Study of H_3 PO_4 Dynamic Leaching for Treatment of Low-cobalt Cemented Carbide Scraps AITranslate

Ministry of Domestic Trade Materials Recycling Research Institute;Ministry of Domestic Trade Materials Recycling Research Institute;Ministry of Domestic Trade Materials Recycling Research Institute
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

H3 PO4 leaching method in presence of oxidizer was used to study the decomposing of the low-cobalt cemented carbide scraps.Based on the results of exper iment, a proper reclamation route was founded. The paper describes the experiment.

KeyWords AITranslate

H_3PO_4 dynamic leaching oxidizer low-cobalt cemented carbide scrap

1林治坤,马成兵,吴玲.从废钼合金催化剂中提取钼等有价元素方法的研究[J].中国钼业,1998,22(2):3-5. 被引量:7

2梁勇.钴基废合金中钴的回收工艺研究进展[J].稀有金属与硬质合金,2009,37(4):58-60. 被引量:6

3秦恬,纪箴,贾成厂,柏慧凝,陈明营,刘博文.废旧硬质合金短流程回收工艺特点及优化[J].粉末冶金技术,2018,0(2):153-158. 被引量:5

1杨万军,杨晓美,薛军.从含钼废催化剂中回收有价金属钼的探讨与实践[J].中国钼业,2005,29(1):35-38. 被引量:22

2马成兵,王淑芳,袁应斌.含钼、镍、铋、钴废催化剂综合回收的实验研究[J].中国钼业,2007,31(5):23-25. 被引量:10

3王海北,蒋开喜,林江顺,刘三平.废旧锂离子电池钴综合回收技术研究[J].日用电器,2010(9):15-17. 被引量:2

4徐志昌,张萍.乏催化剂综合回收工艺现状与展望[J].中国钼业,2011,35(6):21-37.

5李俊,滕浩,郑雅杰.硫酸钴溶液深度净化工艺研究[J].矿冶工程,2012,32(3):99-102. 被引量:10

6张亨.可再生钼资源回收研究进展[J].中国钼业,2014,38(4):1-4. 被引量:1

7张亨.钼酸钠的生产研究进展[J].中国钼业,2014,38(6):1-6. 被引量:2

8郑瑞娟,钟坚海,凌宝龙,黄田富.废旧镍氢电池正极材料中钴的提取研究[J].新乡学院学报,2015,32(9):22-25.

9何沁华,刘维桥,邹超,魏成文,尚通明,周全法,高峰.氨-碳酸盐法分离PTA废渣中的钴和锰[J].化工进展,2016,35(8):2580-2585. 被引量:2

10李平,邓攀,刘宜强,夏侯斌,余音宏,陈星斌.从硬质合金磨削废料中综合回收钴试验研究[J].湿法冶金,2017,36(4):271-274. 被引量:6

1翟昕,周长松,苗兴军.磷酸动态浸出法处理低钴类废硬质合金[J].硬质合金,1997,14(2):126-127. 被引量:3

2佘振辉.废硬质合金回收方法的进展[J].硬质合金,1997,14(1):53-54. 被引量:5

3梁琥琪,陈世琯,胡玉好.电化学法处理废硬质合金直接回收金属钴和碳化钨[J].硬质合金,1995,12(2):89-91. 被引量:7

4张瑞娜,陈善平,张益.焚烧飞灰中重金属离子溶出试验方法论述[J].环境卫生工程,2014,22(2):1-3. 被引量:1

5李橙,刘建国,张俊丽,岳东北,聂永丰,王长海.生态水泥胶砂块中重金属的动态浸出行为研究[J].环境科学,2008,29(3):831-836. 被引量:9

6南旭阳,张碧双.飞灰重金属在海水中动态浸出特性研究[J].陕西农业科学,2009,55(3):64-66.

7翟昕,周长松.刍议我国废旧硬质合金再生利用中存在的几个问题及对策[J].再生资源研究,1991(2):42-44.

8梁琥琪,陈世琯.电化学法处理废硬质合金回收钨钴[J].上海大学学报:自然科学版,1995,1(1):105-112. 被引量:1

9张外平.电溶法处理低钴硬质合金废料的研究[J].硬质合金,2006,23(2):107-109. 被引量:10

10袁书玉.磷酸法处理废硬质合金回收钨和钴[J].现代化工,1996,16(3):34-35. 被引量:4

Basic Information:

DOI:

Chinese Library Classification Number:X758.05[环境科学与工程—环境工程]

Citation Information:

H3 PO4 leaching method in presence of oxidizer was used to study the decomposing of the low-cobalt cemented carbide scraps.Based on the results of exper iment, a proper reclamation route was founded. The paper describes the experiment.

quote

GB/T 7714-2015 [1] DI Xin, ZHOU Chang-song, MIAO Xing-jun. Study of H_3 PO_4 Dynamic Leaching for Treatment of Low-cobalt Cemented Carbide Scraps[J]. Rare Metals and Cemented Carbides, 1996(2): 1-6.
MLA [1] DI Xin, et al., "Study of H_3 PO_4 Dynamic Leaching for Treatment of Low-cobalt Cemented Carbide Scraps." Rare Metals and Cemented Carbides, no. 2, 1996, pp. 1-6.
APA [1] DI Xin, ZHOU Chang-song, & MIAO Xing-jun. (1996). Study of H_3 PO_4 Dynamic Leaching for Treatment of Low-cobalt Cemented Carbide Scraps. Rare Metals and Cemented Carbides(2), 1-6.
IEEE [1] DI Xin, ZHOU Chang-song, and MIAO Xing-jun, "Study of H_3 PO_4 Dynamic Leaching for Treatment of Low-cobalt Cemented Carbide Scraps," Rare Metals and Cemented Carbides, no. 2, pp. 1-6, 1996. keywords: {H_3PO_4,dynamic leaching, oxidizer, low-cobalt cemented carbide scrap}