Development and Application of ITO Film AITranslate
Abstract AITranslate
The properties and applications ,preparation and market situation of indium tin oxide (ITO) films were reviewed. The new material features good properties, good photoelectrical properties and has wide applications in high technique areas,such as in liquid crystal display,solar energy battery, energy saving window glass and so on There is a good market for ITO films both in China and abroad About a half of indium products in the world is used for preparing ITO films China has rich indium resources and hence there is a vast potential market for ITO films in China.
KeyWords AITranslate
1赵宏生,陈炜,翁端,李恒德.玻璃表面功能膜的研究进展[J].材料导报,2004,18(6):1-4. 被引量:2
2付恩刚,庄大明,张弓.掺铝氧化锌薄膜的红外性能及机制[J].金属学报,2005,41(3):333-336. 被引量:18
3李凤雷,王庭慰,沈晓东,崔升.纳米氧化铟锡表面改性研究[J].合成纤维工业,2005,28(2):7-9. 被引量:2
4杨盟,刁训刚,刘海鹰,王天民.氨气和氮气气氛下热处理对ITO薄膜光电性能的影响[J].稀有金属材料与工程,2005,34(10):1637-1641. 被引量:9
5张越举,李晓杰,孙贵磊,陈涛,王小红.制备ITO靶材的探索[J].真空,2005,42(6):27-32. 被引量:3
6周宏明,易丹青,杨小玲.ITO薄膜的生产技术概况及发展趋势探讨[J].表面技术,2006,35(1):1-4. 被引量:13
7李建敏,刘晓红,王贺云,李安.铟的市场、应用及其提取技术[J].江西冶金,2006,26(1):41-43. 被引量:19
8古映莹,秦利平,吴会永,冯圣生,彭穗,宋丰轩,庄树新.溶剂热-煅烧法合成纳米ITO粉体[J].化工新型材料,2006,34(6):36-38. 被引量:2
9杨盟,刁训刚,刘海鹰,武哲,舒远杰.氮化处理对ITO薄膜光电特性影响[J].功能材料,2006,37(9):1518-1521. 被引量:1
10职利,徐华蕊,周怀营.氧化铟锡薄膜制备工艺参数的正交优化设计[J].液晶与显示,2006,21(5):465-468. 被引量:2
1王洁冰,何延春,许旻,邱家稳,吴春华,赵印中.电致变色热控器件透明导电层的制备与研究[J].真空科学与技术学报,2008,28(S1):83-87. 被引量:5
2孙吉梅,侯翠红,张宝林.纳米氧化铟锡制备方法研究[J].山东化工,2007,36(4):14-16. 被引量:1
3刘持,彭新村.氩氧比和工作压强对溅射AZO薄膜光电学性能的影响[J].湖南农机,2014(1):77-78.
4朱协彬,姜涛,邱冠周,黄伯云.ITO nano-powders prepared by microwave-assisted co-precipitation in aqueous phase[J].中国有色金属学会会刊:英文版,2009,0(S3):752-756. 被引量:2
5李世涛,乔学亮,陈建国.射频磁控溅射室温下制备ITO薄膜的光学性能研究[J].材料导报,2005,19(1):101-103. 被引量:5
6赖复兴,刘智勇,王红军,刘志宏,李玉虎.ITO废靶回收制备超细ITO粉末的研究[J].稀有金属快报,2005,24(2):27-29. 被引量:3
7毛黎明,李历历,段学臣.两种不同分散剂对ITO纳米粉末粒度和团聚的影响[J].稀有金属与硬质合金,2005,33(1):5-7. 被引量:5
8杨觉明,余萍,陈平,张海礁,许岗.热处理对ITO薄膜的显微结构及光电特性的影响[J].西安工业学院学报,2005,25(1):52-55. 被引量:5
9徐伟玲,李延升.液相共沉淀法制备氧化铟锡超细粉体材料的研究进展[J].应用化工,2005,34(7):404-407. 被引量:5
10古映莹,刘雪颖,谭坚,李丹,杨天足,赖琼琳.共沉淀法制备高比表面积的铟锡氧化物超细粉末[J].中南大学学报:自然科学版,2005,36(5):837-840. 被引量:4
1张保平.音色由淡薄变醇厚:对集成电路功放的改进[J].无线电与电视,1997(11):40-41.
2马林.金刚石在电子领域的重要用途[J].电子材料(机电部),1991(10):29-30.
3文友.铟锡氧化物薄膜的生产、应用与开发[J].稀有金属与硬质合金,1997,25(3):56-59. 被引量:9
4小文龙.安卓电子书人人都会做[J].软件指南,2012(3):26-29.
5周平.新建小区有线电视工程管理[J].西部广播电视,2016,0(15):255-255.
6关文勇.构建基于ANSYS的行波管分析和设计平台及探讨[J].成都电子机械高等专科学校学报,2004,7(3):1-4.
7闻伟,杨传仁,张继华,陈宏伟,梁鸿秋,张瑞婷.ITO/PLZT薄膜湿法刻蚀研究[J].压电与声光,2008,30(6):745-746. 被引量:7
8刘彤,赵京,孔玉娥,孙鑫.光子晶体光纤的研究与进展[J].硅酸盐通报,2004,23(2):36-39. 被引量:2
9杨钊,崔晓芳,郗雨林.高价金属元素掺杂ITO薄膜性能的研究现状[J].热加工工艺,2016,45(2):14-17.
10李霄,王勇刚,张世强,汪晓波,许晓军.半导体可饱和吸收镜被动锁模侧面抽运Nd∶YAG激光器研究[J].光学学报,2009(11):3103-3107. 被引量:9
Basic Information:
DOI:
Chinese Library Classification Number:TN304.21[电子电信—物理电子学]
Citation Information:
The properties and applications ,preparation and market situation of indium tin oxide (ITO) films were reviewed. The new material features good properties, good photoelectrical properties and has wide applications in high technique areas,such as in liquid crystal display,solar energy battery, energy saving window glass and so on There is a good market for ITO films both in China and abroad About a half of indium products in the world is used for preparing ITO films China has rich indium resources and hence there is a vast potential market for ITO films in China.
quote
| GB/T 7714-2015 | [1] DUAN Xue-chen, YANG Xiang-ping. Development and Application of ITO Film[J]. Rare Metals and Cemented Carbides, 1999(3): 58-60. |
| MLA | [1] DUAN Xue-chen, and YANG Xiang-ping. "Development and Application of ITO Film." Rare Metals and Cemented Carbides, no. 3, 1999, pp. 58-60. |
| APA | [1] DUAN Xue-chen, & YANG Xiang-ping. (1999). Development and Application of ITO Film. Rare Metals and Cemented Carbides(3), 58-60. |
| IEEE | [1] DUAN Xue-chen and YANG Xiang-ping, "Development and Application of ITO Film," Rare Metals and Cemented Carbides, no. 3, pp. 58-60, 1999. keywords: {indium oxide;tin oxide;film;liquid crystal display;solar energy battery} |