Quantitative Determination of Solid Solution Elements in Binder of Ti(CN)Ceramic-metal AITranslate
Abstract AITranslate
Our experiments show that solid solution elements (such asW. Mo. Ti) in binder of Ti (CN) ceramic-metal can not be dissolvedcompletely in concentrated HCl acid at 30℃, which is not in agreementwith results reported in(3), but can be dissolved completely in concentrated HCl acid plus sulphuric acid at 80℃. Method presented in thispaper can simply and effectively be used for quantitive determinationof solid solution elements in binder of Ti(CN) ceramic-metal.
KeyWords AITranslate
1全朝海.Ti(CN)基金属陶瓷刀片切削性能的研究[J].粉末冶金材料科学与工程,1997,2(4):305-309. 被引量:1
2望军,贾碧,邸永江.纳米/超细Ti(CN)基金属陶瓷的研究进展[J].材料导报:纳米与新材料专辑,2010,24(1):12-14.
3全朝海.Ti(CN)基金属陶瓷刀片切削性能的研究[J].水利电力机械,1998(1):12-16.
4何平,蒲熙.Ti(CN)基金属陶瓷微观组织的研究[J].硬质合金,1995,12(4):198-202. 被引量:3
5于军慧,杨锷.Ti(CN)基金属陶瓷刀片的切削性能[J].工具技术,2000,34(7):9-10. 被引量:1
6周书助,彭卫珍,王社权.烧结温度对Ti(CN)基金属陶瓷成分和显微结构的影响[J].硬质合金,2008,25(3):131-134. 被引量:7
7张洁尧.碳含量对Ti(CN)基金属陶瓷力学性能的影响[J].硬质合金,2003,20(3):154-156. 被引量:3
8全朝海.Ti(C,N)基金属陶瓷刀片切削性能的研究[J].硬质合金,1997,14(3):154-158. 被引量:1
9望军,吕凌,孙晓燕,刘颖,任强,叶金文,涂铭旌.VC对微米级Ti(CN)基金属陶瓷微观结构和力学性能的影响[J].工具技术,2008,42(8):14-16. 被引量:3
10周书助,罗成,谭锦灏,朱磊,胡倞.Ti(CN)基金属陶瓷压坯在烧结过程中的成分变化[J].湖南工业大学学报,2009,23(6):52-55. 被引量:2
Basic Information:
DOI:
Chinese Library Classification Number:TG148[金属学及工艺—金属材料]
Citation Information:
Our experiments show that solid solution elements (such asW. Mo. Ti) in binder of Ti (CN) ceramic-metal can not be dissolvedcompletely in concentrated HCl acid at 30℃, which is not in agreementwith results reported in(3), but can be dissolved completely in concentrated HCl acid plus sulphuric acid at 80℃. Method presented in thispaper can simply and effectively be used for quantitive determinationof solid solution elements in binder of Ti(CN) ceramic-metal.
quote
| GB/T 7714-2015 | [1] ZHANG Jie. Quantitative Determination of Solid Solution Elements in Binder of Ti(CN)Ceramic-metal[J]. Rare Metals and Cemented Carbides, 1996(1): 26-28. |
| MLA | [1] ZHANG Jie. "Quantitative Determination of Solid Solution Elements in Binder of Ti(CN)Ceramic-metal." Rare Metals and Cemented Carbides, no. 1, 1996, pp. 26-28. |