The Influence of Rare Earth on Coefficient of Expansion and Binder Phase of Cemented Carbides AITranslate

State Key Laboratory of Powder Metallurgy;State Key Laboratory of Powder Metallurgy;State Key Laboratory of Powder Metallurgy
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

With the addition of rare earth,the effect on coefficient of expansion of cemented carbides, relative percentage and lattice constant of face centred cubic β Co were investigated.

KeyWords AITranslate

rare earth cemented carbides coefficient of expansion binder phase

1李锋,彭孜,陈国权,徐高磊,沈铁军.铜合金带材拉拔用辊模的设计及应用[J].特种铸造及有色合金,2022,42(6):774-776.

2张守全.0.2微米级超细晶硬质合金的烧结行为[J].粉末冶金材料科学与工程,2009,14(4):237-243. 被引量:9

3董建光,傅珠荣,李锋,沈月明,陈国权.不同成分铝杆的辊模拉拔工艺设计[J].特种铸造及有色合金,2021,41(6):743-747. 被引量:2

4董建光,戴登峰,李锋,薛建平,傅珠荣.水箱拉丝机拉拔锌线材用辊模的设计及应用[J].有色金属材料与工程,2021,42(6):35-39. 被引量:3

5张凤林,王成勇,宋月贤.WC-Co硬质合金的强韧化[J].粉末冶金技术,2003,21(4):236-240. 被引量:13

1李锋,彭孜,陈国权,徐高磊,沈铁军.铜合金带材拉拔用辊模的设计及应用[J].特种铸造及有色合金,2022,42(6):774-776.

2饶岩岩,张久兴,王澈,张国珍.钨/钴氧化物SPS直接碳化原位合成超细WC-Co硬质合金[J].稀有金属与硬质合金,2006,34(1):18-21. 被引量:13

3吴厚平,张立,赵晓兆,陈述,黄伯云.混合稀土掺杂硬质合金刀具工作表面稀土富集相的能谱分析[J].粉末冶金材料科学与工程,2010,15(2):117-122. 被引量:7

4魏崇斌,宋晓艳,赵世贤,张立,刘雪梅,刘文彬.超细WC-Co复合粉的原位反应合成及烧结致密化[J].粉末冶金材料科学与工程,2010,15(2):145-150. 被引量:12

5宗霞,鲁玉祥.稀土硬质合金的发展现状[J].矿山机械,2010,38(22):1-6. 被引量:7

6肖满斗.亚微米晶WC-Co硬质合金中粗晶组织的形成[J].粉末冶金材料科学与工程,2010,15(6):620-624. 被引量:1

7谢海唯,张守全,吴冲浒,程登峰.0.2μm级硬质合金的制备及其应用性能[J].粉末冶金材料科学与工程,2010,15(6):640-643. 被引量:8

8杜伟,聂洪波,吴冲浒.烧结工艺对低Co超细晶硬质合金性能的影响[J].粉末冶金材料科学与工程,2010,15(6):650-655. 被引量:16

9陈勤文,栾道成,王正云,陈慧,李重典,李荣钢,汪志超,陈莉.YG10-RE系超细晶硬质合金烧结工艺及晶粒长大抑制剂的研究[J].工具技术,2011,45(2):39-42. 被引量:6

10魏崇斌,宋晓艳,付军,吕效森,陆庆忠,高杨,王海滨.烧结方法对WC-Co硬质合金性能的影响[J].粉末冶金材料科学与工程,2012,17(3):315-320. 被引量:14

1韩胜利,宋月清,崔舜,夏扬,周增林,李明.Mo-Cu合金的开发和研究进展[J].粉末冶金工业,2007,17(5):40-45. 被引量:33

2王临江.大型闪速炉及熔融炉砌砖膨胀缝的设计与计算[J].有色冶金节能,1995,0(4):5-10.

3黄钧声,吴惕言,李健纯.测定硬质合金中钴相相组成的X射线衍射法[J].硬质合金,2003,20(2):109-112. 被引量:4

4赵凯,宫晓然,李杰,刘卫星,邢宏伟.急冷铜渣矿物学及其综合利用[J].中国矿业,2015,24(9):102-106. 被引量:8

5史留勇,刘义敏,张守全,黄继华,赵兴科.初始成分对梯度硬质合金微观组织及脱β层厚度的影响[J].中国有色金属学报,2012,22(7):1984-1990. 被引量:6

6尉海军,张磊,姚广春,刘宜汉,张晓明.改善铝中富铁相形貌对电磁净化的影响[J].铸造,2005,54(4):363-366. 被引量:9

7张磊,焦万丽,蔚海军,姚广春.富铁相杂质形态对电磁净化铝熔体效果的影响[J].特种铸造及有色合金,2005,25(3):131-132. 被引量:4

8刘一峥,杨翠颜,刘智杰.Al-Si合金组织遗传性对6463铝合金含硅相的影响[J].有色金属科学与工程,2013,4(4):81-84. 被引量:5

9孙绪新.梯度硬质合金的研制[J].粉末冶金技术,1998,16(4):260-264. 被引量:20

10白亮,麻永林,XING Shuqing,LIU Chenxin,ZHANG Jieyu.Phase Morphology Evolution in AISI301 Austenite Stainless Steel under Different Cooling Rates[J].武汉理工大学学报:材料科学英文版,2015,0(2):392-396.

Basic Information:

DOI:

Chinese Library Classification Number:TF125.3[冶金工程—粉末冶金];TG135.5[一般工业技术—材料科学与工程]

Citation Information:

With the addition of rare earth,the effect on coefficient of expansion of cemented carbides, relative percentage and lattice constant of face centred cubic β Co were investigated.

quote

GB/T 7714-2015 [1] LIU Hong-wei, CHEN Kang-hua, LV Hai-bo. The Influence of Rare Earth on Coefficient of Expansion and Binder Phase of Cemented Carbides[J]. Rare Metals and Cemented Carbides, 1999(3): 30-33.
MLA [1] LIU Hong-wei, et al., "The Influence of Rare Earth on Coefficient of Expansion and Binder Phase of Cemented Carbides." Rare Metals and Cemented Carbides, no. 3, 1999, pp. 30-33.
APA [1] LIU Hong-wei, CHEN Kang-hua, & LV Hai-bo. (1999). The Influence of Rare Earth on Coefficient of Expansion and Binder Phase of Cemented Carbides. Rare Metals and Cemented Carbides(3), 30-33.
IEEE [1] LIU Hong-wei, CHEN Kang-hua, and LV Hai-bo, "The Influence of Rare Earth on Coefficient of Expansion and Binder Phase of Cemented Carbides," Rare Metals and Cemented Carbides, no. 3, pp. 30-33, 1999. keywords: {rare earth;cemented carbides;coefficient of expansion;binder phase}