A Study of Frictional Wear Behaviors of Steel Bonded Carbide DGJW40 AITranslate
Abstract AITranslate
Various quenching processes have been done to the steel bonded carbide made by a new process before tempering. The tempered alloy was studied for its structure, wear's surface and wear property. The result shows that,the wearability of alloy relates to the dropping of hard phase. The structure of 1 150 ℃ quenched alloy is idealer. It has better wearability after tempering.roperty .Theresul
KeyWords AITranslate
1尤显卿,郑玉春,杜晓东,左其福.DGJW40钢结硬质合金淬火与回火的研究[J].硬质合金,1998,15(1):41-44. 被引量:3
2王荣滨,鹏程.钢结合金在冷挤压冲头上应用的研究[J].硬质合金,1994,11(3):176-180. 被引量:4
3邓志煜.断裂韧性Kic对WC钢复合材料剥层磨损的影响初探.摩擦学全国第三届学术交流会论文集[M].兰州:摩擦学全国第三届学术交流会,1982.49.
4杜晓东,尤显卿,郑玉春.一种新型钢结硬质合金初探[J].硬质合金,1997,14(2):74-77. 被引量:12
1梁和.新闻报道理念浅探[J].中国广播电视学刊,2002(12):79-79. 被引量:1
2杜晓东,丁厚福,郑玉春,许淑珍.锻造对RE-WC-钢复合材料组织与耐磨性的影响[J].材料科学与工艺,2006,14(6):577-579.
3杜晓东.DGJW40钢结硬质合金组织评价与热处理工艺研究[J].新技术新工艺,2001(4):30-31. 被引量:1
4杜晓东.电冶金铁基碳化钨复合材料热处理对组织和耐磨性的影响[J].特殊钢,2003,24(6):20-22.
1沈利群.硬质合金热处理研究进展[J].热处理,2002,17(2):1-6. 被引量:14
2吴昊.从法制与道德看新闻价值的应有之义[J].新闻世界,2015,0(1):144-145.
1罗军明,魏峥,艾云龙,张剑平.微波烧结温度对WC钢结硬质合金组织性能的影响[J].材料热处理学报,2011,32(7):31-36. 被引量:15
2杜晓东,尤显卿,郑玉春.新工艺制造WC钢结硬质合金回火工艺与耐磨性研究[J].硬质合金,1998,15(4):231-234. 被引量:8
3肖逸锋,周年丰,吴靓,许艳飞,钱锦文,李浪浪,贺跃辉.Cr含量对WC钢结硬质合金组织及力学性能的影响[J].金属热处理,2017,42(4):22-26. 被引量:4
4刘洋,陈华辉.WC钢结硬质合金的组织及磨损性能研究[J].热加工工艺,2013,42(18):100-102. 被引量:1
5杜晓东,尤显卿,郑玉春.冲击韧度对DGJW40钢结硬质合金耐磨性的影响[J].热加工工艺,1999,28(6):19-21. 被引量:6
6尤显卿,宋雪峰,张成军,马建国,黄曼平.电冶稀土WC钢结硬质合金中碳化物特征的研究[J].材料热处理学报,2006,27(6):74-77. 被引量:9
7杜晓东.DGJW40钢结硬质合金组织评价与热处理工艺研究[J].新技术新工艺,2001(4):30-31. 被引量:1
8杜晓东,尤显卿,郑玉春.一种新型钢结硬质合金初探[J].硬质合金,1997,14(2):74-77. 被引量:12
9刘爱军,刘宁,陈新杰,马力,石俊.电冶熔铸WC钢结硬质合金断裂韧度研究[J].热处理,2014,29(6):9-12.
10杜晓东,尤显卿,郑玉春.WC基钢结硬质合金磨损机理研究[J].硬质合金,2001,18(1):21-26. 被引量:10
Basic Information:
DOI:
Chinese Library Classification Number:TF125.32[冶金工程—粉末冶金];TG135.5[一般工业技术—材料科学与工程]
Citation Information:
Various quenching processes have been done to the steel bonded carbide made by a new process before tempering. The tempered alloy was studied for its structure, wear's surface and wear property. The result shows that,the wearability of alloy relates to the dropping of hard phase. The structure of 1 150 ℃ quenched alloy is idealer. It has better wearability after tempering.roperty .Theresul
quote
| GB/T 7714-2015 | [1] DU Xiao-dong, YOU Xian-qing, ZHENG Yu-chun, et al. A Study of Frictional Wear Behaviors of Steel Bonded Carbide DGJW40[J]. Rare Metals and Cemented Carbides, 2000(2): 14-17. |
| MLA | [1] DU Xiao-dong, et al., "A Study of Frictional Wear Behaviors of Steel Bonded Carbide DGJW40." Rare Metals and Cemented Carbides, no. 2, 2000, pp. 14-17. |
| APA | [1] DU Xiao-dong, YOU Xian-qing, ZHENG Yu-chun, & ZUO Qi-fu. (2000). A Study of Frictional Wear Behaviors of Steel Bonded Carbide DGJW40. Rare Metals and Cemented Carbides(2), 14-17. |
| IEEE | [1] DU Xiao-dong, YOU Xian-qing, ZHENG Yu-chun, and ZUO Qi-fu, "A Study of Frictional Wear Behaviors of Steel Bonded Carbide DGJW40," Rare Metals and Cemented Carbides, no. 2, pp. 14-17, 2000. keywords: {steel bonded carbide,quenching,wear} |