Co Recovery from Co Slag Arising from Scrap Hard Metal Smelting with Na_2SO_4

Rare Metals and Cemented Carbides | Vol., Issue 2, 2000 | pp. 22-25
The Co slag obtained from scrap hard metal smelting with Na 2SO 4 was analysed by XRD. Results show that the Co in the slag is in the form of Co 9S 8. Analysis of Co 9S 8 by phase diagram shows its formation mechanism, and oxiding roasting method for the Co slag treatment was put forward. Results show that after oxiding roasting of the Co slag,the leaching rate of Co is more than 99%.
DOI: Cited: 0 Download: 0

A New Approach to High-effective Use of Coal Gangue

Rare Metals and Cemented Carbides | Vol., Issue 2, 2000 | pp. 37-38
The paper reviews the comprehensive use of coal gangue in detail.Author highly appraises the new process for preparation of high early(strength) cement from coal gangue (researchers:Xie Zha ji,et al) as a effective method for use of coal gangue, and recommends that the researchers shall transfer the research results into production force as early as possible.
DOI: Cited: 0 Download: 0