Study and Trial-production of Spectrum Grade Ferroniobium Base AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Abstract AITranslate
Spectrum grade ferroniobium base can be produced from selected raw materials and proper aluminium with additives at a suitable temperature.Impurity content in the base is below GB 7737-87 standard for ferroniobium.
KeyWords AITranslate
Spectrum grade ferroniobium base
trial-production
1刘丽华,梁龙飞,贾宁辰,乐可襄.铌钒微合金化BS460钢筋的试制[J].特殊钢,2002,23(2):49-49.
Basic Information:
DOI:
Chinese Library Classification Number:TF841.6[冶金工程—有色金属冶金]
Citation Information:
Spectrum grade ferroniobium base can be produced from selected raw materials and proper aluminium with additives at a suitable temperature.Impurity content in the base is below GB 7737-87 standard for ferroniobium.
quote
| GB/T 7714-2015 | [1] ZHANG Ji-dun, LI Ji-hua, YUAN Ming-xing, et al. Study and Trial-production of Spectrum Grade Ferroniobium Base[J]. Rare Metals and Cemented Carbides, 1994(1): 25-27. |
| MLA | [1] ZHANG Ji-dun, et al., "Study and Trial-production of Spectrum Grade Ferroniobium Base." Rare Metals and Cemented Carbides, no. 1, 1994, pp. 25-27. |
| APA | [1] ZHANG Ji-dun, LI Ji-hua, YUAN Ming-xing, & ZHONG Yue-lian. (1994). Study and Trial-production of Spectrum Grade Ferroniobium Base. Rare Metals and Cemented Carbides(1), 25-27. |
| IEEE | [1] ZHANG Ji-dun, LI Ji-hua, YUAN Ming-xing, and ZHONG Yue-lian, "Study and Trial-production of Spectrum Grade Ferroniobium Base," Rare Metals and Cemented Carbides, no. 1, pp. 25-27, 1994. keywords: {Spectrum grade ferroniobium base,trial-production} |