Abstract AITranslate

By taking La Co Ni triangle system and Nd Cu,Gd Cu binary system for examples,the steps and principles of preparing metallographic samples of rare earth alloys are introduced.The metallographic photoes of 5La 73Co 22Ni,6La 89Co 6Ni,25.6La 34Co 40 4Ni,Nd 69Cu,Gd 12Cu are given with structure analysis.

KeyWords AITranslate

rare earth alloys metallographic sample structure analysis

1(苏)萨维茨基EM.稀土金属合金[M].北京:国防工业出版社,1965.116.

2徐光献.稀土(下)[M].北京:冶金工业出版社,1995.318.

3郑建宜.La-Co-Ni三元系相图[J].物理学报,1982,31(5):674-674.

4郑建宣.Gd-Cu二元系相图[J].物理学报,1983,32(11):1443-1443.

5(西德)岗特 斐卓.金相侵蚀手册[M].北京:科学普及出版社,1982.101.

6郑建宣.Nd-Cu二元系相图[J].物理学报,1983,32(11):1149-1149.

1魏建忠,宗斌,王国红.钕铁硼磁性材料金相样品的制备方法[J].物理测试,2006,24(5):61-62. 被引量:2

2宗斌,魏建忠,王国红.《热处理手册》(第3版)中的一些疏漏[J].实验科学与技术,2008,6(4):37-39.

3万晓东,赵华,黄辉,李颖,巩琛,冀克俭,李本涛.稀土发火合金的制备方法及表征分析概况[J].山东化工,2017,46(24):63-66.

1裴玲,张瑞,张岩,杨仲年.钕铁硼永磁材料电沉积制备工艺设计[J].滨州学院学报,2011,27(3):78-82. 被引量:3

2杜艳华,温丰,贺进明,池春霞.钴块镀镍层金相检验试样制备方法[J].理化检验:物理分册,2022,58(8):13-15.

1马孝娟.钢铁材料金相样品研磨过程中的缺陷分析与控制[J].新疆钢铁,2014,0(3):20-23. 被引量:6

2郦剑,吴涛,谢轶伦.金相样品制备及其对显微组织评判的影响[J].金属热处理,2006,31(10):10-14. 被引量:11

3谢中维.黄铜金相样品的快速制备[J].理化检验:物理分册,1992,28(3):8-8.

4顾美转.工业纯铁金相样品制备中形成的缺陷及消除方法[J].理化检验:物理分册,2000,36(10):468-468.

5童建华,李芳.金相样品制备中的假象对组织鉴别的影响[J].金属热处理,2009,34(5):79-82. 被引量:5

6宗斌,李惠娥,王二平.锌形变孪晶样品的制备[J].理化检验:物理分册,2001,37(12):542-543. 被引量:1

7Ti和Ti合金的金相样品制备[J].航天制造技术,2011(2):70-70.

8张宝良,魏铮,王燕文,孙静远,冯惠平.SiC颗粒增强LY12铝基复合材料金相样品及透射电镜样品的制备[J].理化检验:物理分册,1992,28(2):48-48.

9高力军,姚远程,原海,崔景博.复合抛光法在制备铜及铜合金金相样品中的应用[J].国防技术基础,2005(7):5-5.

10魏建忠,宗斌,王国红.钕铁硼磁性材料金相样品的制备方法[J].物理测试,2006,24(5):61-62. 被引量:2

Basic Information:

DOI:

Chinese Library Classification Number:TG146.45[金属学及工艺—金属材料]

Citation Information:

By taking La Co Ni triangle system and Nd Cu,Gd Cu binary system for examples,the steps and principles of preparing metallographic samples of rare earth alloys are introduced.The metallographic photoes of 5La 73Co 22Ni,6La 89Co 6Ni,25.6La 34Co 40 4Ni,Nd 69Cu,Gd 12Cu are given with structure analysis.

quote

GB/T 7714-2015 [1] XU Guo-fu. Preparation of Metallographic Samples and Structure Analysis of RE Alloys[J]. Rare Metals and Cemented Carbides, 2000(2): 26-29.
MLA [1] XU Guo-fu. "Preparation of Metallographic Samples and Structure Analysis of RE Alloys." Rare Metals and Cemented Carbides, no. 2, 2000, pp. 26-29.
APA [1] XU Guo-fu. (2000). Preparation of Metallographic Samples and Structure Analysis of RE Alloys. Rare Metals and Cemented Carbides(2), 26-29.
IEEE [1] XU Guo-fu, "Preparation of Metallographic Samples and Structure Analysis of RE Alloys," Rare Metals and Cemented Carbides, no. 2, pp. 26-29, 2000. keywords: {rare earth alloys;metallographic sample;structure analysis}