Study of Mechanical Behavior of Low rhenium Molybdenum Alloys AITranslate

Zhongnan University of Technology;Zhongnan University of Technology;Zhongnan University of Technology
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The mechanical behavior of Mo 3%Re alloys prepared by PM was investigated. It was observed that the relation between tensile strength and annealing temperature for the alloy wire specimens conformed to linear regression equation in the range of 900 to 1 400 ℃ annealing temperature. The Mo 3%Re alloy by dry wet mixing method exhibited higher tensile strength and higher recrystallization temperature as compared with that by dry mixing method. The recrystallization temperature for the Mo 3% Re alloy wires is around 1 200 ℃.

KeyWords AITranslate

molybdenum rhenium mechanical behavior

1刘沙.-[J].稀有金属与硬质合金,1997,(4):26-26.

1陈文帅,周增林,李艳,惠志林,何学良,付霄荧.钼材料杂质元素晶界偏聚的研究进展[J].稀有金属,2021,45(12):1512-1520. 被引量:2

2杨尚磊,陈艳,薛小怀,李仕民,楼松年.铼(Re)的性质及应用研究现状[J].上海金属,2005,27(1):45-49. 被引量:47

3曾毅,孙院军,王娜,安耿,孙军.氧化物共还原制备Mo-10Re预合金粉末及其烧结特性研究[J].中国钼业,2023,47(4):50-56.

4曾毅,孙院军,安耿,丁向东,丘玺,王娜,孙军.核反应堆用钼铼合金结构材料研究进展[J].粉末冶金技术,2023,41(4):307-314.

1付小方,侯立玮,杨大宏.四川省稀散元素矿产资源潜力及开发利用对策[J].四川地质学报,2006,26(1):10-18. 被引量:2

2李卫昌.钼精矿焙烧烟尘中铼浸出提取研究[J].中国钼业,2007,31(1):23-26. 被引量:17

3张军良,李中奎,张小明,张清,周军,付洁,王东辉.制备方式对MORe合金组织性能的影响[J].稀有金属材料与工程,2007,36(A03):355-358. 被引量:6

4张勇,何新波,曲选辉,段柏华.超高温材料的研究进展及应用[J].材料导报,2007,21(12):60-64. 被引量:23

5吴贤,李来平,张文钲,张新.铼的性质及铼资源分布[J].矿业快报,2008,24(11):67-69. 被引量:47

6程挺宇,熊宁,彭楷元,杨海兵,殷晶川.铼及铼合金的应用现状及制造技术[J].稀有金属材料与工程,2009,38(2):373-376. 被引量:31

7邱朝辉,钟宏,曹占芳,姚禛.铼的分离分析方法研究进展[J].稀有金属与硬质合金,2010,38(1):56-59. 被引量:13

8于世昆,伍艳辉.铼的分离提取研究进展[J].中国钼业,2010,34(2):7-12. 被引量:30

9张军良,李中奎,付洁,夏明星,殷涛,刘辉.电子束悬浮熔炼钼铼合金铸锭的热加工方法[J].中国钼业,2010,34(5):38-40. 被引量:1

10张然,王学田.ICP—MS法测定地质样品中铼含量[J].江西化工,2011,27(1):125-128. 被引量:8

1刘沙,曹昱,舒金波.低铼钼合金高温烧结过程的研究[J].稀有金属与硬质合金,1999,27(4):18-20. 被引量:3

Basic Information:

DOI:

Chinese Library Classification Number:TG146.412[金属学及工艺—金属材料]

Citation Information:

The mechanical behavior of Mo 3%Re alloys prepared by PM was investigated. It was observed that the relation between tensile strength and annealing temperature for the alloy wire specimens conformed to linear regression equation in the range of 900 to 1 400 ℃ annealing temperature. The Mo 3%Re alloy by dry wet mixing method exhibited higher tensile strength and higher recrystallization temperature as compared with that by dry mixing method. The recrystallization temperature for the Mo 3% Re alloy wires is around 1 200 ℃.

quote

GB/T 7714-2015 [1] LIU Sha, CAO Yu, SHU Jin-bo. Study of Mechanical Behavior of Low rhenium Molybdenum Alloys[J]. Rare Metals and Cemented Carbides, 1999(3): 33-36.
MLA [1] LIU Sha, et al., "Study of Mechanical Behavior of Low rhenium Molybdenum Alloys." Rare Metals and Cemented Carbides, no. 3, 1999, pp. 33-36.
APA [1] LIU Sha, CAO Yu, & SHU Jin-bo. (1999). Study of Mechanical Behavior of Low rhenium Molybdenum Alloys. Rare Metals and Cemented Carbides(3), 33-36.
IEEE [1] LIU Sha, CAO Yu, and SHU Jin-bo, "Study of Mechanical Behavior of Low rhenium Molybdenum Alloys," Rare Metals and Cemented Carbides, no. 3, pp. 33-36, 1999. keywords: {molybdenum rhenium;mechanical behavior}