Preparation of RE-Zinc Alloy AITranslate
Abstract AITranslate
Fused salt electrolysis for preparation of RE Zn alloy has been studied.while zinc is used as cathode (stirred),RE 8%~zinc alloy is obtained at cathode current density of 3.37 A/cm 2, t 760~790 ℃, RE chloride concentration of 28%~32%
KeyWords AITranslate
1田卫平.稀土锌铝合金的发展[J].昆明冶金高等专科学校学报,2002,18(2):14-17. 被引量:3
1杨斌,夏兰廷.锌铝合金的研究进展[J].铸造设备研究,2007(5):30-34. 被引量:16
2孙文声,张锦麟,何林斌,谢先娇,谢全文,张明.变形Zn-2Al合金的热处理硬化行为研究[J].特种铸造及有色合金,2010(12):1168-1170.
3闫洪.2002年云南金属材料与加工年评[J].云南冶金,2003,32(2):42-49. 被引量:1
1邓彤,刘东.铜渣浸出中镍的浸出行为研究[J].稀有金属,2000,24(2):81-84. 被引量:3
2江瑜,袁小武,胡蕴成.金属钠的制备研究[J].东方电气评论,2013,27(1):1-3. 被引量:5
3用熔融电解法制取铅钙合金[J].湖南有色金属,1995,11(2):4-4.
4梁成浩,明石正恒.氯化物溶液中敏化304不锈钢应力腐蚀开裂的临界电位[J].中国腐蚀与防护学报,1994,14(4):271-276. 被引量:1
5王志刚,李久青,吴荫顺.氯化物浓度及pH值对ICr13不锈钢微动腐蚀的影响[J].材料保护,2000,33(3):46-49. 被引量:3
6邵本逑.不锈钢箔片点蚀增长的研究。Ⅱ.温度、氯化物浓度和硫酸盐加剂的影响[J].腐蚀与防护,2003,24(2):91-91.
7张琳,曹备,吴荫顺,崔强,陈卓,方智.316L不锈钢楔形缝隙内溶液化学[J].北京科技大学学报,1996,18(S2):37-41. 被引量:3
8金创石,张廷安,牟望重,郑大录,曾勇,蒋孝丽.液氯化法浸金过程热力学[J].稀有金属,2012,36(1):129-134. 被引量:20
9高性能不锈钢(16)[J].不锈:市场与信息,2009(14):15-16.
10O.赫雷洛斯,R.夸罗茨,E.曼扎诺,魏明.用氯浸出法从反射炉和闪烁炉的炉渣中提出铜[J].现代矿业,1999,0(17):6-8.
Basic Information:
DOI:
Chinese Library Classification Number:TG174.443[金属学及工艺—金属表面处理];TF125.21[冶金工程—粉末冶金]
Citation Information:
Fused salt electrolysis for preparation of RE Zn alloy has been studied.while zinc is used as cathode (stirred),RE 8%~zinc alloy is obtained at cathode current density of 3.37 A/cm 2, t 760~790 ℃, RE chloride concentration of 28%~32%
quote
| GB/T 7714-2015 | [1] TAO Xiao-ping, XU Ying-chun. Preparation of RE-Zinc Alloy[J]. Rare Metals and Cemented Carbides, 2000(2): 18-21. |
| MLA | [1] TAO Xiao-ping, and XU Ying-chun. "Preparation of RE-Zinc Alloy." Rare Metals and Cemented Carbides, no. 2, 2000, pp. 18-21. |
| APA | [1] TAO Xiao-ping, & XU Ying-chun. (2000). Preparation of RE-Zinc Alloy. Rare Metals and Cemented Carbides(2), 18-21. |
| IEEE | [1] TAO Xiao-ping and XU Ying-chun, "Preparation of RE-Zinc Alloy," Rare Metals and Cemented Carbides, no. 2, pp. 18-21, 2000. keywords: {RE Zn alloy;fused salt electrolysis;technological condition} |