Complex Utilization of Tungsten Resources AITranslate

Zhongnan University of Technology
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The importance of complex utilization of tungsten resources is described.The technology and processes for complex utilization of tungsten resources abroad are introduced and evaluated.

KeyWords AITranslate

Tungsten resources complex utilization solvent extraction

1B.Townsend,钱惠明.溶剂萃取铜的前景[J].矿产保护与利用,1990(5):42-46.

Basic Information:

DOI:

Chinese Library Classification Number:TD983[矿业工程—选矿]

Citation Information:

The importance of complex utilization of tungsten resources is described.The technology and processes for complex utilization of tungsten resources abroad are introduced and evaluated.

quote

GB/T 7714-2015 [1] PAN Ye-jin. Complex Utilization of Tungsten Resources[J]. Rare Metals and Cemented Carbides, 1994(1): 42-44.
MLA [1] PAN Ye-jin. "Complex Utilization of Tungsten Resources." Rare Metals and Cemented Carbides, no. 1, 1994, pp. 42-44.
APA [1] PAN Ye-jin. (1994). Complex Utilization of Tungsten Resources. Rare Metals and Cemented Carbides(1), 42-44.
IEEE [1] PAN Ye-jin, "Complex Utilization of Tungsten Resources," Rare Metals and Cemented Carbides, no. 1, pp. 42-44, 1994. keywords: {Tungsten resources,complex utilization,solvent extraction}