话铊(Tl)[J].金属世界,1992(2):14-14.

8杨尚磊,陈艳,薛小怀,李仕民,楼松年.铼(Re)的性质及应用研究现状[J].上海金属,2005,27(1):45-49. 被引量:47

9刘春民.有色金属简介[J].黑龙江冶金,1995,0(3):27-29.

10周令治,邹家炎.稀散金属近况[J].有色金属:冶炼部分,1994(1):42-46. 被引量:26

Basic Information:

DOI:

Chinese Library Classification Number:TG146.43[金属学及工艺—金属材料]

Citation Information:

This paper is a review of the scattered metals(such as Ga In.T1.Ge.Se.Te and Re),including their geology. reserch. process technology. uses.market,environment and outlook both at home and abroad in recent years.It indicates that the scattered metals have played an important part in the Gulf War and have a great significance in state security.

quote

GB/T 7714-2015 [1] ZHOU Ling-zhi, ZOU Jia-yan. A Review of Scattered Metels(Ⅰ)[J]. Rare Metals and Cemented Carbides, 1994(1): 35-41.
MLA [1] ZHOU Ling-zhi, and ZOU Jia-yan. "A Review of Scattered Metels(Ⅰ)." Rare Metals and Cemented Carbides, no. 1, 1994, pp. 35-41.
APA [1] ZHOU Ling-zhi, & ZOU Jia-yan. (1994). A Review of Scattered Metels(Ⅰ). Rare Metals and Cemented Carbides(1), 35-41.
IEEE [1] ZHOU Ling-zhi and ZOU Jia-yan, "A Review of Scattered Metels(Ⅰ)," Rare Metals and Cemented Carbides, no. 1, pp. 35-41, 1994. keywords: {Scattered metals(Ga,In T1,Ge,Se,Te and Re), review both at home and abroad}