daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

A Wet process for Extracting As_2O_3 from As-containing Material:Design Consideration and Production AITranslate

Changsha Nonferrous Metallurgical Design Research Institute
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

This paper introduces the wet process for extracting As 2O 3 from As containing material.It improves the quality of product and reduces the air pollution in comparison with fire method.

KeyWords AITranslate

As containing material As pollution wet process for As extraction As 2O 3

1田文增,陈白珍,仇勇海.有色冶金工业含砷物料的处理及利用现状[J].湖南有色金属,2004,20(6):11-15. 被引量:32

2白猛,刘万宇,郑雅杰,张传福.冶炼厂含砷废水的硫化沉淀与碱浸[J].铜业工程,2007(2):19-22. 被引量:16

3胡斌,姚金江,王智友,周坐东.含砷烟灰脱砷现状[J].湖南有色金属,2013,29(5):41-44. 被引量:16

4胡斌.有色金属行业含砷废弃物处置技术的研究进展[J].化工环保,2014,34(2):114-118. 被引量:9

5彭长宏,唐谟堂.砷污染防治与含砷木材防腐剂的开发应用[J].安全与环境学报,2001,1(4):10-13. 被引量:16

6石靖,易宇,郭学益.湿法冶金处理含砷固废的研究进展[J].有色金属科学与工程,2015,6(2):14-20. 被引量:26

7吴俊升,陆跃华.高砷铅阳极泥预处理工艺述评[J].有色金属,2002,54(B07):180-185. 被引量:6

8宁阳坤,杨涛,李涛,任保增.铜冶炼白烟尘综合利用技术现状[J].河南化工,2017,34(2):7-10. 被引量:12

9宁阳坤,赵恒勤,刘红召,甄逢生,严龙飞,任保增.某白烟尘碱浸试验研究[J].矿产综合利用,2017,0(4):90-93. 被引量:6

10杨坤.含砷烟尘脱砷工艺研究进展[J].云南冶金,2022,51(2):76-81. 被引量:2

1张桂芳,朱道飞,刘能生,张礼进.Fe(Ⅲ)负载732强酸性阳离子交换树脂对铜冶炼污酸中砷离子的吸附研究[J].离子交换与吸附,2021,37(5):414-426.

2王青,廖亚龙,周娟,黄斐荣,李冰洁.含砷物料制备As_2O_3的研究进展[J].环境工程,2015,33(3):97-101. 被引量:7

3温炎燊,陈昌铭,陈志传.利用含铜蚀刻废液生产碱式碳酸铜[J].化工环保,2004,24(2):131-134. 被引量:20

4田文增,陈白珍,仇勇海.有色冶金工业含砷物料的处理及利用现状[J].湖南有色金属,2004,20(6):11-15. 被引量:32

5刘树根,田学达.含砷固体废物的处理现状与展望[J].湿法冶金,2005,24(4):183-186. 被引量:51

6赵晓军,张旭.高砷氯氧锑碱浸脱砷试验研究[J].云南冶金,2005,34(6):37-39. 被引量:3

7李宁,吴龙华,孙小峰,李法云,骆永明.修复植物产后处置技术现状与展望[J].土壤,2005,37(6):587-592. 被引量:33

8赵玉娜,朱国才.白烟灰浸出液砷与锌的分离与回收[J].矿冶,2006,15(4):84-87. 被引量:20

9李敦顺,易求实,马明兰.烟气制酸中的污酸处理方法[J].化学与生物工程,2006,23(12):55-56. 被引量:7

10吕水源,戴金兰,钟茂生.L-半胱氨酸预还原断续流动-HG-AFS法测定木材及木制品中微量砷[J].分析测试学报,2007,26(3):423-425. 被引量:3

1陈钢,袁海滨.铜精矿双顶吹冶炼工艺中砷的分布及流向[J].云南冶金,2016,45(1):30-33. 被引量:4

2余新华.炼砷工艺的发展及加压浸出工业试验[J].铜业工程,2008(3):30-32. 被引量:2

3张荣良.江西铜业公司含砷物料的现状及其综合利用[J].铜业工程,1996,0(4):9-11. 被引量:1

4彭建蓉,杨大锦,杨兰,李胜明.从高砷铅烟尘中回收铟的试验研究[J].云南冶金,2007,36(4):28-30. 被引量:6

5曲胜利,董准勤.干法收砷工艺的应用实践[J].中国有色冶金,2010,39(4):37-39. 被引量:8

6张晓峰,曹佐英,肖连生,李立清,王福源,张虎.焙烧对高砷白烟灰中铜浸出率的影响及其热力学分析[J].矿冶工程,2012,32(5):86-89. 被引量:22

7朱晓宇.不锈钢搅拌槽腐蚀的原因分析[J].铜业工程,2003(2):65-67.

8周晓源,郑子恩,李有刚.朝鲜平北冶炼厂湿法提砷工艺设计[J].有色金属,2003,55(3):62-64. 被引量:5

9欧阳辉.贵溪冶炼厂亚砷酸工艺综述[J].有色金属:冶炼部分,1999(4):10-12. 被引量:12

10陈锦安.黑铜中铜砷湿法分离试验研究[J].有色冶炼,1999,28(3):26-29. 被引量:10

Basic Information:

DOI:

Chinese Library Classification Number:TF814.052[冶金工程—有色金属冶金];TE126.43[石油与天然气工程—油气勘探]

Citation Information:

This paper introduces the wet process for extracting As 2O 3 from As containing material.It improves the quality of product and reduces the air pollution in comparison with fire method.

quote

GB/T 7714-2015 [1] DAI Xue-yu. A Wet process for Extracting As_2O_3 from As-containing Material:Design Consideration and Production[J]. Rare Metals and Cemented Carbides, 2000(2): 34-36.
MLA [1] DAI Xue-yu. "A Wet process for Extracting As_2O_3 from As-containing Material:Design Consideration and Production." Rare Metals and Cemented Carbides, no. 2, 2000, pp. 34-36.
APA [1] DAI Xue-yu. (2000). A Wet process for Extracting As_2O_3 from As-containing Material:Design Consideration and Production. Rare Metals and Cemented Carbides(2), 34-36.
IEEE [1] DAI Xue-yu, "A Wet process for Extracting As_2O_3 from As-containing Material:Design Consideration and Production," Rare Metals and Cemented Carbides, no. 2, pp. 34-36, 2000. keywords: {As containing material;As pollution;wet process for As extraction;As 2O 3}