5-Br-PADAP Spectrophotometry of Nb and Ta in W Concentrate and Difficult Cassiterite AITranslate

Test and Analysis Center of Zhongnan University of Technology
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Use of spectrophotometry with several wave lengths in mixed complex system with 5-Br-PADAP developer to determine Nb and Ta from W concentrate and cassiterite can make the determination fast, accurate and sensitive with relative standard deviation 0. 021 (n= 16). The paper deals with this method.

KeyWords AITranslate

spectrophotometry 5-Br-PADAP Nb Ta

1周名成,晋勇,白华.用5—Br—PADAP—OP及水杨基萤光酮—CPC体系分光光度法测定微量铌钽[J]冶金分析,1986(02).

2岩石矿物及测试一九八五年(第四卷)总目录[J]岩石矿物及测试,1985(04).

3《分析化学手册》内容简介[J].化工学报,1983,0(1):46-46. 被引量:613

4石油地质实验室工作中若干问题的讨论——中心实验室参加实验会议的综合报导[J]石油地质实验文摘,1963(02).

1李彤,任凤莲.钨及其化合物中杂质元素的分析进展[J].冶金分析,2005,25(6):33-38. 被引量:4

2王献科,李莉芬.液膜分离富集钽[J].中国钼业,2006,30(6):23-25.

3王献科,李玉萍.液膜分离富集钽及测定微量钽[J].有色金属与稀土应用,1999(1):42-44. 被引量:1

4吴辛友,童坚.我国钨工业化学分析进展[J].稀有金属,2000,24(6):427-433. 被引量:7

5冯尚彩.铌的光度分析应用进展[J].理化检验:化学分册,2003,39(8):499-502. 被引量:2

1李波.多波长和导数方法在钨分光光度分析中的应用[J].稀有金属与硬质合金,2005,33(3):56-58. 被引量:1

2史艳丰,董红星.乳状液膜的应用及数学模型[J].化工时刊,2005,19(10):66-69.

3姚素薇,朱建红,刘春松,张卫国,王宏智.Ni-W合金镀液中钨的分光光度分析[J].电镀与精饰,2007,29(1):45-47. 被引量:3

4李艳芬,刘英,童坚.离子色谱-膜去溶-ICP-MS法测定高纯钨粉中痕量金属杂质[J].分析试验室,2009,28(1):104-106. 被引量:13

5申云香,高灿柱.Ni-W-P合金电镀液中钨的测定[J].材料保护,2009,42(4):70-72. 被引量:1

6戴亚明.原子光谱分析法测定纯钨中痕量杂质和钨基硬质合金中组成元素[J].现代科学仪器,2009,26(6):96-100. 被引量:4

7黄俊杰,陈晓波.新的极谱催化体系连续测定岩溶地下水中钨和钼[J].光谱实验室,2010,27(3):854-858.

8郝登越,于秀兰.混合表面活性剂存在条件下安替吡啉偶氮水杨醛与铌的显色反应[J].湿法冶金,2014,33(2):158-160. 被引量:1

9苑海涛,陈强,周丽华,陈福平,丁海云,张慧妍.硫氰酸盐光度法测定钨矿浸出液中的钨[J].铀矿冶,2016,35(2):145-148.

10王佳翰,冯俊,王达成,张亚峰.电感耦合等离子体质谱法测定地球化学样品中钼镉钨铀锡[J].冶金分析,2017,37(6):20-25. 被引量:10

1滕松根.ICP-AES法同时测定钨精矿中的多种元素[J].光谱实验室,1990,7(4). 被引量:2

2膝松根.ICP─AES法测定钨精矿中钒铌钽钛[J].现代商检科技,1996,6(1):32-33. 被引量:2

3刘青.钨精矿中砷的测定[J].硅谷,2013,6(7):188-189.

4刘绍忠.从跌倒处前行[J].湖南安全与防灾,2012(1):37-37.

5龙宝林.赣南地区新一轮钨矿调查评价实施背景和工作重点[J].资源调查与环境,2006,27(2):83-84. 被引量:1

6报导与摘要[J].国外金属矿选矿,2008,45(6):42-43.

7白林山,陈庆.5-Br-PADAP分光光度法测定雨水中微量过氧化氢[J].环境科学与技术,1996(4):20-21. 被引量:2

8钨精矿开采量逐年增长行业急寻新平衡点 中国钨的生产[J].中国粉体工业,2010(2):45-46.

9郑美蓉.钨精矿中含磷量测定方法的改进[J].福建化工,1990(2):45-49.

10杨召会.钨:坚冰之旅等待打破[J].中国有色金属,2008(4):64-65.

Basic Information:

DOI:

Chinese Library Classification Number:P618.67[天文地球—矿床学];P575.4[天文地球—矿物学]

Citation Information:

Use of spectrophotometry with several wave lengths in mixed complex system with 5-Br-PADAP developer to determine Nb and Ta from W concentrate and cassiterite can make the determination fast, accurate and sensitive with relative standard deviation 0. 021 (n= 16). The paper deals with this method.

quote

GB/T 7714-2015 [1] LI Tian-rui. 5-Br-PADAP Spectrophotometry of Nb and Ta in W Concentrate and Difficult Cassiterite[J]. Rare Metals and Cemented Carbides, 1996(3): 48-51.
MLA [1] LI Tian-rui. "5-Br-PADAP Spectrophotometry of Nb and Ta in W Concentrate and Difficult Cassiterite." Rare Metals and Cemented Carbides, no. 3, 1996, pp. 48-51.
APA [1] LI Tian-rui. (1996). 5-Br-PADAP Spectrophotometry of Nb and Ta in W Concentrate and Difficult Cassiterite. Rare Metals and Cemented Carbides(3), 48-51.
IEEE [1] LI Tian-rui, "5-Br-PADAP Spectrophotometry of Nb and Ta in W Concentrate and Difficult Cassiterite," Rare Metals and Cemented Carbides, no. 3, pp. 48-51, 1996. keywords: {spectrophotometry;5-Br-PADAP;Nb;Ta}