Reclaiming Cemented Carbide Scrap by Electrolysis
Rare Metals and Cemented Carbides | Vol., Issue 3, 1996 |
pp. 38-42
A new-type electrolytic cell is designed, in which the technology for the recovery of cemented scrap is studied. The results show that the anode passivation can be decreased through the mechanical force of the drum anode, and the current efficiency can be improved.