Method Selection for Treatment of Shizhuyuan Low-grade Tungsten Ore
Rare Metals and Cemented Carbides | Vol., Issue 1, 1996 |
pp. 1-3
From the point of view of the technology-mineralogicalcharacteristic of Shizhuyuan tungsten middling, present metallurgicalprocesses for treatment of tungsten ores have been compared and screened and with reference to development work at home and abroad, a new mechanically activating soda leaching process is proposed. Laboratorytests discovered that the proposed process can effectively decomposedthe middling up to 98 6%-99% under the following conditions: sodaconsumption less 300% of stechiometric, T<200℃, t<1 5h.