Influence of Active Spheroidization Agent on the Morphology of Cobalt Oxalate

Rare Metals and Cemented Carbides | Vol., Issue 3, 2001 | pp. 20-22
Study is made of the influence of active spheroidization agent on the morphology of the cobalt oxalate.Analysis is made of the microstructures of industrial cobalt oxalate and spheroidial cobalt oxalate by X-diffractmeter and their morphology is observed under scanning eletron microscope.The experiment results showed addition of active spheroidization agent can result in distinct morphology change with better physical properties on the prerequisite of unchanged crystalline structure of the cobalt oxalate.
DOI: Cited: 0 Download: 0

Catalytic Synthesis of DOP,DOM and DOA with Ln_2O_3/ZrO_2 Catalyst

Rare Metals and Cemented Carbides | Vol., Issue 3, 2001 | pp. 23-26
The catalytic synthesis of DOP,DOM and DOA with catalyst Ln 2O 3/ZrO 2 (Ln=Nd,Sm,Er),prepared by coprecipitation-calcination method,has resulted in distinct efficiency improvement and due to its larger specific surface area and better dispersion by~60% less carrier Ln 2O 3 consumption compared with pure Ln 2O 3.
DOI: Cited: 0 Download: 0

Sol-Gel Process and Its Application for Preparation of Metallic Oxide Powder and the Coating

Rare Metals and Cemented Carbides | Vol., Issue 3, 2001 | pp. 30-33
Three types of Sol-Gel methods used in manufacturing metallic oxides were analyzed in this paper: gelation Sol-Gel method, organo-metal polyment Gel method and organo-polymer Silica-Gel method,their suitable applications were also reviewed.The paper focused on the discussion on powder agglomeration and coating crack propagation during oxide ceramic manufacturing.