Trial Production of PVC Sheet by thd Addition of RE Stablizer AITranslate
Abstract AITranslate
Description is made of the reaction principle of RE Stablizer on the PVC plastics and the test on PVC sheet preparation by the said stablizer. The test results show that 0.2%~ 0.4 % addition of RE thermal stablizer can result in uniform plasticization of PVC plastics, longer thermal decomposition of the sheet, and a >50% decrease of “fish eyes” in the transparent sheet, 10~16° increase of the whiteness of the opal sheet, and 3~5° increase of the glossiness.
KeyWords AITranslate
1L·马西亚 王佩云(译).塑料添加剂的作用[M].北京:轻工业出版社,1980..
2刘光烨,杨智明,沈经炜.硬脂酸稀土作为聚氯乙烯稳定剂及其稳定机理的研究[J].稀土,1989(3):36-38. 被引量:17
1詹志洪.稀土在塑料和涂料制品中的应用与展望[J].稀土,2004,25(6):80-83. 被引量:3
1张玉玺,唐黎明,曹鸿璋.稀土在涂料工业中的应用[J].涂料工业,2009,39(3):61-63. 被引量:8
2汪怀远,冯新,史以俊,陆小华.Effects of Treated Nano-Lanthanum Oxide on the Mechanical and Tribological Properties of PTFE Nanocomposites[J].稀土学报:英文版,2007,0(S2):40-44.
3戴越,陈逸珺,张孟群.微波消解-电感耦合等离子体原子发射光谱法测定催干剂中金属元素含量[J].理化检验:化学分册,2010,46(4):371-373. 被引量:4
1韩涛.CPE在PVC磁白片中的应用[J].塑料科技,1992,20(3):21-25. 被引量:1
2韩涛.CPE在PVC磁白片中的应用[J].塑料工程,1992(1):32-36.
3张治华.改善聚丙稀透明片热成型性和:透明性的制造方法[J].塑料加工应用,1989(4):22-24.
4让你变笨的10种食物[J].今日民族,2010(5):61-61.
5赵冬尚.PVC透明硬片的生产工艺探讨[J].塑料开发,1989(2):49-52.
6魏永涛,王建兵.悬浮聚氯乙烯树脂指标对制品的影响[J].中国氯碱,2004(11):13-15. 被引量:2
7杨中文,刘西文.RETM热稳定剂在PVC-U透明片中的应用[J].塑料科技,2008,36(1):84-87. 被引量:1
8阿科玛推出高效MBS抗冲改性剂,迁新总部[J].聚合物与助剂,2008(1):60-60.
9韩涛.CPE在PVC磁白片中的应用[J].聚氯乙烯,1993,0(1):16-21.
10汪秋荣,楼树均.硬聚氯乙烯透明片加工中内外润滑剂的国产化[J].塑料,1989,18(4):24-28.
Basic Information:
DOI:
Chinese Library Classification Number:TQ325.3[化学工程—合成树脂塑料工业]
Citation Information:
Description is made of the reaction principle of RE Stablizer on the PVC plastics and the test on PVC sheet preparation by the said stablizer. The test results show that 0.2%~ 0.4 % addition of RE thermal stablizer can result in uniform plasticization of PVC plastics, longer thermal decomposition of the sheet, and a >50% decrease of “fish eyes” in the transparent sheet, 10~16° increase of the whiteness of the opal sheet, and 3~5° increase of the glossiness.
quote
| GB/T 7714-2015 | [1] CHEN Ruo-xian, ZHENG Jian-yu, YANG Jian-mei. Trial Production of PVC Sheet by thd Addition of RE Stablizer[J]. Rare Metals and Cemented Carbides, 1999(1): 23-26. |
| MLA | [1] CHEN Ruo-xian, et al., "Trial Production of PVC Sheet by thd Addition of RE Stablizer." Rare Metals and Cemented Carbides, no. 1, 1999, pp. 23-26. |
| APA | [1] CHEN Ruo-xian, ZHENG Jian-yu, & YANG Jian-mei. (1999). Trial Production of PVC Sheet by thd Addition of RE Stablizer. Rare Metals and Cemented Carbides(1), 23-26. |
| IEEE | [1] CHEN Ruo-xian, ZHENG Jian-yu, and YANG Jian-mei, "Trial Production of PVC Sheet by thd Addition of RE Stablizer," Rare Metals and Cemented Carbides, no. 1, pp. 23-26, 1999. keywords: {rare earth, thermal stablizer, PVC} |