Study on the WC 20% (Fe Co Ni) Hard Metals Polyester Cut off Tool AITranslate

Tianjin Institute of Hard Alloy;Tianjin Institute of Hard Alloy;Tianjin Institute of Hard Alloy;Tianjin Institute of Hard Alloy
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Study is made of YF 20 WC 20%(65%Fe 19%Co 16%Ni) hard alloy polyester cut off tools instead of YG 20 WC 20%Co tools. Results show that the physical/ mechanical property of YF 20 is close or up to that of YG 20 .

KeyWords AITranslate

WC 20%(Fe Co Ni) hard alloy polyester cut off tool property

1孙宝琦.硬质合金中铁镍代钴问题浅析[J].硬质合金,1996,13(1):47-55. 被引量:32

2李沐山.八十年世界硬质合金技术进展[M].株洲:硬质合金编辑部,1991.441.

3谭映国.-[J].硬质合金,1997,(1):3-3.

4铃木寿.-[J].粉末及粉末冶金(日),1974,20(8):31-31.

5刘永福.-[J].硬质合金,1996,(3):178-178.

1原一高,朱世根.化纤切断刀的锋利度与刃口半径的关系[J].纺织学报,2005,26(2):59-60. 被引量:3

2徐二锋,原一高,朱世根.化纤丝束切断刀的发展趋势[J].纺织器材,2005,32(6):5-7.

3徐二锋,原一高,朱世根.涤纶短纤维切断刀的发展现状[J].合成纤维工业,2006,29(1):56-58. 被引量:1

4唐清亮,原一高,朱世根.化纤切断刀刃口角度的模拟分析与设计[J].工具技术,2010,44(8):68-70. 被引量:1

5雍志华,汪仕元,程娟,冯钰鑫,张伟,朱俊峰.WC-8(Fe/Ni/Co)R硬质合金的研究[J].稀有金属材料与工程,2000,29(4):273-275. 被引量:1

6陈鼎,成亮,李经宇,王喜斌.基于有限元方法的翅片切断刀刃口角度的模拟分析[J].工具技术,2013,47(10):44-46. 被引量:1

7原一高,朱世根,丁浩.降低涤纶短纤维切断刀成本的技术途径[J].东华大学学报:自然科学版,2002,28(1):131-134.

1汤中科,李辉.烟丝切刀锋利度的影响因素分析[J].机械工程师,2008(12):143-145.

2史晓亮,杨凯华,汤凤林,邵刚勤.稀土Ce的添加方式对WC-Co硬质合金性能的影响[J].中南大学学报:自然科学版,2005,36(2):204-208. 被引量:12

3牛建峰.涤纶短纤维切断刀失效原因分析及对策[J].合成技术及应用,2014,29(3):39-42.

4陈蕾,徐道春,田海龙,柯清禅.木材用高速螺旋式玉米铣刀的变形分析与优化[J].工具技术,2014,48(9):29-32.

5俞圆,怀华培,戴立强,凌国平.尼龙丝切口形貌与旋转剃须刀锋利度关系[J].理化检验:物理分册,2015,51(12):874-879. 被引量:1

6冯克明,赵金坠,丁春生,张国威,董德胜,高秋菊,高翀.砂轮锋利性及其关联分析与试验研究[J].超硬材料工程,2022,34(3):7-13.

7陈士忠,苏伟,王永华,贾千业.钢筋调直切断机切刀刃角对飞剪切断效果影响的数值模拟[J].沈阳建筑大学学报:自然科学版,2019,0(4):731-740. 被引量:1

1刘先曙.用废塑料生产高强度的聚合物[J].科技导报,2003(7):27-27.

2王尚志.WC-(15~20)m%Fe-Co-Ni硬质合金研究[J].硬质合金,1998,15(1):21-24. 被引量:6

3赵国栋,王军,潘治梁,蔡绪福.ABS合金的最新研究进展[J].上海塑料,2009,37(2):1-5. 被引量:3

4原永威,李学训,吴靖嘉.PC/ABS合金研究的进展[J].兰化科技,1994,12(1):46-53. 被引量:20

5王国建,李勇进.高分子合金增容剂与增韧机理研究[J].化学建材,1998,14(4):12-14. 被引量:4

6新技术与成果[J].中国金属通报,1997,0(25):21-22.

7于桂复,焦成革,戴圣龙.快速凝固(RS)A1-Li合金研究[J].高技术通讯,1994,4(1):21-25. 被引量:1

8赵文聘,徐丽芳,王丽缓,黄平.高性能PC/ABS合金研究[J].塑料科技,2000,28(3):28-30. 被引量:4

9余海霞,郭卫红.国内ABS合金研究的最新进展[J].塑料开发,1999,25(2):1114-1117.

10朱伟平.ABS树脂及其合金研究进展与应用[J].塑料加工应用,1998,20(4):55-60. 被引量:1

Basic Information:

DOI:

Chinese Library Classification Number:TQ342.206[化学工程—化纤工业];TF125.31[冶金工程—粉末冶金]

Citation Information:

Study is made of YF 20 WC 20%(65%Fe 19%Co 16%Ni) hard alloy polyester cut off tools instead of YG 20 WC 20%Co tools. Results show that the physical/ mechanical property of YF 20 is close or up to that of YG 20 .

quote

GB/T 7714-2015 [1] WANG Shang-zhi, WANG Wen-zhai, SHI Yu-hui, et al. Study on the WC 20% (Fe Co Ni) Hard Metals Polyester Cut off Tool[J]. Rare Metals and Cemented Carbides, 1999(1): 14-16.
MLA [1] WANG Shang-zhi, et al., "Study on the WC 20% (Fe Co Ni) Hard Metals Polyester Cut off Tool." Rare Metals and Cemented Carbides, no. 1, 1999, pp. 14-16.
APA [1] WANG Shang-zhi, WANG Wen-zhai, SHI Yu-hui, & FAN Bo-jian. (1999). Study on the WC 20% (Fe Co Ni) Hard Metals Polyester Cut off Tool. Rare Metals and Cemented Carbides(1), 14-16.
IEEE [1] WANG Shang-zhi, WANG Wen-zhai, SHI Yu-hui, and FAN Bo-jian, "Study on the WC 20% (Fe Co Ni) Hard Metals Polyester Cut off Tool," Rare Metals and Cemented Carbides, no. 1, pp. 14-16, 1999. keywords: {WC 20%(Fe Co Ni) hard alloy, polyester cut off tool, property}