Trial Production of PVC Sheet by thd Addition of RE Stablizer

Rare Metals and Cemented Carbides | Vol., Issue 1, 1999 | pp. 23-26
Description is made of the reaction principle of RE Stablizer on the PVC plastics and the test on PVC sheet preparation by the said stablizer. The test results show that 0.2%~ 0.4 % addition of RE thermal stablizer can result in uniform plasticization of PVC plastics, longer thermal decomposition of the sheet, and a >50% decrease of “fish eyes” in the transparent sheet, 10~16° increase of the whiteness of the opal sheet, and 3~5° increase of the glossiness.
DOI: Cited: 0 Download: 0

Research and Manufacture of Composite Rolling Mill Guide Plate

Rare Metals and Cemented Carbides | Vol., Issue 1, 1999 | pp. 26-30
In this paper, on the basis of anal ysis of guide plate's damage form, according to hard alloy's properties and characteristics, we put forward that guide plate is made from hard alloy. In order to improve the fracture resistance of the plate and decrease the production cost, we develop acomposite cast technology of hard alloy. The results obtained show that the composite guide plate is safe and reliable in use, its service effect is more excellent than that of high Ni Cr steel and high Cr cast iron (steel) guide plate. The adoption of the composite guide plate will result in high precision rolled products with good surface quality, as well as increase of production rate by 2%~4%.
DOI: Cited: 0 Download: 0

Estimation of the Heat Capacity of Complex Organic Compounds by a Novel Topological Index

Rare Metals and Cemented Carbides | Vol., Issue 1, 1999 | pp. 30-35
A colored hydrogen depleted graph was proposed to replace molecular graph so as to obtain good discrimination of the complex organic compounds by dyeing both the edges and the vertices. Furthermore,the topological index Xu based on the adjacency matrix A and distance matrix D was derived and further adapted to the multiplybonds,heteroatom containing compounds by using the related bond length to C-C bond instead of the adjacent topological distance and the valence δ i instead of the degree of vertex ν i in this paper.The index was highly correlated with the heat capacity of alkanes, unsaturated hydrocarbons, aromatics and sulfur containing compounds,etc.,and the calculated values were in good agreement with experimental data. The proposed Xu index promised to be a useful parameter in QSPR/QSAR research.
DOI: Cited: 0 Download: 0

Microyield Strength of Beryllium Materials Used in Inertial Guidance Instrument

Rare Metals and Cemented Carbides | Vol., Issue 1, 1999 | pp. 43-47
Survey is made of study and testing methods of microyield strength(MYS) of beryllium materials used in inertial guidance instrument. The influence of grain size, impurity (BeO), heat treatment and microalloying on MYS of beryllium is discussed. The conclusion is that impact attritioned powder with finer grain size and lower oxide content and its isostatic press ing consolidation are an important way to obtain high MYS beryllium materials.
DOI: Cited: 0 Download: 0