Additives for Vanadium Roasting AITranslate
Abstract AITranslate
Study on additives for vanadium roasting was carried out.It is found that NaC1 Na2CO3 may be used instead of NaC1.In this way,air pollution will be reduced and converting rate of vanadium will be raised.
KeyWords AITranslate
1古映莹,庄树新,钟世安,周建良,田俊杰,侯淼淼.硅质岩钒矿中提取钒的无污染焙烧工艺研究[J].稀有金属,2007,31(1):102-106. 被引量:23
2樊青林.页岩钒选冶工艺技术研究进展[J].中国钼业,2021,45(5):36-40. 被引量:1
1邢丽华,余志伟.石墨伴生钒矿中钒的焙烧浸取及分析研究[J].非金属矿,2007,30(6):38-40. 被引量:3
2古映莹,周琼华,周建良,钟世安,庄树新.钒矿石活化焙烧-酸浸新工艺的研究[J].化学世界,2009,50(7):392-395. 被引量:6
3付自碧.石煤空焙—低酸浸出提钒的试验研究[J].金属矿山,2009(9):78-80. 被引量:2
4王耀宁,马红周,陈向阳,兰新哲.石煤中钒酸浸出工艺研究[J].稀有金属,2009,33(6):940-942. 被引量:4
5付自碧,张林,张涛,邱正秋.石煤无盐焙烧—酸浸提钒工艺试验研究[J].铁合金,2009,40(6):24-27. 被引量:1
6李社锋,方梦祥,余斌,周宛谕,王勤辉,施正伦,骆仲泱,岑可法.新疆石煤料团流化床焙烧提钒试验研究[J].浙江大学学报:工学版,2010,44(6):1133-1137. 被引量:2
7李兰杰,张力,郑诗礼,娄太平,张懿,陈东辉,张燕.钒钛磁铁矿钙化焙烧及其酸浸提钒[J].过程工程学报,2011,11(4):573-578. 被引量:57
8雷辉,陈建梅,胡盛强,胡蓝双,高峰,颜文斌.复合添加剂对石煤提钒焙烧与浸出工艺研究[J].无机盐工业,2012,44(1):33-36. 被引量:13
9李昌林,周云峰,费海霞,周向阳,李劼.石煤提钒工艺研究及应用现状[J].稀有金属与硬质合金,2012,40(6):9-14. 被引量:12
10陶长元,于永波,刘作华,杜军,范兴.硼钙石强化转炉钒渣氧化焙烧的研究[J].钢铁钒钛,2014,35(4):6-13. 被引量:2
1卢琛.低价钒冶炼钒铁的研究[J].钒钛,1992(6):43-48. 被引量:1
2谭武现.模糊控制技术在转炉提钒中的应用探讨[J].攀枝花科技与信息,1998,23(4):40-43.
3古映莹,庄树新,钟世安,周建良,田俊杰,侯淼淼.硅质岩钒矿中提取钒的无污染焙烧工艺研究[J].稀有金属,2007,31(1):102-106. 被引量:23
4陈津,刘浏,曾加庆.竖炉型含碳球团有机粘结剂的选择与应用[J].烧结球团,2000,25(6):29-31. 被引量:5
5广西今年前1O个月淘汰造纸落后产能近11万吨[J].中国包装,2013,33(12):76-76.
6王以森,王小亚,陈任辉.钒冶炼3种浸取方法的对比分析[J].企业技术开发,2007,26(2):22-23.
7王晨,张传福.铜熔炼过程最佳冰铜品位选择研究[J].世界有色金属,2016,41(9):21-22. 被引量:3
8付利攀,张一敏,刘涛,黄晶,杨晓,赵杰.添加剂DN对石煤提钒焙烧效果的影响[J].矿冶工程,2013,33(1):65-68. 被引量:2
9李兰杰,张力,郑诗礼,娄太平,张懿,陈东辉,张燕.钒钛磁铁矿钙化焙烧及其酸浸提钒[J].过程工程学报,2011,11(4):573-578. 被引量:57
10吴在玖.焙烧-酸浸-氰化法从复杂金精矿中回收金银铜[J].有色金属科学与工程,2013,4(2):25-29. 被引量:10
Basic Information:
DOI:
Chinese Library Classification Number:TF841.3[冶金工程—有色金属冶金]
Citation Information:
Study on additives for vanadium roasting was carried out.It is found that NaC1 Na2CO3 may be used instead of NaC1.In this way,air pollution will be reduced and converting rate of vanadium will be raised.
quote
| GB/T 7714-2015 | [1] YI Jian-min, YAN Jian-hui, GAO Di-qun, et al. Additives for Vanadium Roasting[J]. Rare Metals and Cemented Carbides, 1994(1): 5-9. |
| MLA | [1] YI Jian-min, et al., "Additives for Vanadium Roasting." Rare Metals and Cemented Carbides, no. 1, 1994, pp. 5-9. |
| APA | [1] YI Jian-min, YAN Jian-hui, GAO Di-qun, & LIU Kang. (1994). Additives for Vanadium Roasting. Rare Metals and Cemented Carbides(1), 5-9. |
| IEEE | [1] YI Jian-min, YAN Jian-hui, GAO Di-qun, and LIU Kang, "Additives for Vanadium Roasting," Rare Metals and Cemented Carbides, no. 1, pp. 5-9, 1994. keywords: {Vanadium smelting,roasting additives NaCl Na_2CO_3.} |