Development and Production of High-quality Low-cobalt Mining Hard Metals AITranslate

Jianghan Drill Bit Factory
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

According to the theory of non-uniform structure of mininghard metals, a high-quality low-cobalt (Co 6%) mining hard metal isdeveloped from high-grade WC powder and high-purity, ultra-fine Copowder with advanced SIP technology. The product proves satisfactoryin use.Its quality is near to that of similar Sandvik product.Mass production of this product has started.

KeyWords AITranslate

low-cobalt high quality mining hard metal developmentand production

1黄丽容,陈宇航,王晓雷.微孔结构对低钴粗晶WC硬质合金摩擦性能的影响[J].金属功能材料,2016,23(3):37-41. 被引量:6

2HUANG Lirong,CHEN Yuhang,WANG Xiaolei.Surface Features and Friction Characteristics of Porous and Coarse-grain WC-3%Co[J].硅酸盐学报:英文版,2016,0(2):102-110.

1白洋,张丽丽,李刚.WC基体育器械用复合材料的制备及磨损性能研究[J].铸造技术,2017,38(5):1017-1020. 被引量:1

2王蕾,刘辛,谢焕文,邹黎明,蔡一湘.不同方法制备的球形铸造碳化钨粉末的性能研究[J].粉末冶金工业,2017,27(4):7-11. 被引量:2

3郑娟,赵志伟,刘晓芳,陈飞晓,杨宝震.纳米复合抑制剂对微波法制备WC-TiC-Co硬质合金组成和微观结构的影响[J].粉末冶金工业,2018,28(4):21-25. 被引量:2

4秦琴,王楠,颜子镒,田金欣,唐诗佳,杨昊栋,黄泰博.WC粗晶硬质合金摩擦性能影响因素分析[J].稀有金属与硬质合金,2021,49(5):82-86. 被引量:2

5罗亿,丁昊昊,郭俊,刘启跃,王文健.不同法向载荷下TiN涂层磨损寿命与失效机理研究[J].摩擦学学报,2022,42(5):978-989.

6杨宇,袁建坤,陈鹏起,郎宏彬,霍俊豪,程继贵.微晶蜡基粘结剂应用于YG10硬质合金注射成形的研究[J].粉末冶金工业,2022,32(6):10-15. 被引量:1

1刘曼玥.专利信息[J].粉末冶金工业,2012,22(5):64-64.

2孟繁德,包燕平.瑞典山特维克钢公司[J].上海冶金情报,1997(1):42-45.

3刘荣湘,易凯华.镍代钴矿用硬质合金的新进展[J].稀有金属与硬质合金,1994,22(2):46-49. 被引量:6

4张俊熙,王和斌.用电溶法回收的碳化钨制取的矿用硬质合金的特性及其使用效果[J].硬质合金,1993,10(3):133-142. 被引量:1

5张武装,刘咏,羊建高,黄伯云.正碳烧结法制备WC-Co梯度结构硬质合金的研究[J].稀有金属与硬质合金,2004,32(1):32-35. 被引量:8

6吴国钦,黄昌元,张旭.湿法炼锌低钴硫酸锌溶液两段连续深度净化工业实践[J].中国有色冶金,2014,43(2):5-8. 被引量:3

7王国栋,商鸿亮.颗粒增强复合材料研究及矿用硬质合金进展[J].山东化工,2015,44(6):68-70. 被引量:2

8张武装,刘咏,黄伯云,羊建高.WC-Co梯度结构硬质合金的研究进展[J].粉末冶金材料科学与工程,2004,9(2):121-125. 被引量:5

9唐受捷,胡启明.YT15非均匀结构硬质合金的试制[J].硬质合金,2001,18(2):74-76. 被引量:3

10自贡硬质合金厂Z系列矿用硬质合金获总公司技术进步四等奖[J].中国钨业,1993,0(6):17-17.

Basic Information:

DOI:

Chinese Library Classification Number:TF125.3[冶金工程—粉末冶金]

Citation Information:

According to the theory of non-uniform structure of mininghard metals, a high-quality low-cobalt (Co 6%) mining hard metal isdeveloped from high-grade WC powder and high-purity, ultra-fine Copowder with advanced SIP technology. The product proves satisfactoryin use.Its quality is near to that of similar Sandvik product.Mass production of this product has started.

quote

GB/T 7714-2015 [1] SUN Dong-ping. Development and Production of High-quality Low-cobalt Mining Hard Metals[J]. Rare Metals and Cemented Carbides, 1996(1): 15-19.
MLA [1] SUN Dong-ping. "Development and Production of High-quality Low-cobalt Mining Hard Metals." Rare Metals and Cemented Carbides, no. 1, 1996, pp. 15-19.
APA [1] SUN Dong-ping. (1996). Development and Production of High-quality Low-cobalt Mining Hard Metals. Rare Metals and Cemented Carbides(1), 15-19.
IEEE [1] SUN Dong-ping, "Development and Production of High-quality Low-cobalt Mining Hard Metals," Rare Metals and Cemented Carbides, no. 1, pp. 15-19, 1996. keywords: {low-cobalt, high quality, mining hard metal, developmentand production}