daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Co Recovery from Co Slag Arising from Scrap Hard Metal Smelting with Na_2SO_4 AITranslate

Zhuzhou Hard Alloy Factory;Zhuzhou Hard Alloy Factory;Zhuzhou Hard Alloy Factory;Zhuzhou Hard Alloy Factory
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The Co slag obtained from scrap hard metal smelting with Na 2SO 4 was analysed by XRD. Results show that the Co in the slag is in the form of Co 9S 8. Analysis of Co 9S 8 by phase diagram shows its formation mechanism, and oxiding roasting method for the Co slag treatment was put forward. Results show that after oxiding roasting of the Co slag,the leaching rate of Co is more than 99%.

KeyWords AITranslate

scrap hard metal smelting with Na 2SO 4 Co 9S 8 oxiding roasting Co recovery

1陈立宝,贺跃辉,黄伯云,刘业翔.钨合金废料的资源再生利用技术[J].粉末冶金材料科学与工程,2002,7(1):38-49. 被引量:5

2潘泽强,杨声海,夏志美,唐朝波,唐谟堂.从硬质合金处理渣中回收氧化钴[J].再生资源研究,2004(4):25-28. 被引量:2

3李安国,廖春发,饶先发.从含钴废料中回收钴的研究进展[J].中国资源综合利用,2009,27(2):16-18. 被引量:13

4梁勇.钴基废合金中钴的回收工艺研究进展[J].稀有金属与硬质合金,2009,37(4):58-60. 被引量:6

5邓朝勇,张谊,杨茂麟,徐本军.硫酸-双氧水浸出废旧锂离子电池中的钴[J].电池,2011,41(3):170-171. 被引量:6

6杨斌,陈广军,石安红,刘柏雄.废旧硬质合金短流程回收技术的研究现状[J].材料导报,2015,29(3):68-74. 被引量:15

7邝海.锌熔法回收废旧硬质合金的研究进展[J].稀有金属与硬质合金,2016,44(5):79-82. 被引量:13

8夏侯斌,李平,朱红英,邓攀,余音宏,刘宜强.真空冶金法回收WC-Co硬质合金废料的研究[J].有色金属:冶炼部分,2017(12):11-14. 被引量:3

9秦恬,纪箴,贾成厂,柏慧凝,陈明营,刘博文.废旧硬质合金短流程回收工艺特点及优化[J].粉末冶金技术,2018,0(2):153-158. 被引量:5

10陈广,陈思竹,熊平,羊坤,Sultan Ahmed Khoso.硬质合金磨削废料拌酸熟化保湿法工艺优化[J].四川有色金属,2023(1):44-48.

1李亮星,朱志城,贾孟熹,黄茜琳.硬质合金废料电解回收钨及W(Ⅵ)在熔盐中的电化学行为[J].材料导报,2022,36(S01):448-453.

2高海燕,王新平,贺跃辉,任斌,陈立宝,黄伯云.再生高密度钨合金的性能[J].中国有色金属学报,2004,14(12):2035-2042. 被引量:1

3赵万军,杨海林,阮建明.再生料制备的硬质合金组织与性能研究[J].硬质合金,2008,25(3):169-174. 被引量:17

4赵慕岳,范景莲,刘涛,成会朝,韩勇.中国钨加工业的现状与发展趋势[J].中国钨业,2010,25(2):26-30. 被引量:11

5郑雅杰,滕浩,闫海泉.硝酸氧化浸出难冶炼高砷钴矿[J].中国有色金属学报,2010,20(7):1418-1423. 被引量:10

6李军,武四平.碳化钨粉闭路循环生产新工艺[J].江西有色金属,2010,24(3):159-160.

7胡威,黄兴远,李小理.低品位磁铁矿尾矿中钴金属的回收[J].有色矿冶,2010,26(6):29-31. 被引量:2

8焦翠燕,郭学益.钴白合金处理工艺进展及研究方向[J].金属材料与冶金工程,2011,39(2):58-63. 被引量:9

9刘红斌,蒋伟,蒋训雄,汪胜东,范艳青.铜转炉渣湿法回收钴[J].有色金属:冶炼部分,2012(2):19-22. 被引量:7

10李俊,滕浩,郑雅杰.硫酸钴溶液深度净化工艺研究[J].矿冶工程,2012,32(3):99-102. 被引量:10

12011050复杂锑精矿的硫酸钠熔炼法[J].中国有色冶金,2011,40(5):78-78.

2张长理.电解法再生废硬质合金工艺进展[J].有色金属:冶炼部分,1990(2):40-42. 被引量:1

3栾广英,关晓宇.钴渣提取氧化钴工艺的改进[J].有色金属:冶炼部分,1993(3):15-16. 被引量:3

4李继铮,陈宝云.保护渣熔渣结晶性能的研究[J].钢铁研究,1998(1):11-15. 被引量:5

5周长松,康平.电解法处理废硬质合金工艺及发展前景[J].硬质合金,1989(1):47-52. 被引量:1

6张长理.电解法处理废硬质合金[J].中国物资再生,1992(8):13-15.

7储志强.选择性电解法处理废硬质合金的研究[J].湖南冶金,1997(2):4-7. 被引量:4

8翟昕,周长松.废硬质合金再生利用现状与化学浸出法工艺的发展动向[J].中国再生资源,1993,0(3):13-16.

9翟昕,周长松.废硬质合金再生利用现状与化学浸出法工艺的发展动向[J].中国再生资源,1993(2):26-28. 被引量:1

10李俊萌.难处理金矿石预处理工艺研究与应用现状[J].有色矿山,2002,31(5):21-29. 被引量:11

Basic Information:

DOI:

Chinese Library Classification Number:TF816.052[冶金工程—有色金属冶金]

Citation Information:

The Co slag obtained from scrap hard metal smelting with Na 2SO 4 was analysed by XRD. Results show that the Co in the slag is in the form of Co 9S 8. Analysis of Co 9S 8 by phase diagram shows its formation mechanism, and oxiding roasting method for the Co slag treatment was put forward. Results show that after oxiding roasting of the Co slag,the leaching rate of Co is more than 99%.

quote

GB/T 7714-2015 [1] JIANG Wen-wei, GAO Jin, PU Chong-en, et al. Co Recovery from Co Slag Arising from Scrap Hard Metal Smelting with Na_2SO_4[J]. Rare Metals and Cemented Carbides, 2000(2): 22-25.
MLA [1] JIANG Wen-wei, et al., "Co Recovery from Co Slag Arising from Scrap Hard Metal Smelting with Na_2SO_4." Rare Metals and Cemented Carbides, no. 2, 2000, pp. 22-25.
APA [1] JIANG Wen-wei, GAO Jin, PU Chong-en, & XIE Sheng-de. (2000). Co Recovery from Co Slag Arising from Scrap Hard Metal Smelting with Na_2SO_4. Rare Metals and Cemented Carbides(2), 22-25.
IEEE [1] JIANG Wen-wei, GAO Jin, PU Chong-en, and XIE Sheng-de, "Co Recovery from Co Slag Arising from Scrap Hard Metal Smelting with Na_2SO_4," Rare Metals and Cemented Carbides, no. 2, pp. 22-25, 2000. keywords: {scrap hard metal;smelting with Na 2SO 4;Co 9S 8;oxiding roasting;Co recovery}