Investigation of Ca Removal Method During APT Production by Ion Exchange Process AITranslate

Nanning Hard Alloy Factory
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Detailed description is made of the sources of Ca impurityand its removal method during APT production by ion exchange processIt is mentioned in the paper that Ca mainly comes from process water and ammonium chloride and occurs in the form of CaWO_4 in the process.For Ca removal to improve APT quality, the following methods maybe made: adoption of pure water instead of tap water, regular treatmentof ion exchange resin with acid or alkali, and filtration of (NH_4)_2WO_4solution.

KeyWords AITranslate

ion exchange APT production Ca removal technologicalinvestigation

1黄培,阙正波,蒋英,王晓东.聚酰亚胺薄膜表面改性研究进展[J].材料导报,2009,23(13):107-110. 被引量:11

2姚秀敏,谭寿洪,黄政仁.聚氨酯海绵的预处理对网眼多孔陶瓷性能的影响[J].硅酸盐学报,2005,33(10):1215-1219. 被引量:23

3马志鸿,孟晓维.NdFeB磁体的酸碱处理及电沉积[J].稀土,1995,16(4):13-18. 被引量:5

4易锦琼,熊兴耀.木质纤维素预处理技术[J].农产品加工:下,2010(6):4-7. 被引量:11

5范利灵,吴建功,林宝伟,王志强.用化学沉积法在以废碎玻璃瓶为原料制备的玻璃微珠表面镀二氧化钛薄膜[J].大连工业大学学报,2016,35(4):289-292. 被引量:1

6张磊,黄利,丁佳,陈辉宇,陈伟,胡丽丽.酸碱处理对磷酸盐激光玻璃表面的侵蚀研究[J].无机材料学报,2012,27(6):627-632. 被引量:1

7李培,李远,叶方玉,曹兵.聚芳硫醚砜纳滤膜的制备及耐溶剂特性表征[J].北京化工大学学报:自然科学版,2016,43(2):6-11. 被引量:4

8太阳能多晶硅尾气回收液相二氧化硅提纯方法[J].无机盐工业,2010(6):38-38.

9刘露,王罗新,吴静,王桦.酸碱液相处理对聚氧亚甲基(POM)纤维性能的影响[J].化工新型材料,2013,41(11):145-148. 被引量:1

10谭惠芬,陈中海,刘涛,王铭,潘巧明.海水淡化反渗透商品膜耐酸碱性研究[J].水处理技术,2016,42(7):70-74.

Basic Information:

DOI:

Chinese Library Classification Number:TQ113.79[化学工程—无机化工]

Citation Information:

Detailed description is made of the sources of Ca impurityand its removal method during APT production by ion exchange processIt is mentioned in the paper that Ca mainly comes from process water and ammonium chloride and occurs in the form of CaWO_4 in the process.For Ca removal to improve APT quality, the following methods maybe made: adoption of pure water instead of tap water, regular treatmentof ion exchange resin with acid or alkali, and filtration of (NH_4)_2WO_4solution.

quote

GB/T 7714-2015 [1] LI Jin-fa. Investigation of Ca Removal Method During APT Production by Ion Exchange Process[J]. Rare Metals and Cemented Carbides, 1996(1): 8-11.
MLA [1] LI Jin-fa. "Investigation of Ca Removal Method During APT Production by Ion Exchange Process." Rare Metals and Cemented Carbides, no. 1, 1996, pp. 8-11.
APA [1] LI Jin-fa. (1996). Investigation of Ca Removal Method During APT Production by Ion Exchange Process. Rare Metals and Cemented Carbides(1), 8-11.
IEEE [1] LI Jin-fa, "Investigation of Ca Removal Method During APT Production by Ion Exchange Process," Rare Metals and Cemented Carbides, no. 1, pp. 8-11, 1996. keywords: {ion exchange, APT production, Ca removal, technologicalinvestigation}