Investigation on the Mechanical Properties and Chemical Stability of WC Fe/Ni/Co Cemented Carbides
Rare Metals and Cemented Carbides | Vol., Issue 3, 1999 |
pp. 26-29
The study was carried out on the two WC Fe/Ni/Co cemented carbides whose binders are Fe+Co+Ni (10%) and Fe+Co+Ni(20%). The influence of elements of Fe, Ni,and their contents in the materials on mechanical properties and chemical stability was in vestigated. The experimental results show that Co could be successfully replaced by optimum Fe/Ni/Co binder using “dual grain structure” wet grinding process.