Study of Extraction of Uranium with Tertiary Amine for the Separation from Th and Rare Earths AITranslate
Abstract AITranslate
Monazite is leached by caustic soda. The leached residue isselectively dissolved by HCl with obtained 'selectively dissolved'residue. The later subjects to H_2SO_4 leaching and extraction. This paperdesert bes the results of study on the extraction of U from the H_2SO_4 leached solution with tertiary amine N235 for the separation from Thand rare earth. The results show that >99.5% uranium extraction yieldis obtained and ThO_2/U in the stripped U solution is (1.8-3.8) × 10 ̄(-3),RE_xO_y/U is (1.0-1 .6) ×10 ̄(-3) while U/ThO_2 in U raffinate is only(3.5-5. 6) × 10 ̄(-6).
KeyWords AITranslate
1刘铭,周雍茂.用N_(235)-TBP混合体系从硫酸盐溶液中协同萃取除铁[J].中国有色金属学报,2005,15(10):1648-1654. 被引量:36
2张志磊,宁桂玲,林源,叶俊伟,杨雪峰.以硼泥为原料制备的硫酸镁溶液萃取除铁研究[J].化学试剂,2008,30(6):461-464. 被引量:2
3侯会丽,张广心,郑水林,孙青.硼泥中有价组分提取工艺现状及发展趋势[J].中国非金属矿工业导刊,2013(3):32-35. 被引量:4
4支梅峰,张永明,王皓,舒祖骏,赵凤岐,周志全,马嘉.优溶渣中铀的硫酸浸出试验研究[J].铀矿冶,2018,37(4):241-246. 被引量:2
5曾广军,王桂硕,刘忠臣,向秋林,刘会武,黄永.用N235从某铀矿石酸性浸出液中萃取铀试验研究[J].湿法冶金,2022,41(4):324-328.
1廖春发,聂华平,焦云芬,梁勇,杨少华.Study on the diffusion kinetics of adsorption of heavy rare earth with Cyanex272-P507 impregnated resin[J].稀土学报:英文版,2010(S1):120-124. 被引量:4
2廖春发,焦芸芬,邱定蕃,薛济来.Cyanex272-P_(507)浸渍树脂协同萃取色层分离铥镱镥的研究[J].中国稀土学报,2007,25(2):249-252. 被引量:11
3王菊,杨东洁,伏宏彬.硫酸法二氧化钛生产中萃取分离钛、铁的研究进展[J].涂料工业,2009,39(9):16-17. 被引量:3
4潘庆辉,刘厚凡.硫酸介质中P507萃取Fe^(3+)的实验研究[J].江西化工,2010,26(1):86-89. 被引量:5
5程永华,李青彬.Amberlite XAD-2000树脂固相萃取富集-火焰原子吸收法测定水中痕量铜[J].化学试剂,2010,32(8):718-720. 被引量:5
6廖春发,焦芸芬,梁勇,姜平国,聂华平.Adsorption-extraction mechanism of heavy rare earth by Cyanex272-P507 impregnated resin[J].中国有色金属学报:英文版,2010,20(8):1511-1516. 被引量:3
7叶国华,童雄,路璐.含钒钢渣的选矿预处理及其对后续浸出的影响[J].中国有色金属学报,2010,20(11):2233-2238. 被引量:18
8薛茹君.粉煤灰硫酸浸出液中钛和铁的萃取分离[J].应用化学,2011,28(7):804-808. 被引量:4
9童秋桃,朱高远,肖奇.铝土矿选矿尾矿酸法提铝除铁实验研究[J].湖南有色金属,2012,28(1):21-24. 被引量:4
10侯会丽,张广心,郑水林,孙青.硼泥中有价组分提取工艺现状及发展趋势[J].中国非金属矿工业导刊,2013(3):32-35. 被引量:4
1董国愔,刘卫军,陈连山,何钟林,赵国良.叔胺N_(235)萃取柠檬酸的研究[J].光谱实验室,1997,14(6):62-64. 被引量:2
2刘月英,陈景,谢琦莹.N_(235)萃取Pt体系产生第三相的影响因素[J].中国有色金属学报,2009,19(7):1316-1321. 被引量:6
3谭文进,贺小塘,肖雄,张选冬,刘伟,刘文,鲁俊余,林波,马王蕊,金云杰,朱利亚.ICP-AES法测定废催化剂不溶渣中的铂、钯和铑[J].贵金属,2015,36(3):72-77. 被引量:19
4杨冬,林承志,安利佳,周春芳,陈连山.叔胺N_(235-)正辛醇-石油醚协萃柠檬酸机理的研究[J].光谱实验室,1999,16(4):378-381.
5邹兴.高质量高附加值四氧化三锰制备技术研制成功[J].中国稀土学报,2004(z1). 被引量:1
6彭图治,施清照,吕荣山.N_(235)萃取型碳糊修饰电极测定金的研究[J].应用科学学报,1990,8(4):367-370. 被引量:2
7刘兴芝,房大维,李春梅,王燕,李俊,臧树良.硫酸体系中N235萃取铼的热力学研究[J].化学工程,2007,35(5):44-47. 被引量:5
8韩泳平.叔胺从硫酸氢钾溶液中萃取硫酸机理的研究[J].四川化工,1996(3):9-11. 被引量:7
9谢琦莹,陈景,杨项军,王宇.N_(235)萃取HCl体系中TBP消除第三相的作用机理[J].无机化学学报,2007,23(1):57-62. 被引量:25
10徐立进,邱发礼,吕绍洁.在ThO_2-SrCO_3/BaSO_4催化剂中甲烷氧化偶联反应的研究[J].天然气化工—C1化学与化工,1996,21(3):26-29. 被引量:5
Basic Information:
DOI:
Chinese Library Classification Number:O614.42[理学—无机化学];O652.62[理学—分析化学]
Citation Information:
Monazite is leached by caustic soda. The leached residue isselectively dissolved by HCl with obtained 'selectively dissolved'residue. The later subjects to H_2SO_4 leaching and extraction. This paperdesert bes the results of study on the extraction of U from the H_2SO_4 leached solution with tertiary amine N235 for the separation from Thand rare earth. The results show that >99.5% uranium extraction yieldis obtained and ThO_2/U in the stripped U solution is (1.8-3.8) × 10 ̄(-3),RE_xO_y/U is (1.0-1 .6) ×10 ̄(-3) while U/ThO_2 in U raffinate is only(3.5-5. 6) × 10 ̄(-6).
quote
| GB/T 7714-2015 | [1] HU Hai-nan. Study of Extraction of Uranium with Tertiary Amine for the Separation from Th and Rare Earths[J]. Rare Metals and Cemented Carbides, 1996(1): 4-7. |
| MLA | [1] HU Hai-nan. "Study of Extraction of Uranium with Tertiary Amine for the Separation from Th and Rare Earths." Rare Metals and Cemented Carbides, no. 1, 1996, pp. 4-7. |
| APA | [1] HU Hai-nan. (1996). Study of Extraction of Uranium with Tertiary Amine for the Separation from Th and Rare Earths. Rare Metals and Cemented Carbides(1), 4-7. |
| IEEE | [1] HU Hai-nan, "Study of Extraction of Uranium with Tertiary Amine for the Separation from Th and Rare Earths," Rare Metals and Cemented Carbides, no. 1, pp. 4-7, 1996. keywords: {selectively-dissolved residue, extraction with N235 tertiary.amine, U, Th rare earths} |